Preparation of titanium carbide nanosheet and tribological properties of copper matrix composites
Source abstract
Abstract
TiC nanosheets with a thickness of about 50 nm were successfully prepared via solvent thermal etching Ti 3 AlC 2 in hydrofluoric acid solution at 120°C. TiC reinforced copper‐matrix composites with a content of 3, 5, 7, 9, 10, and 12 wt% were prepared by powder metallurgy with copper powder and TiC nanosheet as raw materials. The friction and wear behaviours of copper matrix composites were tested on a ball on disc under dry sliding conditions. The results showed that TiC particles were evenly distributed on the substrate and had a good combination with the substrate. The friction coefficient and wear scar widths of the composites gradually decreased with the increase of TiC nanosheet content, the maximum reduction of friction and wear was achieved under the content of 7 wt% for the TiC nanosheets. The increase in load causes the increase of friction coefficient and wear scar widths. The wear of pure copper is mainly adhesive wear and peel wear. The addition of TiC nanosheets improves the bearing capacity of copper matrix composites, and the wear mechanism is mainly abrasive wear.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Changzhou Institute of Industry Technology Changzhou Jiangsu 213164 People's Republic of China
Funding
Qinglan Project of Jiangsu Province of China
References (24)
Show source-provided references
1. 10.1007/BF0054444810.1007/BF00544448 ↗
2. 10.1007/s00170‐017‐1494‐410.1007/s00170‐017‐1494‐4 ↗
3. 10.1016/j.wear.2012.11.02910.1016/j.wear.2012.11.029 ↗
4. 10.1016/j.scriptamat.2012.12.02710.1016/j.scriptamat.2012.12.027 ↗
5. 10.1007/s10853‐015‐9354‐910.1007/s10853‐015‐9354‐9 ↗
6. 10.1016/j.powtec.2014.08.05110.1016/j.powtec.2014.08.051 ↗
7. 10.1016/j.matdes.2013.02.03010.1016/j.matdes.2013.02.030 ↗
8. 10.1016/j.vacuum.2016.06.00810.1016/j.vacuum.2016.06.008 ↗
9. 10.1016/S1003‐6326(13)62648‐510.1016/S1003‐6326(13)62648‐5 ↗
10. 10.1016/j.jallcom.2014.10.01210.1016/j.jallcom.2014.10.012 ↗
11. 10.1007/s00170‐009‐2474‐010.1007/s00170‐009‐2474‐0 ↗
12. 10.1016/j.jallcom.2016.03.08510.1016/j.jallcom.2016.03.085 ↗
13. 10.1080/14786435.2015.111244210.1080/14786435.2015.1112442 ↗
14. Effect of weight percentage of TiC on their tribological properties of magnesium composites
15. 10.1016/j.powtec.2011.10.05010.1016/j.powtec.2011.10.050 ↗
16. 10.1016/j.ijrmhm.2010.06.00510.1016/j.ijrmhm.2010.06.005 ↗
17. 10.1016/j.powtec.2015.01.04710.1016/j.powtec.2015.01.047 ↗
18. 10.1039/C4TA02638A10.1039/C4TA02638A ↗
19. 10.1149/2.0371501jes10.1149/2.0371501jes ↗
20. 10.1021/acs.chemmater.7b0284710.1021/acs.chemmater.7b02847 ↗
21. 10.1016/j.ceramint.2016.07.15010.1016/j.ceramint.2016.07.150 ↗
22. 10.1179/1743676114Y.000000015410.1179/1743676114Y.0000000154 ↗
23. 10.1142/S179329201550071X10.1142/S179329201550071X ↗
24. 10.1016/j.jpcs.2014.10.02410.1016/j.jpcs.2014.10.024 ↗