journal article·2019-05Open access

Double‐layer resist method to improve descum result when removing negative photoresist

Zheng Yang, Qiusen Wang, Liping Qi, Xing Wang, Kehong Li, Da Chen, Chen Li, Helin Zou

Micro & Nano Letters· Volume 14· Issue 6

Abstract

A novel double‐layer resist method was presented in this work to decrease the negative photoresist scum. Positive photoresist was chosen as the bottom layer resist and negative photoresist as the top layer resist. This work studied the effect of viscosity and thickness of bottom layer resist on the mean number of scum. The experiment shows that the low viscosity positive photoresist AZ703, with the spin speed of 3000 r/min and the thickness of 1.10 um, had prominent effect on the removal of photoresist. To minimise the area of the top layer contact with substrate and further reduce the scum, 8 µm was selected as the optimal retracting distance d of the bottom layer resist.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Photolithography Techniques · Thin-Film Transistor Technologies · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory for Micro/Nano Technology and Systems of Liaoning Province Dalian University of Technology Dalian 116024 People's Republic of China

School of Biomedical Engineering Dalian University of Technology Dalian 116024 People's Republic of China

Funding

National Natural Science Foundation of China

References (27)

Show source-provided references
1. TakahashiT.: ‘Adaptability of piezoelectric inkjet head’ 2001 pp.323–32710.2352/ISSN.2169-4451.2001.17.1.art00071_1 ↗
2. 10.1007/BF0247477710.1007/BF02474777 ↗
3. 10.1039/C7TC02558K10.1039/C7TC02558K ↗
4. 10.5370/KIEEP.2016.65.1.05710.5370/KIEEP.2016.65.1.057 ↗
5. 10.1016/j.snb.2017.08.01210.1016/j.snb.2017.08.012 ↗
6. 10.1007/s11837‐010‐0109‐410.1007/s11837‐010‐0109‐4 ↗
7. 10.1088/1758‐5082/6/1/01500110.1088/1758‐5082/6/1/015001 ↗
8. 10.1038/s41598‐017‐01804‐210.1038/s41598‐017‐01804‐2 ↗
9. 10.1007/s10971‐014‐3608‐x10.1007/s10971‐014‐3608‐x ↗
10. Characterization of photoresist films exposed to high‐dose implantation conditions
11. 10.1016/j.optlastec.2017.10.02610.1016/j.optlastec.2017.10.026 ↗
12. Patterning of platinum (Pt) thin films by chemical wet etching in Aqua Regia
13. 10.1016/j.snb.2017.10.00510.1016/j.snb.2017.10.005 ↗
14. 10.1016/j.optlaseng.2017.10.00910.1016/j.optlaseng.2017.10.009 ↗
15. 10.1143/JJAP.31.203510.1143/JJAP.31.2035 ↗
16. 10.1116/1.149590410.1116/1.1495904 ↗
17. 10.1016/j.mee.2012.02.04210.1016/j.mee.2012.02.042 ↗
18. 10.1016/j.mee.2013.03.16310.1016/j.mee.2013.03.163 ↗
19. 10.1016/j.snb.2017.08.21510.1016/j.snb.2017.08.215 ↗
20. 10.1149/1.212916210.1149/1.2129162 ↗
21. ChuC.‐Y.HsuT.‐J.ChiangT.‐H.et al.: ‘Development of new photoresist stripping agent’ 2014 pp.408–41010.1109/IMPACT.2014.7048392 ↗
22. 10.1117/12.47420710.1117/12.474207 ↗
23. 10.1016/j.apsusc.2016.03.10010.1016/j.apsusc.2016.03.100 ↗
24. 10.1149/1.212967610.1149/1.2129676 ↗
25. 10.1002/app.4587110.1002/app.45871 ↗
26. 10.1049/mnl.2010.015510.1049/mnl.2010.0155 ↗
27. 10.1088/1361‐6439/aa9c1e10.1088/1361‐6439/aa9c1e ↗