Abstract

Regarding to the problems of low electrical conductivity and slow redox kinetics in Zn-S batteries, it is extremely urgent to find a simple and effective construction strategy. Herein, a conversion cathode material (SxI, x = 9.3, 1) was prepared by bonding commercial sulfur and iodine. Compared with commercial sulfur, the conductivity of SxI are increased by 7 orders of magnitude. Density functional theory (DFT) calculated results show that new S-I chemical bonds are formed in SxI materials, the band gaps are significantly reduced. Their charge-discharge voltage differences, the differential capacity curves and the redox peak potential difference of sulfur are significantly reduced. In the voltage window of 1.20-1.40 V, the I0/I- reversible redox reaction can provide additional capacity contribution of 38.36 mAh g-1. At the current density of 1.5 A g-1, the capacity of S9.3I could reach up to 370.32 mAh g-1 and SI could reach up to 220.04 mAh g-1. SxI materials have a lower degree of polarization, a smaller Tafel slope and activation energies. The in-situ ultraviolet-visible spectroscopy results indicate that the dissociation of the Zn-S bond during the charging process is mainly due to the interaction between I- and the ZnS surface, promoting the rapid conversion of I3- to I-. This work presents a paradigm for effectively enhancing the conductivity of sulfur cathode materials, increasing additional capacity and catalyzing sulfur conversion reactions, thereby significantly improving the performance of Zn-S batteries.
Source: openalex_inverted_index · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced battery technologies research · Electrocatalysts for Energy Conversion · Gas Sensing Nanomaterials and Sensors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. D. Patel. Minireview on aqueous zinc–sulfur batteries: Recent advances and future perspectives. 2023, 37: 10897-10914.10.1021/acs.energyfuels.3c01938 ↗
2. H. T. Xu. Advances in aqueous zinc ion batteries based on conversion mechanism: Challenges, strategies, and prospects. 2024, 20: 2310972.10.1002/smll.202310972 ↗
3. X. Y. Nie. Cholinium cations enable highly compact and dendrite-free Zn metal anodes in aqueous electrolytes. 2022, 32: 2203905.10.1002/adfm.202203905 ↗
4. X. Wang. High energy density aqueous zinc–chalcogen (S, Se, Te) batteries: Recent progress, challenges, and perspective. 2023, 13: 2302927.10.1002/aenm.202302927 ↗
5. J. J. Chen. Suppression of hydrogen evolution reaction by modulating the surface redox potential toward long-life zinc metal anodes. 2024, 34: 2312564.10.1002/adfm.202312564 ↗
6. N. Gao. Elimination of concentration polarization under ultra-high current density zinc deposition by nanofluid self-driven ion enrichment. 2025, 37: 2419034.10.1002/adma.202419034 ↗
7. K. N. Wang. Coupling oxygen vacancies and heterophase homostructure achieving high-rate-endurable aqueous zinc-ion storage. 2023, 11: 15818-15825.10.1021/acssuschemeng.3c03636 ↗
8. J. W. Wang. Dual modulation of homogeneous nanomaterialization and electrochemical activation enhancing zinc ion storage. 2025, 68: 385-393.10.1007/s11426-024-2166-7 ↗
9. Y. X. Zeng. Construction of Co–Mn Prussian blue analog hollow spheres for efficient aqueous Zn-ion batteries. 2021, 60: 22189-22194.10.1002/anie.202107697 ↗
10. C. L. Feng. Recent advances in aqueous zinc–sulfur batteries: Overcoming challenges for sustainable energy storage. 2023, 11: 18029-18045.10.1039/D3TA03338D ↗
11. H. Zhang. Internal electron donor accelerated sulfur redox for aqueous Zn–S batteries. 2024, 34: 2406125.10.1002/adfm.202406125 ↗
12. D. Yan. Tactics to optimize conversion-type metal fluoride/sulfide/oxide cathodes toward advanced lithium metal batteries. 2023, 16: 8173-8190.10.1007/s12274-023-5427-7 ↗
13. J. M. Kang. An overview of aqueous zinc-ion batteries based on conversion-type cathodes. 2022, 2: 200009.10.20517/energymater.2022.05 ↗
14. Y. N. Cao. Recent progress in aqueous zinc-ion batteries based on conversion-type cathodes. 2025, 4: 100278.10.1016/j.apmate.2025.100278 ↗
15. X. Liu. Rechargeable metal (Li, Na, Mg, Al)–sulfur batteries: Materials and advances. 2021, 61: 104-134.10.1016/j.jechem.2021.02.028 ↗
16. D. Patel. Hybrid electrolyte with biomass-derived carbon host for high-performance aqueous Zn–S battery. 2024, 479: 147722.10.1016/j.cej.2023.147722 ↗
17. L. Xu. Pitch-derived multifunctional carbon and bimetallic sulfide composite electrodes for aqueous energy storage. 2025, 1010: 177957.10.1016/j.jallcom.2024.177957 ↗
18. K. N. Wang. Pitch-derived 3D amorphous carbon encapsulated sulfur-rich cathode for aqueous Zn–S batteries. 2023, 66: 2711-2718.10.1007/s11426-023-1711-x ↗
19. W. W. Zhang. Bidirectional atomic iron catalysis of sulfur redox conversion in high-energy flexible Zn–S battery. 2023, 33: 2210899.10.1002/adfm.202210899 ↗
20. W. Zong. Dynamical Janus interface design for reversible and fast-charging zinc-iodine battery under extreme operating conditions. 2024, 146: 21377-21388.10.1021/jacs.4c03615 ↗
21. W. Li. A low cost aqueous Zn–S battery realizing ultrahigh energy density. 2020, 7: 2000761.10.1002/advs.202000761 ↗
22. S. Mehta. Unleashing ultrahigh capacity and lasting stability: Aqueous zinc-sulfur batteries. 2024, 14: 2401515.10.1002/aenm.202401515 ↗
23. H. Y. Zhao. Highly electrically conductive polyiodide ionic liquid cathode for high-capacity dual-plating zinc-iodine batteries. 2024, 146: 6744-6752.10.1021/jacs.3c12695 ↗
24. R. Wang. Remolding the interface stability for practical aqueous Zn/I 2 batteries via sulfonic acid‐rich electrolyte and separator design. 2025, 37: 2419502.10.1002/adma.202419502 ↗
25. L. J. Zhang. Chain breakage in the supercooled liquid–liquid transition and re-entry of the λ -transition in sulfur. 2018, 8: 4558.10.1038/s41598-018-22775-y ↗
26. S. B. Zeng. Highly crosslinked organosulfur copolymer nanosheets with abundant mesopores as cathode materials for efficient lithium–sulfur batteries. 2018, 263: 53-59.10.1016/j.electacta.2017.12.179 ↗
27. A. G. Prabhudessai. Correlation between Raman spectroscopy and mechanical properties of As–Sb–S–I chalcogenide glasses. 2019, 507: 56-65.10.1016/j.jnoncrysol.2018.10.016 ↗
28. J. B. Zhou. Healable and conductive sulfur iodide for solid-state Li–S batteries. 2024, 627: 301-305.10.1038/s41586-024-07101-z ↗
29. P. Hei. Facilitating the electrochemical oxidation of ZnS through iodide catalysis for aqueous zinc-sulfur batteries. 2024, 63: e202316082.10.1002/anie.202316082 ↗
30. W. L. Wu. A dual-mediator for a sulfur cathode approaching theoretical capacity with low overpotential in aqueous Zn–S batteries. 2023, 16: 4326-4333.10.1039/D3EE01749D ↗
31. T. S. Zhang. Redox mediator chemistry regulated aqueous batteries: Insights into mechanisms and prospects. 2022, 4: 2874-2887.10.31635/ccschem.022.202202125 ↗
32. M. W. Cui. I 3 − /I − redox reaction-mediated organic zinc-air batteries with accelerated kinetics and long shelf lives. 2023, 62: e202303845.10.1002/anie.202303845 ↗
33. Y. Z. Li. ZnS/MoS 2 heterostructures on MXene: A strategy for improved polysulfide adsorption and conversion in Li–S batteries. 2024, 502: 158151.10.1016/j.cej.2024.158151 ↗
34. Y. Zhu. Screened d-p orbital hybridization in turing structure of confined nickel for sulfion oxidation accelerated hydrogen production. 2025, 64: e202419572.10.1002/anie.202419572 ↗
35. H. L. Jiang. Constructing highly active sulfur atoms on MoS 2 surface via p–p orbital covalent coupling matching the liquid–solid transition in lithium–sulfur batteries. 2025, 77: 104203.10.1016/j.ensm.2025.104203 ↗
36. Y. R. Zhu. Anion vacancies coupling with heterostructures enable advanced aerogel cathode for ultrafast aqueous zinc-ion storage. 2025, 37: 2419582.10.1002/adma.202419582 ↗
37. Y. F. Guo. Engineering electrolyte network structure for improved kinetics and dendrite suppression in Zn–S batteries. 2025, 64: e202422047.10.1002/anie.202422047 ↗
38. Y. X. Li. Multi-site high-entropy immobilizer for all-iodine species fixation in high-performance zinc-iodine batteries. 2025, 35: 2419821.10.1002/adfm.202419821 ↗
39. P. F. Zhang. Toward shuttle-free Zn–I 2 battery: Anchoring and catalyzing iodine conversion by high-density P-doping sites in carbon host. 2024, 34: 2306359.10.1002/adfm.202306359 ↗
40. D. D. Yin. Polymeric iodine transport layer enabled high areal capacity dual plating zinc-iodine battery. 2025, 64: e202418069.10.1002/anie.202418069 ↗