Abstract
Prelithiation has been widely accepted as one of the most promising strategies to compensate for the loss of active substance and to improve the initial Coulombic efficiency in silicon-based anodes for advanced high-energy-density batteries. But because of their unstable solid electrolyte interface (SEI) layer and low initial Coulombic efficiency, they expand in volume during prelithiation and react with moisture, which makes commercialization a difficult process. Herein, we have developed a strategy using lithium bis(fluorosulfonyl)imide (LiFSI) treatment to eliminate redundant lithium and generate LiF-based inorganic compounds on the surface of the prelithiated electrode. Such method not only reduces the reactiveness of the prelithiated anode but also enhances the ionic conductivity of the SEI. The rich LiF surface works as an artificial SEI, and according to electrochemical evaluation, the initial Coulombic efficiency of the prelithiated silicon anode treated with LiFSI can reach 92.9%. This technique not only increases the battery’s energy density but also its cycle stability, resulting in superior capacity retention and a longer cycling life.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Metallurgy and Environment, Central South University, Changsha 410083, China
School of Chemistry and Materials Science, Nanjing University of Information Science and Technology, Nanjing 210044, China
Australian Centre for Advanced Photovoltaics, School of Photovoltaic and Renewable Energy Engineering, University of New South Wales, Kensington, NSW 2052, Australia
References (29)
Show source-provided references
1. 25th Anniversary Article: Understanding the Lithiation of Silicon and Other Alloying Anodes for Lithium-Ion Batteries10.1002/adma.201301795 ↗
2. High-performance lithium battery anodes using silicon nanowires10.1038/nnano.2007.411 ↗
3. Nonaqueous Liquid Electrolytes for Lithium-Based Rechargeable Batteries10.1021/cr030203g ↗
4. Examining Solid Electrolyte Interphase Formation on Crystalline Silicon Electrodes: Influence of Electrochemical Preparation and Ambient Exposure Conditions10.1021/jp307372m ↗
5. Running out of lithium? A route to differentiate between capacity losses and active lithium losses in lithium-ion batteries10.1039/C7CP05405J ↗
6. Prelithiation: A Crucial Strategy for Boosting the Practical Application of Next-Generation Lithium Ion Battery10.1021/acsnano.0c10664 ↗
7. Challenges of prelithiation strategies for next generation high energy lithium-ion batteries10.1016/j.ensm.2022.02.005 ↗
8. Overcoming Chemical and Mechanical Instabilities in Lithium Metal Anodes with Sustainable and Eco-Friendly Artificial SEI Layer10.1002/adma.202407381 ↗
9. In Situ Prelithiation by Direct Integration of Lithium Mesh into Battery Cells10.1021/acs.nanolett.3c00859 ↗
10. Generation and Evolution of the Solid Electrolyte Interphase of Lithium-Ion Batteries10.1016/j.joule.2019.08.018 ↗
11. Lv, X., Liu, J., Li, C., Yu, F., Xiao, D., Zhao, S., Wu, Y., and Chen, Y. (2024). Probing a solid electrolyte interphase layer with sub-nanometer pores using redox mediators. eScience, in press.10.1016/j.esci.2024.100351 ↗
12. Sustainable Prelithiation Strategy: Enhancing Energy Density and Lifespan with Ultrathin Li-Mg-Al Alloy Foil10.1002/aenm.202304097 ↗
13. Fluorinating solid electrolyte interphase by regulating polymer–solvent interaction in lithium metal batteries10.1016/j.ensm.2023.102799 ↗
14. Tuning Reaction Kinetics of Fluorinated Molecules to Construct Robust Solid Electrolyte Interphases on SiOx Anode10.1002/anie.202413927 ↗
15. Effect of LiFSI Concentrations To Form Thickness- and Modulus-Controlled SEI Layers on Lithium Metal Anodes10.1021/acs.jpcc.8b02314 ↗
16. A comprehensive review of pre-lithiation/sodiation additives for Li-ion and Na-ion batteries10.1016/j.jechem.2022.10.001 ↗
17. Quantification of Inactive Lithium and Solid–Electrolyte Interphase Species on Graphite Electrodes after Fast Charging10.1021/acsenergylett.0c00859 ↗
18. Artificial Solid Electrolyte Interphase-Protected LixSi Nanoparticles: An Efficient and Stable Prelithiation Reagent for Lithium-Ion Batteries10.1021/jacs.5b04526 ↗
19. Pre-Lithiation Strategies for Next-Generation Practical Lithium-Ion Batteries10.1002/advs.202005031 ↗
20. In Situ Construction of Specific SEI Layer Affords Effective Prelithiation10.1021/acsami.4c07895 ↗
21. Artificial Electron Channels Enable Contact Prelithiation of Li-Ion Battery Anodes with Ultrahigh Li-Source Utilization10.1002/anie.202413926 ↗
22. Insights into Electrolytic Pre-Lithiation: A Thorough Analysis Using Silicon Thin Film Anodes10.1002/smll.202206092 ↗
23. Prelithiation strategies for enhancing the performance of lithium-ion batteries10.1039/D4RA08234F ↗
24. Progress and challenges of prelithiation technology for lithium-ion battery10.1002/cey2.256 ↗
25. Promises and Challenges of the Practical Implementation of Prelithiation in Lithium-Ion Batteries10.1002/aenm.202101565 ↗
26. Hydroxylated Graphene-Sulfur Nanocomposites for High-Rate Lithium-Sulfur Batteries10.1002/aenm.201201080 ↗
27. Pitaya-inspired Li Metal-free Prelithiation of silicon monoxide into anode materials for Li-ion batteries10.1016/j.electacta.2024.143814 ↗
28. Degradation and Speciation of Li Salts during XPS Analysis for Battery Research10.1021/acsenergylett.2c01587 ↗
29. Breathing parylene-based nanothin artificial SEI for highly-stable long life three-dimensional silicon lithium-ion batteries10.1016/j.cej.2021.132077 ↗