Origin of Rectification in Boron Nitride Heterojunctions to Silicon
Source abstract
Abstract
Cubic and hexagonal boron nitride (cBN and hBN) heterojunctions to n-type Si are fabricated under low-energy ion bombardment by inductively coupled plasma-enhanced chemical vapor deposition using the chemistry of fluorine. The sp2-bonded BN/Si heterojunction shows no rectification, while the cBN/sp2BN/Si heterojunction has rectification properties analogue to typical p-n junction diodes despite a large thickness (∼130 nm) of the sp2BN interlayer. The current-voltage characteristics at temperatures up to 573 K are governed by thermal excitation of carriers, and mostly described with the ideal diode equation and the Frenkel-Poole emission model at low and high bias voltages, respectively. The rectification in the cBN/sp2BN/Si heterojunction is caused by a bias-dependent change in the barrier height for holes arising from stronger p-type conduction in the cBN layer and enhanced with the thick sp2BN interlayer for impeding the reverse current flow at defect levels mainly associated with grain boundaries.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Applied Science for Electronics and Materials, Interdisciplinary Graduate School of Engineering Sciences, Kyushu University, Kasuga, Fukuoka 816-8580, Japan
Exploratory Materials Research Laboratory for Energy and Environment, National Institute for Materials Science, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047, Japan
References (31)
Show source-provided references
1. Watanabe K. · Phys. Stat. Sol., A. · 2004 · 201 · 256110.1002/pssa.200405188 ↗
2. Mishima O. · Science · 1987 · 238 · 18110.1126/science.238.4824.181 ↗
3. Ronning C. · Diamond Relat. Mater. · 1997 · 6 · 112910.1016/S0925-9635(97)00021-6 ↗
4. Litvinov D. · Diamond Relat. Mater. · 1998 · 7 · 36010.1016/S0925-9635(97)00216-1 ↗
5. Nose K. · Appl. Phys. Lett. · 2006 · 89 · 11212410.1063/1.2354009 ↗
6. Yin H. · J. Appl. Phys. · 2008 · 104 · 02370310.1063/1.2956739 ↗
7. Ying J. · J. Appl. Phys. · 2011 · 109 · 02371610.1063/1.3544065 ↗
8. Mirkarimi P. B. · Mater. Sci. Eng., R Rep. · 1997 · 21 · 4710.1016/S0927-796X(97)00009-0 ↗
9. Weidner S. · Diamond Relat. Mater. · 2012 · 22 · 8810.1016/j.diamond.2011.12.024 ↗
10. Sugino T. · Appl. Phys. Lett. · 1997 · 71 · 1810.1063/1.120183 ↗
11. He B. · Appl. Phys. Lett. · 2008 · 92 · 10210810.1063/1.2896643 ↗
12. Nose K. · Appl. Phys. Lett. · 2003 · 83 · 94310.1063/1.1597744 ↗
13. Nose K. · Diamond Relat. Mater. · 2005 · 14 · 129710.1016/j.diamond.2004.11.044 ↗
14. Matsumoto S. · Jpn. J. Appl. Phys. Part 2 · 2000 · 39 · L44210.1143/JJAP.39.L442 ↗
15. Zhang W. J. · Appl. Phys. Lett. · 2001 · 79 · 453010.1063/1.1428762 ↗
16. Teii K. · J. Appl. Phys. · 2007 · 101 · 03330110.1063/1.2431401 ↗
17. Teii K. · Appl. Phys. Lett. · 2008 · 92 · 01311510.1063/1.2830006 ↗
18. Teii K. · J. Appl. Phys. · 2009 · 106 · 11370610.1063/1.3261845 ↗
19. Teii K. · J. Appl. Phys. · 2012 · 111 · 09372810.1063/1.4711093 ↗
20. Teii K. · ACS Appl. Mater. Interfaces · 2012 · 4 · 524910.1021/am301133d ↗
21. Teii K. · J. Appl. Phys. · 2001 · 89 · 471410.1063/1.1359159 ↗
22. Teii K. · J. Appl. Phys. · 2007 · 101 · 01330210.1063/1.2402972 ↗
23. Teii K. · Thin Solid Films · 2011 · 519 · 181710.1016/j.tsf.2010.10.017 ↗
24. Kimura C. · Diamond Relat. Mater. · 2001 · 10 · 140410.1016/S0925-9635(00)00509-4 ↗
25. Sze S. M. · 2001
26. Frenkel J. · Phys. Rev. · 1938 · 54 · 64710.1103/PhysRev.54.647 ↗
27. Sze S. M. · 200610.1002/0470068329 ↗
28. Karim M. Z. · Surf. Coat. Technol. · 1993 · 60 · 50210.1016/0257-8972(93)90141-A ↗
29. Gielisse P. J. · Phys. Rev. · 1967 · 155 · 103910.1103/PhysRev.155.1039 ↗
30. Simmons J. G.. · Phys. Rev. · 1967 · 155 · 65710.1103/PhysRev.155.657 ↗
31. Watanabe K. · Nat. Mater. · 2004 · 3 · 40410.1038/nmat1134 ↗