Suppressing Sponge-Like Li Deposition via AlN-Modified Substrate for Stable Li Metal Anode
Source abstract
Abstract
Sponge-like lithium (Li) deposition results in high-surface-area morphology that harmfully accelerates the side reactions between Li and electrolyte, arousing serious safety issues of next high energy density Li metal batteries (LMBs). Herein, we propose a strategy to suppress the sponge-like Li deposition by plating Li metal on aluminum nitride (AlN)-modified substrates. For a practical Li deposition of 4 mAh cm–2 on a AlN-modified copper (Cu) electrode, the roughness and thickness of the as-deposited Li layer are only ∼10% and ∼50% of those for the Li layer deposited on bare Cu. Only based on the compacted Li deposition layer without any other protective remedies, the AlN-modified Cu electrode could provide a Li cycling life of 5 times longer than that on bare Cu, and an AlN-modified carbon felt was proved as an efficient interlayer to boost the cycling stability of Li||LiFePO4 batteries. These results demonstrate the high importance of suppressing the sponge-like Li deposition for high energy density LMBs.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering, Materials Genome Institute, Shanghai University, Shanghai 200444, China
Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China
Tianmu Lake Institute of Advanced Energy Storage Technologies, Liyang 213300, China
Funding
Natural Science Foundation of Ningbo · Ministry of Science and Technology of the People's Republic of China · Natural Science Foundation of Zhejiang Province · Ningbo 2025 Project
References (38)
Show source-provided references
1. 10.1016/j.ensm.2015.07.00110.1016/j.ensm.2015.07.001 ↗
2. 10.1021/acs.chemrev.7b0011510.1021/acs.chemrev.7b00115 ↗
3. 10.1039/C3EE40795K10.1039/C3EE40795K ↗
4. 10.1016/j.joule.2017.10.00710.1016/j.joule.2017.10.007 ↗
5. 10.1038/ncomms736210.1038/ncomms7362 ↗
6. 10.1002/adma.20170610210.1002/adma.201706102 ↗
7. 10.1038/s41565-018-0183-210.1038/s41565-018-0183-2 ↗
8. 10.1016/j.chempr.2018.05.00210.1016/j.chempr.2018.05.002 ↗
9. 10.1021/acsenergylett.9b0038110.1021/acsenergylett.9b00381 ↗
10. 10.1002/adma.20150452610.1002/adma.201504526 ↗
11. 10.1038/nenergy.2017.11910.1038/nenergy.2017.119 ↗
12. 10.1021/acs.nanolett.7b0102010.1021/acs.nanolett.7b01020 ↗
13. 10.1021/acsami.7b1466210.1021/acsami.7b14662 ↗
14. 10.1016/j.chempr.2017.01.00310.1016/j.chempr.2017.01.003 ↗
15. 10.1002/adfm.20170583810.1002/adfm.201705838 ↗
16. 10.1038/s41565-018-0061-y10.1038/s41565-018-0061-y ↗
17. 10.1038/s41563-019-0305-810.1038/s41563-019-0305-8 ↗
18. 10.1016/j.ensm.2017.06.00410.1016/j.ensm.2017.06.004 ↗
19. 10.1021/jacs.7b0176310.1021/jacs.7b01763 ↗
20. 10.1002/adma.20170038910.1002/adma.201700389 ↗
21. 10.1002/adma.20170621610.1002/adma.201706216 ↗
22. 10.1016/j.jechem.2018.11.01610.1016/j.jechem.2018.11.016 ↗
23. 10.1038/s41560-018-0104-510.1038/s41560-018-0104-5 ↗
24. 10.1038/nenergy.2016.1010.1038/nenergy.2016.10 ↗
25. 10.1002/adma.20170271410.1002/adma.201702714 ↗
26. 10.1016/j.joule.2018.02.00110.1016/j.joule.2018.02.001 ↗
27. 10.1002/anie.20181195510.1002/anie.201811955 ↗
28. 10.1038/ncomms1099210.1038/ncomms10992 ↗
29. 10.1002/aenm.20170340410.1002/aenm.201703404 ↗
30. 10.1016/j.nanoen.2017.12.05510.1016/j.nanoen.2017.12.055 ↗
31. 10.1149/1.139264910.1149/1.1392649 ↗
32. 10.1002/anie.20170209910.1002/anie.201702099 ↗
33. 10.1039/C4RA07955H10.1039/C4RA07955H ↗
34. 10.1103/PhysRevB.47.55810.1103/PhysRevB.47.558 ↗
35. 10.1103/PhysRevB.54.1116910.1103/PhysRevB.54.11169 ↗
36. 10.1103/PhysRevB.50.1795310.1103/PhysRevB.50.17953 ↗
37. 10.1103/PhysRevB.59.175810.1103/PhysRevB.59.1758 ↗
38. 10.1103/PhysRevLett.77.386510.1103/PhysRevLett.77.3865 ↗