journal article·2016-12

Observing the evolution of graphene layers at high current density

Chun-Wei Huang, Jui-Yuan Chen, Chung-Hua Chiu, Cheng-Lun Hsin, Tseung-Yuen Tseng, Wen-Wei Wu

Nano Research· Volume 9· Issue 12
Publisher page

Abstract

Graphene has demonstrated its potential in several practical applications owing to its remarkable electronic and physical properties. In this study, we successfully fabricated a suspended graphene device with a width down to 20 nm. The morphological evolution of graphene under various electric field effects was systematically examined using an in-situ transmission electron microscope (TEM). The hourglass-shaped graphene sample instantly broke apart at 7.5 mA, indicating an impressive breakdown current density. The current-carrying capacity was calculated to be ~1.6 × 109 A·cm–2, which is several orders higher than that of copper. The current-carrying capacity depended on the resistivity of graphene. In addition, atomic volume changes occurred in the multilayer graphene samples due to surface diffusion and Ostwald ripening (OR), indicating that the breakdown mechanism is well approximated by the electric field. This study not only provides a theory to explain the breakdown behavior but also presents the effects on materials contacted with a graphene layer used as the transmission path.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Graphene research and applications · Advancements in Battery Materials · Low-power high-performance VLSI design

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Wu, Y. Q.; Lin, Y. M.; Bol, A. A.; Jenkins, K. A.; Xia, F. N.; Farmer, D. B.; Zhu, Y.; Avouris, P. High-frequency, scaled graphene transistors on diamond-like carbon. Nature 2011, 472, 74–78.10.1038/nature09979 ↗
2. Lu, Y.; Goldsmith, B. R.; Kybert, N. J.; Johnson, A. T. C. DNA-decorated graphene chemical sensors. Appl. Phys. Lett. 2010, 97, 083107.
3. Bae, S.; Kim, H.; Lee, Y.; Xu, X. F.; Park, J. S.; Zheng, Y.; Balakrishnan, J.; Lei, T.; Ri Kim, H.; Song, Y. I. et al. Roll-to-roll production of 30-inch graphene films for transparent electrodes. Nat. Nanotechnol. 2010, 5, 574–578.10.1038/nnano.2010.132 ↗
4. Merchant, C. A.; Healy, K.; Wanunu, M.; Ray, V.; Peterman, N.; Bartel, J.; Fischbein, M. D.; Venta, K.; Luo, Z. T.; Johnson, A. T. C.; Drndic, M. DNA translocation through graphene nanopores. Nano Lett. 2010, 10, 2915–2921.10.1021/nl101046t ↗
5. Schneider, G. F.; Kowalczyk, S. W.; Calado, V. E.; Pandraud, G.; Zandbergen, H. W.; Vandersypen, L. M. K.; Dekker, C. DNA translocation through graphene nanopores. Nano Lett. 2010, 10, 3163–3167.10.1021/nl102069z ↗
6. Garaj, S.; Hubbard, W.; Reina, A.; Kong, J.; Branton, D.; Golovchenko, J. A. Graphene as a subnanometre transelectrode membrane. Nature 2010, 467, 190–193.10.1038/nature09379 ↗
7. Li, X. S.; Zhu, Y. W.; Cai, W. W.; Borysiak, M.; Han, B. Y.; Chen, D.; Piner, R. D.; Colombo, L.; Ruoff, R. S. Transfer of large-area graphene films for high-performance transparent conductive electrodes. Nano Lett. 2009, 9, 4359–4363.10.1021/nl902623y ↗
8. Xia, F. N.; Mueller, T.; Lin, Y. M.; Valdes-Garcia, A.; Avouris, P. Ultrafast graphene photodetector. Nat. Nanotechnol. 2009, 4, 839–843.10.1038/nnano.2009.292 ↗
9. Bolotin, K. I.; Sikes, K. J.; Jiang, Z.; Klima, M.; Fudenberg, G.; Hone, J.; Kim, P.; Stormer, H. L. Ultrahigh electron mobility in suspended graphene. Solid State Commun. 2008, 146, 351–355.10.1016/j.ssc.2008.02.024 ↗
10. Wang, X. R.; Ouyang, Y. J.; Li, X. L.; Wang, H. L.; Guo, J.; Dai, H. J. Room-temperature all-semiconducting sub-10-nm graphene nanoribbon field-effect transistors. Phys. Rev. Lett. 2008, 100, 206803.10.1103/PhysRevLett.100.206803 ↗
11. Lu, Y.; Merchant, C. A.; Drndic, M.; Johnson, A. T. C. In situ electronic characterization of graphene nanoconstrictions fabricated in a transmission electron microscope. Nano Lett. 2011, 11, 5184–5188.10.1021/nl2023756 ↗
12. Barreiro, A.; Börrnert, F.; Rümmeli, M. H.; Büchner, B.; Vandersypen, L. M. K. Graphene at high bias: Cracking, layer by layer sublimation, and fusing. Nano Lett. 2012, 12, 1873–1878.10.1021/nl204236u ↗
13. Baringhaus, J.; Ruan, M.; Edler, F.; Tejeda, A.; Sicot, M.; Taleb-Ibrahimi, A.; Li, A.-P.; Jiang, Z. G.; Conrad, E. H.; Berger, C. et al. Exceptional ballistic transport in epitaxial graphene nanoribbons. Nature 2014, 506, 349–354.10.1038/nature12952 ↗
14. Han, M. Y.; Özyilmaz, B.; Zhang, Y. B.; Kim, P. Energy band-gap engineering of graphene nanoribbons. Phys. Rev. Lett. 2007, 98, 206805.10.1103/PhysRevLett.98.206805 ↗
15. Pospischil, A.; Humer, M.; Furchi, M. M.; Bachmann, D.; Guider, R.; Fromherz, T.; Mueller, T. CMOS-compatible graphene photodetector covering all optical communication bands. Nat. Photonics 2013, 7, 892–896.10.1038/nphoton.2013.240 ↗
16. Li, X. L.; Wang, X. R.; Zhang, L.; Lee, S.; Dai, H. J. Chemically derived, ultrasmooth graphene nanoribbon semiconductors. Science 2008, 319, 1229–1232.10.1126/science.1150878 ↗
17. Ponomarenko, L. A.; Schedin, F.; Katsnelson, M. I.; Yang, R.; Hill, E. W.; Novoselov, K. S.; Geim, A. K. Chaotic dirac billiard in graphene quantum dots. Science 2008, 320, 356–358.10.1126/science.1154663 ↗
18. Murali, R.; Yang, Y. X.; Brenner, K.; Beck, T.; Meindl, J. D. Breakdown current density of graphene nanoribbons. Appl. Phys. Lett. 2009, 94, 243114.10.1063/1.3147183 ↗
19. Chen, K. C.; Wu, W. W.; Liao, C. N.; Chen, L. J.; Tu, K. N. Observation of atomic diffusion at twin-modified grain boundaries in copper. Science 2008, 321, 1066–1069.10.1126/science.1160777 ↗
20. Chen, L. J.; Wu, W. W. In situ TEM investigation of dynamical changes of nanostructures. Mat. Sci. Eng. R 2010, 70, 303–319.10.1016/j.mser.2010.06.014 ↗
21. Chen, J. Y.; Huang, C. W.; Chiu, C. H.; Huang, Y. T.; Wu, W. W. Switching kinetic of VCM-based memristor: Evolution and positioning of nanofilament. Adv. Mater. 2015, 27, 5028–5033.10.1002/adma.201502758 ↗
22. Huang, Y. T.; Huang, C. W.; Chen, J. Y.; Ting, Y. H.; Lu, K. C.; Chueh, Y. L.; Wu, W. W. Dynamic observation of phase transformation behaviors in indium(III) selenide nanowire based phase change memory. ACS Nano 2014, 8, 9457–9462.10.1021/nn503576x ↗
23. Huang, C. W.; Chen, J. Y.; Chiu, C. H.; Wu, W. W. Revealing controllable nanowire transformation through cationic exchange for RRAM application. Nano Lett. 2014, 14, 2759–2763.10.1021/nl500749q ↗
24. Chen, J. Y.; Hsin, C. L.; Huang, C. W.; Chiu, C. H.; Huang, Y. T.; Lin, S. J.; Wu, W. W.; Chen, L. J. Dynamic evolution of conducting nanofilament in resistive switching memories. Nano Lett. 2013, 13, 3671–3677.10.1021/nl4015638 ↗
25. Hsin, C. L.; Huang, C. W.; Chen, J. Y.; Liao, K. C.; Liu, P. L.; Wu, W. W.; Chen, L. J. Direct observation of sublimation behaviors in one-dimensional In2Se3/In2O3 nanoheterostructures. Anal. Chem. 2015, 87, 5584–5588.10.1021/acs.analchem.5b00255 ↗
26. Huang, C. W.; Hsin, C. L.; Wang, C. W.; Chu, F. H.; Kao, C. Y.; Chen, J. Y.; Huang, Y. T.; Lu, K. C.; Wu, W. W.; Chen, L. J. Direct observation of melting behaviors at the nanoscale under electron beam and heat to form hollow nanostructures. Nanoscale 2012, 4, 4702–4706.10.1039/c2nr30724c ↗
27. Chen, K. C.; Liao, C. N.; Wu, W. W.; Chen, L. J. Direct observation of electromigration induced surface atomic steps in Cu lines by in situ transmission electron microscopy. Appl. Phys. Lett. 2007, 90, 203101.10.1063/1.2740109 ↗
28. Liu, X. F.; Xu, T.; Wu, X.; Zhang, Z. H.; Yu, J.; Qiu, H.; Hong, J. H.; Jin, C. H.; Li, J. X.; Wang, X. R. et al. Top-down fabrication of sub-nanometre semiconducting nanoribbons derived from molybdenum disulfide sheets. Nat. Commun. 2013, 4, 1776.10.1038/ncomms2803 ↗
29. Xu, T.; Yin, K. B.; Xie, X.; He, L. B.; Wang, B. J.; Sun, L. T. Size-dependent evolution of graphene nanopores under thermal excitation. Small 2012, 8, 3422–3426.10.1002/smll.201200979 ↗
30. Ferrari, A. C.; Meyer, J. C.; Scardaci, V.; Casiraghi, C.; Lazzeri, M.; Mauri, F.; Piscanec, S.; Jiang, D.; Novoselov, K. S.; Roth, S. et al. Raman spectrum of graphene and graphene layers. Phys. Rev. Lett. 2006, 97, 187401.10.1103/PhysRevLett.97.187401 ↗
31. Börrnert, F.; Barreiro, A.; Wolf, D.; Katsnelson, M. I.; Büchner, B.; Vandersypen, L. M. K.; Rümmeli, M. H. Lattice expansion in seamless bilayer graphene constrictions at high bias. Nano Lett. 2012, 12, 4455–4459.10.1021/nl301232t ↗
32. Jia, X. T.; Hofmann, M.; Meunier, V.; Sumpter, B. G.; Campos-Delgado, J.; Romo-Herrera, J. M.; Son, H.; Hsieh, Y. P.; Reina, A.; Kong, J. et al. Controlled formation of sharp zigzag and armchair edges in graphitic nanoribbons. Science 2009, 323, 1701–1705.10.1126/science.1166862 ↗
33. Wang, X.; Zhi, L. J.; Müllen, K. Transparent, conductive graphene electrodes for dye-sensitized solar cells. Nano Lett. 2008, 8, 323–327.10.1021/nl072838r ↗
34. Zhang, X. T.; Sui, Z. Y.; Xu, B.; Yue, S. F.; Luo, Y. J.; Zhan, W. C.; Liu, B. Mechanically strong and highly conductive graphene aerogel and its use as electrodes for electrochemical power sources. J. Mater. Chem. 2011, 21, 6494–6497.10.1039/c1jm10239g ↗
35. Ostwald, W. Studien über die bildung und umwandlung fester Körper. 1. Abhandlung: Übersättigung und Überkaltung. Z. Phys. Chem. 1897, 22, 289–330.10.1515/zpch-1897-2233 ↗
36. Hannon, J. B.; Kodambaka, S.; Ross, F. M.; Tromp, R. M. The influence of the surface migration of gold on the growth of silicon nanowires. Nature 2006, 440, 69–71.10.1038/nature04574 ↗