journal article·2020-09-14Open access

Three-Step Description of Single-Pulse Formation of Laser-Induced Periodic Surface Structures on Metals

Evgeny L. Gurevich, Yoann Levy, Nadezhda M. Bulgakova

Nanomaterials· Volume 10· Issue 9

Abstract

Two different scenarios are usually invoked in the formation of femtosecond Laser-Induced Periodic Surface Structures (LIPSS), either “self-organization” mechanisms or a purely “plasmonic” approach. In this paper, a three-step model of formation of single-laser-shot LIPSS is summarized. It is based on the periodic perturbation of the electronic temperature followed by an amplification, for given spatial periods, of the modulation in the lattice temperature and a final possible relocation by hydrodynamic instabilities. An analytical theory of the evolution of the temperature inhomogeneities is reported and supported by numerical calculations on the examples of three different metals: Al, Au, and Mo. The criteria of the possibility of hydrodynamic instabilities are also discussed.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Laser Material Processing Techniques · nanoparticles nucleation surface interactions · Laser-induced spectroscopy and plasma

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

University of Applied Sciences Münster, Laser Center (LFM), Stegerwaldstraße 39, 48565 Steinfurt, Germany

HiLASE Centre, Institute of Physics of the Czech Academy of Sciences, Za Radnicí 828, 2524 Dolní Břežany, Czech Republic

Funding

European Regional Development Fund

References (51)

Show source-provided references
1. Semiconductor Surface Damage Produced by Ruby Lasers10.1063/1.1703071 ↗
2. Assessment and Formation Mechanism of Laser-Induced Periodic Surface Structures on Polymer Spin-Coated Films in Real and Reciprocal Space10.1021/la200451c ↗
3. Femtosecond laser induced periodic surface structures on multi-layer graphene10.1063/1.4902950 ↗
4. Simultaneous nanopatterning and reduction of graphene oxide by femtosecond laser pulses10.1016/j.apsusc.2018.03.086 ↗
5. Modification of dielectric surfaces with ultra-short laser pulses10.1016/S0169-4332(01)00675-4 ↗
6. Self-organized pattern formation upon femtosecond laser ablation by circularly polarized light10.1016/j.apsusc.2005.08.120 ↗
7. Gräf, S., Kunz, C., Engel, S., Derrien, T., and Müller, F. (2018). Femtosecond Laser-Induced Periodic Surface Structures on Fused Silica: The Impact of the Initial Substrate Temperature. Materials, 11.10.3390/ma11081340 ↗
8. Laser mirror damage in germanium at 10.6 μm10.1063/1.1654761 ↗
9. Laser-induced periodic surface structure. I. Theory10.1103/PhysRevB.27.1141 ↗
10. Interaction of powerful laser radiation with the surfaces of semiconductors and metals: Nonlinear optical effects and nonlinear optical diagnostics10.1070/PU1985v028n12ABEH003986 ↗
11. On the role of surface plasmon polaritons in the formation of laser-induced periodic surface structures upon irradiation of silicon by femtosecond-laser pulses10.1063/1.3261734 ↗
12. Mechanisms of femtosecond LIPSS formation induced by periodic surface temperature modulation10.1016/j.apsusc.2015.09.091 ↗
13. Self-organization of thin metal films by irradiation with nanosecond laser pulses10.1016/j.apsusc.2009.04.099 ↗
14. Plasmonic and Hydrodynamic Effects in Ultrafast Laser-Induced Periodic Surface Structures on Metals10.2961/jlmn.2012.03.0023 ↗
15. Atomistic modeling of nanoparticle generation in short pulse laser ablation of thin metal films in water10.1016/j.jcis.2016.10.029 ↗
16. Relaxation dynamics of femtosecond-laser-induced temperature modulation on the surfaces of metals and semiconductors10.1016/j.apsusc.2015.10.159 ↗
17. Role of the temperature dynamics in formation of nanopatterns upon single femtosecond laser pulses on gold10.1103/PhysRevB.95.054305 ↗
18. Wavelength dependence of picosecond laser-induced periodic surface structures on copper10.1016/j.apsusc.2017.02.068 ↗
19. Laser-induced modification of transparent crystals and glasses10.1070/QE2010v040n11ABEH014445 ↗
20. Rippled area formed by surface plasmon polaritons upon femtosecond laser double-pulse irradiation of silicon: The role of carrier generation and relaxation processes10.1007/s00339-013-8205-2 ↗
21. On a Remarkable Case of Uneven Distribution of Light in a Diffraction Grating Spectrum10.1088/1478-7814/18/1/325 ↗
22. Note on the remarkable case of diffraction spectra described by Prof. Wood10.1080/14786440709463661 ↗
23. The Theory of Anomalous Diffraction Gratings and of Quasi-Stationary Waves on Metallic Surfaces (Sommerfeld’s Waves)10.1364/JOSA.31.000213 ↗
24. Laser Induced Periodic Surface Structures induced by surface plasmons coupled via roughness10.1016/j.apsusc.2013.10.141 ↗
25. Laser-induced surface relief nanocrowns as a manifestation of nanoscale Rayleigh-Plateau hydrodynamic instability10.1016/j.apsusc.2020.145463 ↗
26. Ablation with femtosecond pulses: The effect of temporal contrast10.1016/j.apsusc.2007.02.105 ↗
27. High-speed manufacturing of highly regular femtosecond laser-induced periodic surface structures: Physical origin of regularity10.1038/s41598-017-08788-z ↗
28. Efficiency of local surface plasmon polariton excitation on ridges10.1103/PhysRevB.78.115115 ↗
29. Excitation of surface plasmon polaritons on silicon with an intense femtosecond laser pulse10.1103/PhysRevB.96.045122 ↗
30. Reduced damping of surface plasmon polaritons on silicon with intense femtosecond laser pulse10.7567/1347-4065/ab13db ↗
31. Selected problems of laser ablation theory10.1070/PU2002v045n03ABEH000966 ↗
32. Levy, Y., Bulgakova, N.M., and Mocek, T. Laser-Induced Periodic Surface Structures Formation: Investigation of the Effect of Nonlinear Absorption of Laser Energy in Different Materials, Proc. SPIE 10228, Nonlinear Optics and Applications X.
33. The role of electron-phonon coupling in femtosecond laser damage of metals
34. Electron-Phonon Coupling and Electron Heat Capacity in Metals at High Electron Temperatures10.1103/PhysRevB.77.075133 ↗
35. Bäuerle, D. (2011). Laser Processing and Chemistry, Springer.10.1007/978-3-642-17613-5 ↗
36. Ultrafast dynamics of nonequilibrium electrons in metals under femtosecond laser irradiation10.1103/PhysRevB.65.214303 ↗
37. Palik, E.D. (1985). Handbook of Optical Constants of Solids, Academic Press.
38. Strogatz, S. (1994). Nonlinear Dynamics and Chaos: With Applications to Physics, Biology, Chemistry, and Engineering, Westview Press. Advanced Book Program.
39. Application of a two-temperature model for the investigation of the periodic structure formation on Si surface in femtosecond laser interaction
40. Influence of surface plasmon polaritons on laser energy absorption and structuring of surfaces10.1016/j.apsusc.2019.144420 ↗
41. Electron-Ion Relaxation, Phase Transitions, and Surface Nano-Structuring Produced by Ultrashort Laser Pulses in Metals10.1002/ctpp.201310049 ↗
42. Mechanism of single-pulse ablative generation of laser-induced periodic surface structures10.1103/PhysRevB.96.205429 ↗
43. Self-Arranged Periodic Nanovoids by Ultrafast Laser-Induced Near-Field Enhancement10.1021/acsphotonics.7b01438 ↗
44. Spallation-induced roughness promoting high spatial frequency nanostructure formation on Cr10.1007/s00339-018-1716-0 ↗
45. Long-scale evolution of thin liquid films10.1103/RevModPhys.69.931 ↗
46. Fefferman, C.L. (2006). Existence and Smoothness of the Navier–Stokes Equation. The Millennium Prize Problems, Clay Math. Inst.
47. Thermocapillary instabilities10.1146/annurev.fl.19.010187.002155 ↗
48. High-frequency periodic patterns driven by non-radiative fields coupled with Marangoni convection instabilities on laser-excited metal surfaces10.1016/j.actamat.2020.04.058 ↗
49. Coherent structures in ablatively compressed ICF targets and Rayleigh-Taylor instability10.1088/0031-8949/1996/T63/024 ↗
50. Measurement of Feedthrough and Instability Growth in Radiation-Driven Cylindrical Implosions10.1103/PhysRevLett.78.3876 ↗
51. On the physics of self-organized nanostructure formation upon femtosecond laser ablation10.1007/s00339-014-8339-x ↗