Abstract

Silicon carbide materials are excellent candidates for high-performance applications due to their outstanding thermomechanical properties and their strong corrosion resistance. SiC materials can be processed in various forms, from nanomaterials to continuous fibers. Common applications of SiC materials include the aerospace and nuclear fields, where the material is used in severely oxidative environments. Therefore, it is important to understand the kinetics of SiC oxidation and the parameters influencing them. The first part of this review focuses on the oxidation of SiC in dry air according to the Deal and Grove model showing that the oxidation behavior of SiC depends on the temperature and the time of oxidation. The oxidation rate can also be accelerated with the presence of H2O in the system due to its diffusion through the oxide scales. Therefore, wet oxidation is studied in the second part. The third part details the effect of hydrothermal media on the SiC materials that has been explained by different models, namely Yoshimura (1986), Hirayama (1989) and Allongue (1992). The last part of this review focuses on the hydrothermal corrosion of SiC materials from an application point of view and determine whether it is beneficial (manufacturing of materials) or detrimental (use of SiC in latest nuclear reactors).
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

CNRS, University of Bordeaux, Bordeaux INP, ICMCB, UMR 5026, 33600 Pessac, France

WPI-Advanced Institute for Materials Research (WPI-AIMR), Tohoku University, 2-1-1 Katahira, Aoba-ku, Sendai 980-8577, Japan

Department of Materials Science and Engineering, National Cheng Kung University, No. 1, University Road, Tainan 70101, Taiwan

Funding

WPI- Advanced Institute for Materials Research (WPI-AIMR) · “Région Nouvelle Aquitaine” and “Direction Générale de l’Armement”

References (100+)

Show source-provided references
1. Riedel, R. (2000). Handbook of Ceramic Hard Materials, Wiley-VCH.10.1002/9783527618217 ↗
2. Continuous silicon fibre of high tensile strength10.1246/cl.1975.931 ↗
3. Silicon Carbide–A Survey of Synthetic Approaches, Properties and Applications
4. The high-temperature oxidation, reduction, and volatilization reactions of silicon and silicon carbide10.1007/BF00613092 ↗
5. Rosenqvist, T. (1974). Principles of Extractive Metallurgy, McGraw-Hill.
6. Cooper, A.R., and Heuer, A.H. (1975). Mass Transport Phenomena in Ceramics, Plenum Press.10.1007/978-1-4684-3150-6 ↗
7. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
8. Oxidation effects on the mechanical properties of SiC fiber-reinforced reaction-bonded silicon nitride matrix composites10.1111/j.1151-2916.1992.tb08194.x ↗
9. Oxidation of Single-Crystal Silicon Carbide. Part 1990, I. Experimental Studies10.1149/1.2086568 ↗
10. Oxidation behavior of silicon carbide at 1200 °C in both air and water-vapor-rich environments10.1016/j.corsci.2014.07.052 ↗
11. General Relationship for the Thermal Oxidation of Silicon10.1063/1.1713945 ↗
12. Oxidation of 6H- Silicon Carbide Platelets10.1111/j.1151-2916.1975.tb18969.x ↗
13. Thermal Oxidation of Silicon in Dry Oxygen Growth-rate Enchancement in the Thin Regime. I. Experimental Results
14. Thermal Oxidation of Silicon in Dry Oxygen Growth-rate Enchancement in the Thin Regime. II. Physical Mechanisms
15. Unified theory of silicon carbide oxidation based on the Si and C emission model10.1088/0022-3727/49/22/225103 ↗
16. Universal theory of Si oxidation rate and importance of interfacial Si emission10.1143/JJAP.38.L971 ↗
17. Oxygen partial pressure dependence of the SiC oxidation process studied by in-situ spectroscopic ellipsometry10.1063/1.4736801 ↗
18. Macroscopic simulations of the SiC thermal oxidation process based on the Si and C emission model10.1016/j.diamond.2019.01.012 ↗
19. Hasunuma, R. (2017, January 23–25). Interfacial transition layer in thermally grown SiO2 film on 4H-SiC. Proceedings of the IEEE International Conference on IC Design and Technology (ICICDT), Austin, TX, USA.10.1109/ICICDT.2017.7993525 ↗
20. Unraveling the mechanisms responsible for the interfacial region formation in 4H-SiC dry thermal oxidation10.1063/1.4999332 ↗
21. Reaction mechanisms at 4H-SiC/SiO2 interface during wet SiC oxidation10.7567/JJAP.57.04FR08 ↗
22. Oxidation simulation study of silicon carbide nanowires: A carbon-rich interface state10.1016/j.apsusc.2019.07.016 ↗
23. Investigation of silicon carbide oxidation mechanism using ReaxFF molecular dynamics simulation10.2514/1.A34669 ↗
24. Ab initio calculations for the effect of wet oxidation condition on the reaction mechanism at 4H-SiC/SiO2 interface10.35848/1347-4065/ab85dd ↗
25. Oxidation Behavior of Silicon Carbide10.1111/j.1151-2916.1958.tb12932.x ↗
26. Thermal oxidation of sputtered silicon carbide thin Films
27. Passive-oxidation kinetics of high-purity silicon carbide from 800° to 1100 °C10.1111/j.1151-2916.1996.tb08724.x ↗
28. Oxidation kinetics of hot-pressed silicon carbide10.1007/BF00545142 ↗
29. Oxidation kinetics of hot-pressed and sintered alpha-SiC10.1111/j.1151-2916.1981.tb10297.x ↗
30. Oxidation kinetics of silicon carbide crystals and ceramics: I, In dry oxygen10.1111/j.1151-2916.1986.tb07470.x ↗
31. High-temperature passive oxidation of chemically vapor deposited silicon carbide10.1111/j.1151-2916.1989.tb07658.x ↗
32. Oxidation Kinetics of Chemically Vapor-Deposited Silicon Carbide in Wet Oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
33. A comparison of the oxidation kinetics of SiC and Si3N10.1149/1.2048559 ↗
34. Effect of oxygen partial pressure on the high-temperature oxidation of CVD SiC10.1016/S0010-938X(01)00066-X ↗
35. Silicon carbide non-ohmic resistors. II. Oxidation rates of silicon carbide
36. Oxidation of silicon carbide in the temperature range 1200 to 1500 °C10.1021/j150572a045 ↗
37. Oxidation of Silicon Carbide10.1111/j.1151-2916.1959.tb13582.x ↗
38. Effects of Oxygen Partial Pressure on the Oxidation of Silicon Carbide
39. The formation and devitrification of oxides on silicon10.1007/BF00549716 ↗
40. Temperature and oxygen pressure dependence of silicon carbide oxidation10.1021/j100872a067 ↗
41. High temperature kinetics of the oxidation and nitridation of pyrolytic silicon carbide in dissociated gases10.1021/j100704a002 ↗
42. Antill, J.E., and Warburton, J.B. (1970, January 1). Oxidation of silicon and silicon carbide in gaseous atmospheres at 1000–1300 °C. Proceedings of the AGARD Conference Proceedings, Paris, France.
43. Permeation of gaseous oxygen through vitreous silica10.1038/191701a0 ↗
44. On the rate of oxidation of silicon and of silicon carbide in oxygen, and correlation with the permability of silica glass10.3891/acta.chem.scand.18-1596 ↗
45. Effects of water vapour on oxidation of silicon carbide10.1111/j.1151-2916.1961.tb15374.x ↗
46. Microstructural evolution of silica on single-crystal silicon carbide. Part I: Devitrification and oxidation rates10.1111/j.1551-2916.2009.02930.x ↗
47. Crystallization kinetics of internally nucleated vitreous silica
48. Phase transformation of diphasic aluminosilicate gels10.1111/j.1151-2916.1988.tb05023.x ↗
49. The Effect of Surface Orientation on Silicon Oxidation Kinetics10.1149/1.2100881 ↗
50. Thermal oxidation of SiC and elelectric properties of Al-SiO2-SiC MOS structure10.1143/JJAP.21.579 ↗
51. Silicon oxycarbide formation on SiC surfaces and at the SiC/SiO2 interface10.1116/1.580951 ↗
52. Growth of SiO2 on SiC by dry thermal oxidation: Mechanisms10.1088/0022-3727/40/20/S10 ↗
53. First-principles-based investigation of kinetic mechanism of SiC 0001 dry oxidation including defect generation and passivation10.1063/1.3006004 ↗
54. High-carbon concentrations at the silicon dioxide-silicon carbide interface identified by electron energy loss spectroscopy10.1063/1.1314293 ↗
55. A study of the oxidation of pure silicon carbide powders10.2109/jcersj1950.65.736_88 ↗
56. A study of native oxides of B-SiC using Auger electron spectroscopy10.1557/JMR.1989.0404 ↗
57. Marshall, R.C., Faust, J.W., and Ryan, C.E. (1974). Kinetic Studies on the Oxidation of Silicon Carbide, University of South Carolina Press.
58. Effect of water vapor on the oxidation of hot-pressed silicon nitride and silicon carbide10.1111/j.1151-2916.1976.tb09398.x ↗
59. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys10.1149/1.2424115 ↗
60. Silicon oxidation studies: The role of H2O
61. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
62. Mass spectrometric identification of Si-O-H(g) species from the reaction of silica with water vapor at atmospheric pressure10.1111/j.1151-2916.1997.tb02935.x ↗
63. McNallan, M.J., Opila, E.J., Maruyama, T., and Narita, T. (1999). The oxidation rate of SiC in high pressure water vapor environments. High-temperature Corrosion Materials Chemistry, The Electrochemical Soc.
64. Oxidation and volatilization of silica formers in water vapor
65. Vincenzini, P. (2003). High temperature corrosion of silicon carbide and silicon nitride in water vapor. Advances in Science and Technology, NASA Glenn Researcher Center.
66. Variation of the oxidation rate of silicon carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
67. Effects of high water-vapor pressure on oxidation of silicon carbide at 1200 °C
68. Transitions from Parabolic to Linear Kinetics in Scaling of Metals10.1149/1.2427495 ↗
69. WET and Dry Oxidation of Single Crystal β-SiC: Kinetics and Interface Characteristics10.1557/PROC-54-553 ↗
70. Oxidation of silicon carbide in oxygen and in water vapour at 1500 °C10.3891/acta.chem.scand.35a-0247 ↗
71. Thermal oxidation of 3C silicon carbide single-crystal layers on silicon10.1063/1.95394 ↗
72. High-temperature oxidation of chemically vapor-deposited silicon carbide in wet oxygen at 1823 to 1923 K10.1111/j.1151-2916.1990.tb04261.x ↗
73. Ithaca, N. (1960). The Nature of the Chemical Bond, Cornell University Press.
74. Oxidation of silicon carbide in a wet atmosphere10.1007/BF01106816 ↗
75. The properties of silica: An introduction to the properties of substances in the solid non conducting state
76. Oxygen mobility in silicon dioxide and silicate glasses: A review10.1016/0955-2219(92)90010-B ↗
77. Passivity during the Oxidation of Silicon at Elevated Temperatures10.1063/1.1723429 ↗
78. Water in silica glass10.1039/tf9615701208 ↗
79. Water in Vitreous Silica
80. Properties and structure of vitreous silica10.1016/0022-3093(71)90032-9 ↗
81. Mitchell, J.W., and Devries, R.C. (1969). The diffusion of water in fused silica. Reactivity of Solids, Wiley.
82. Diffusion of water in crystalline; glass oxides: Diffusion-reaction-model10.1557/JMR.1999.0508 ↗
83. Shewmon, P.G. (1963). Diffusion in Solids, McGraw-Hill Book Company.
84. An oxygen tracer investigation of the diffusion of ‘water’ in silica glass
85. Diffusion of Water into Silica Glass at Low Temperature10.1111/j.1151-2916.1989.tb05990.x ↗
86. An empirical model for predicting diffusion coefficients in silicate minerals10.1126/science.245.4925.1481 ↗
87. Oxidationsverhalten des pyrolytisch abgeschiedenen B-SiC unter einer atmosphäre aus CO-CO2-gasgemischen10.1016/0022-3115(77)90186-6 ↗
88. Wood, J., Lindqvist, O., Helgesson, C., and Vannerberg, N.-G. (1977). Study of Oxygen Diffusion in Quartz by Activation Analysis. Reactivity of Solids, Springer.10.1007/978-1-4684-2340-2 ↗
89. Studies in diffusion: III. Oxidation in feldspars: An ion microprobe determination. Geochem10.1016/0016-7037(78)90215-6 ↗
90. Water effects on corrosion behavior of SiC ceramics10.1557/S0883769400048211 ↗
91. Corrosion behaviors of sintered; chemically vapor deposited silicon carbide ceramics in water at 360 °C10.1023/A:1023390111074 ↗
92. Oxidation of SiC powder by high-temperature, high-pressure H2O10.1557/JMR.1986.0100 ↗
93. Corrosion behavior of silicon carbide in 290 °C water10.1111/j.1151-2916.1989.tb06029.x ↗
94. In situ STM observations of the etching of n-Si (111) in NaOH solutions10.1016/0039-6028(92)90814-M ↗
95. Etching of Silicon in NaOH Solutions. Part II. Electrochemical studies of n-Si (111) and (100) and mechanism of the dissolution10.1149/1.2056190 ↗
96. Mechanism of Strength Degradation for Hot Corrosion of alpha-SiC10.1111/j.1151-2916.1986.tb07336.x ↗
97. Pitting corrosion in CVD SiC at 300 °C in deoxygenated high-purity water10.1016/j.jnucmat.2008.03.025 ↗
98. Corrosion of CVD Silicon Carbide in 500 °C Supercritical Water10.1111/j.1551-2916.2006.01401.x ↗
99. Corrosion behavior of reaction-bonded silicon carbide ceramics in high-temperature water10.1023/A:1015797324658 ↗
100. Long-term corrosion behavior of CVD SiC in 360 °C water and 400 °C steam10.1016/j.jnucmat.2013.07.058 ↗