t ‐ZrO 2 prepared by a novel zirconium oxalate synthesised solvothermally

Siyu Ni, Yafeng Li

Micro & Nano Letters· Volume 13· Issue 7

Abstract

In this work, the authors intentionally employ the oxalic acid (OA) to replace terephthalic acid to synthesise a novel zirconium oxalate under the similar reaction condition with UIO‐66. The powder X‐ray diffraction and thermal gravimetric analysis confirm that as‐synthesised zirconium oxalate is a pure phase and oxalate serves as bridging ligand. Scanning electron microscope indicates that zirconium oxalate is aggregated together by several micrometres of needle‐like crystals. After zirconium oxalate is calcined at 500°C, the product is the pure tetragonal zirconia (ZrO 2 ) with high crystallinity. The morphology and particle size of ZrO 2 are basically unmodified with a comparison with the zirconium oxalate. X‐ray photoelectron spectroscopy reveals that the structural carbon acts as a phase transformation promoter to stabilise the tetragonal ZrO 2 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal-Organic Frameworks: Synthesis and Applications · Zeolite Catalysis and Synthesis · Chemical Synthesis and Characterization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Chemical Engineering Changchun University of Technology Changchun 130012 People's Republic of China

References (25)

Show source-provided references
1. 10.1016/0920‐5861(94)80003‐010.1016/0920‐5861(94)80003‐0 ↗
2. 10.1016/0920‐5861(94)80002‐210.1016/0920‐5861(94)80002‐2 ↗
3. 10.1016/S0926‐860X(98)00397‐410.1016/S0926‐860X(98)00397‐4 ↗
4. 10.1016/j.biortech.2012.04.03510.1016/j.biortech.2012.04.035 ↗
5. 10.1006/jcat.1995.127210.1006/jcat.1995.1272 ↗
6. 10.1016/j.apt.2010.12.01210.1016/j.apt.2010.12.012 ↗
7. 10.1016/0926‐860X(95)00077‐110.1016/0926‐860X(95)00077‐1 ↗
8. 10.1016/S0926‐860X(96)00373‐010.1016/S0926‐860X(96)00373‐0 ↗
9. 10.1016/S0926‐860X(98)00197‐510.1016/S0926‐860X(98)00197‐5 ↗
10. 10.1016/j.jpcs.2010.03.00210.1016/j.jpcs.2010.03.002 ↗
11. 10.1016/j.jssc.2005.03.00510.1016/j.jssc.2005.03.005 ↗
12. 10.1016/j.powtec.2006.07.00810.1016/j.powtec.2006.07.008 ↗
13. 10.1021/jp037532x10.1021/jp037532x ↗
14. Factors influencing the stability of low temperature tetragonal ZrO2
15. 10.1016/j.molcata.2014.06.04110.1016/j.molcata.2014.06.041 ↗
16. 10.1063/1.238814610.1063/1.2388146 ↗
17. 10.1021/nl025660b10.1021/nl025660b ↗
18. 10.1039/C5RA04932F10.1039/C5RA04932F ↗
19. 10.1016/j.ceramint.2013.10.15910.1016/j.ceramint.2013.10.159 ↗
20. 10.1021/ja805795310.1021/ja8057953 ↗
21. 10.1039/B914919H10.1039/B914919H ↗
22. 10.1002/ejic.20120122810.1002/ejic.201201228 ↗
23. 10.1021/ja500330a10.1021/ja500330a ↗
24. 10.1039/C4CE00526K10.1039/C4CE00526K ↗
25. 10.1002/cber.1997130040610.1002/cber.19971300406 ↗