Abstract

Abstract The identification, evaluation, and prevention of micro internal short circuits (ISCs) are crucial for the safety of large-capacity high-energy-density (HED) Li-ion cells. However, the evolution mechanism and the premonitory signals of the micro ISCs are not yet completely understood. Via a high-precision penetration test and accelerating rate calorimetry, we successfully trigger and investigate on-demand ISCs on a 60 Ah HED (≥ 290 Wh kg–1) Li-ion pouch cell with Si-based anode/Ni-rich cathode couple. Detailed behaviors of the cell components during micro ISCs, such as pinhole and crack formation, pore-closing, and rupture of the separators, as well as the destruction of positive electrodes and fusion of Al current collectors, are observed. Moreover, the correlation of these internal effects with external cell signals is identified. We demonstrate that voltage change signals, even at millivolt level, are noteworthy and can be used as premonitory signals for early warning of micro ISCs and leading indicators for predicting cell thermal runaway. The disclosed micro ISC propagation, alleviation, and acceleration mechanisms could guide the design of safe HED Li-ion cells.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Batteries and fuel cells for emerging electric vehicle markets10.1038/s41560-018-0108-1 ↗
2. Current status and challenges for automotive battery production technologies10.1038/s41560-018-0130-3 ↗
3. A materials perspective on Li-ion batteries at extreme temperatures10.1038/nenergy.2017.108 ↗
4. Mitigating thermal runaway of lithium-ion batteries10.1016/j.joule.2020.02.010 ↗
5. Differential scanning calorimetry material studies: implications for the safety of lithium-ion cells10.1016/S0378-7753(97)02611-6 ↗
6. High-energy cathode material for long-life and safe lithium batteries10.1038/nmat2418 ↗
7. High-nickel layered oxide cathodes for lithium-based automotive batteries10.1038/s41560-019-0513-0 ↗
8. Stable cycling of double-walled silicon nanotube battery anodes through solid–electrolyte interphase control10.1038/nnano.2012.35 ↗
9. Nanostructured silicon for high capacity lithium battery anodes10.1039/C0EE00281J ↗
10. Thermal runaway caused fire and explosion of lithium ion battery10.1016/j.jpowsour.2012.02.038 ↗
11. A review of recent developments in membrane separators for rechargeable lithium-ion batteries10.1039/C4EE01432D ↗
12. Battery separators10.1021/cr020738u ↗
13. Safer electrolytes for lithium-ion batteries: state of the art and perspectives10.1002/cssc.201500284 ↗
14. Progress of enhancing the safety of lithium ion battery from the electrolyte aspect10.1016/j.nanoen.2018.10.035 ↗
15. Toxicity, a serious concern of thermal runaway from commercial Li-ion battery10.1016/j.nanoen.2016.06.031 ↗
16. A review of international abuse testing standards and regulations for lithium ion batteries in electric and hybrid electric vehicles10.1016/j.rser.2017.05.195 ↗
17. Mechanism of the entire overdischarge process and overdischarge-induced internal short circuit in lithium-ion batteries10.1038/srep30248 ↗
18. Safety issues and mechanisms of lithium-ion battery cell upon mechanical abusive loading: a review10.1016/j.ensm.2019.06.036 ↗
19. Microscale failure mechanisms leading to internal short circuit in Li-ion batteries under complex loading scenarios10.1016/j.jpowsour.2016.04.005 ↗
20. Internal short circuit and failure mechanisms of lithium-ion pouch cells under mechanical indentation abuse conditions: an experimental study10.1016/j.jpowsour.2020.227939 ↗
21. Operando analysis of thermal runaway in lithium ion battery during nail-penetration test using an X-ray inspection system10.1149/2.0701906jes ↗
22. Direct observation of internal state of thermal runaway in lithium ion battery during nail-penetration test10.1016/j.jpowsour.2018.04.092 ↗
23. Thermal runaway features of large format prismatic lithium ion battery using extended volume accelerating rate calorimetry10.1016/j.jpowsour.2014.01.005 ↗
24. Analysis of internal short-circuit in a lithium ion cell10.1016/j.jpowsour.2009.05.002 ↗
25. Investigation of short-circuit scenarios in a lithium-ion battery cell10.1149/2.096206jes ↗
26. A review of safety-focused mechanical modeling of commercial lithium-ion batteries10.1016/j.jpowsour.2017.12.034 ↗
27. Study of the mechanisms of internal short circuit in a Li/Li cell by synchrotron X-ray phase contrast tomography10.1021/acsenergylett.6b00589 ↗
28. A superior thermostable and nonflammable composite membrane towards high power battery separator10.1016/j.nanoen.2014.10.001 ↗
29. Fast and reversible thermoresponsive polymer switching materials for safer batteries10.1038/nenergy.2015.9 ↗
30. Temperature-sensitive cathode materials for safer lithium-ion batteries10.1039/c0ee00590h ↗
31. Progress and perspectives on halide lithium conductors for all-solid-state lithium batteries10.1039/C9EE03828K ↗
32. Recent progress on solid-state hybrid electrolytes for solid-state lithium batteries10.1016/j.ensm.2019.06.021 ↗
33. Towards high-performance solid-state Li–S batteries: from fundamental understanding to engineering design10.1039/C9CS00635D ↗
34. Experimental triggers for internal short circuits in lithium-ion cells10.1016/j.jpowsour.2011.03.035 ↗
35. Internal short circuit trigger method for lithium-ion battery based on shape memory alloy10.1149/2.0731713jes ↗
36. Characterising thermal runaway within lithium-ion cells by inducing and monitoring internal short circuits10.1039/C7EE00385D ↗
37. Understanding Li-Ion cell internal short circuit and thermal runaway through small, slow and in situ sensing nail penetration10.1149/1945-7111/ab8878 ↗
38. Internal short circuit in Li-ion cells10.1016/j.jpowsour.2009.02.070 ↗
39. Comparative study of thermal runaway and cell failure of lab-scale Li-ion batteries using accelerating rate calorimetry10.1016/j.jiec.2019.11.034 ↗
40. Thermally induced reactions between lithiated nano-silicon electrode and electrolyte for lithium-ion batteries10.1149/2.095205jes ↗
41. Enhanced thermal stability of a lithiated nano-silicon electrode by fluoroethylene carbonate and vinylene carbonate10.1016/j.jpowsour.2012.08.066 ↗
42. Thermal behavior of lithiated graphite with electrolyte in lithium-ion batteries10.1149/1.2139955 ↗
43. Effect of a thin ceramic-coating layer on thermal and electrochemical properties of polyethylene separator for lithium-ion batteries10.1016/j.jpowsour.2014.07.142 ↗
44. In situ analysis of high temperature characteristics of prismatic polymer lithium - ion batteries10.1007/s10800-004-2459-5 ↗
45. Generalized separator failure criteria for internal short circuit of lithium-ion battery10.1016/j.jpowsour.2020.228360 ↗
46. Li-ion battery separators, mechanical integrity and failure mechanisms leading to soft and hard internal shorts10.1038/srep32578 ↗
47. New insights into nail penetration of Li‐ion batteries: effects of heterogeneous contact resistance10.1002/batt.201900081 ↗
48. Investigation on internal short circuits of lithium polymer batteries with a ceramic-coated separator during nail penetration10.1016/j.jpowsour.2015.04.010 ↗
49. Fusing phenomenon of lithium-ion battery internal short circuit10.1149/2.1721712jes ↗
50. Characterization of microporous separators for lithium-ion batteries10.1016/S0378-7753(98)00168-2 ↗
51. Characterization of thermal cut-off mechanisms in prismatic lithium-ion batteries10.1016/S0378-7753(01)00782-0 ↗
52. Improvement of thermal stability and safety of lithium ion battery using SiO anode material10.1016/j.jpowsour.2015.10.106 ↗
53. High-capacity Li-ion batteries using SiO-Si composite anode and Li-rich layered oxide cathode: cell design and its safety evaluation10.1149/2.0991508jes ↗