Understanding and regulation of stress‐induced structural evolution in silicon anodes for high-energy-density batteries

Xiangrui Duan, Yangtao Ou, Shuibin Tu, Wenyu Wang, Hengtao Shen, Guocheng Li, Yuanjian Li, Junjie Fu, Ruikang Feng, Renming Zhan, Yongming Sun

Nano Research· Volume 19· Issue 10

Abstract

Abstract Silicon (Si)-based electrodes are widely regarded as a promising anode option for next-generation high-energy batteries. Although the substantial volume expansion during charge/discharge cycles is recognized as a primary cause of Si-based anode failure, the correlation between material volume changes, electrode-scale electrochemical-mechanical behavior, and electrochemical performance remains unclear. This poses a significant obstacle to the design of high-performance Si-based anodes. Herein, by combining operando detection of spatial stress in pouch cells (8 cm × 8 cm) with materials characterization, we elucidate the dependence of electrochemical performance on the inner stress-driven structural evolution of Si-based anodes, where large, uneven stress/strain dominates their mechanical degradation, compromising electrochemical reversibility. Significantly, we unveil that, beyond the basic function of Li compensation, prelithiation redirects the stress-induced structural evolution of the electrode from pore and crack formation to a void-filling-dominated process, effectively mitigating volume changes and reaction inhomogeneity. With ~ 25% prelithiation degree of the anode, LiCoO2||Si/C pouch cells, featuring an anode specific capacity of ~ 1300 mAh·g−1 and areal capacity of ~ 2.3 mAh·cm−2, deliver a remarkable reduction in anode porosity of 14.4% during the initial charge, in contrast to a 5.4% increase in the unprelithiated counterpart. Synchronously, electrode swelling diminishes from over 153% to below 18%. Harnessing this favorable electrochemical-mechanical behavior, the pouch cell delivers a 27.1% improvement in capacity retention after 200 cycles at 0.5 C, outside of a 90.4% increase in cumulative discharge capacity.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Molten salt chemistry and electrochemical processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. S. Choi. Highly elastic binders integrating polyrotaxanes for silicon microparticle anodes in lithium ion batteries. 2017, 357: 279-283.10.1126/science.aal4373 ↗
2. Y. Jin. Challenges and recent progress in the development of Si anodes for lithium-ion battery. 2017, 7: 1700715.10.1002/aenm.201700715 ↗
3. Y. Cui. Silicon anodes. 2021, 6: 995-996.10.1038/s41560-021-00918-2 ↗
4. P. L. Yu. Hierarchical yolk-shell silicon/carbon anode materials enhanced by vertical graphene sheets for commercial lithium-ion battery applications. 2025, 35: 2413081.10.1002/adfm.202413081 ↗
5. C. Wang. Self-healing chemistry enables the stable operation of silicon microparticle anodes for high-energy lithium-ion batteries. 2013, 5: 1042-1048.10.1038/nchem.1802 ↗
6. E. Pomerantseva. Energy storage: The future enabled by nanomaterials. 2019, 366: eaan8285.10.1126/science.aan8285 ↗
7. L. H. Ye. Fast cycling of lithium metal in solid-state batteries by constriction-susceptible anode materials. 2024, 23: 244-251.10.1038/s41563-023-01722-x ↗
8. Z. D. Chen. Emerging organic surface chemistry for Si anodes in lithium-ion batteries: Advances, prospects, and beyond. 2022, 12: 2200924.10.1002/aenm.202200924 ↗
9. N. Kim. Issues impeding the commercialization of laboratory innovations for energy-dense Si-containing lithium-ion batteries. 2023, 8: 921-933.10.1038/s41560-023-01333-5 ↗
10. N. Liu. A pomegranate-inspired nanoscale design for large-volume-change lithium battery anodes. 2014, 9: 187-192.10.1038/nnano.2014.6 ↗
11. J. Sung. Subnano-sized silicon anode via crystal growth inhibition mechanism and its application in a prototype battery pack. 2021, 6: 1164-1175.10.1038/s41560-021-00945-z ↗
12. D. X. Xu. Reduced volume expansion of micron-sized SiO x via closed-nanopore structure constructed by Mg-induced elemental segregation. 2024, 63: e202401973.10.1002/anie.202401973 ↗
13. T. W. Kwon. Prospect for supramolecular chemistry in high-energy-density rechargeable batteries. 2019, 3: 662-682.10.1016/j.joule.2019.01.006 ↗
14. J. Lin. Stainless steel-like passivation inspires persistent silicon anodes for lithium-ion batteries. 2023, 62: e202216557.10.1002/anie.202216557 ↗
15. Z. Y. He. The acupuncture effect of carbon nanotubes induced by the volume expansion of silicon-based anodes. 2024, 17: 3358-3364.10.1039/D4EE00710G ↗
16. C. H. Li. Regulating the mechano-electrochemistry of graphite-silicon hybrid anode through layered electrode structure design. 2025, 104: 176-184.10.1016/j.jechem.2024.12.048 ↗
17. A. M. Li. Asymmetric electrolyte design for high-energy lithium-ion batteries with micro-sized alloying anodes. 2024, 9: 1551-1560.10.1038/s41560-024-01619-2 ↗
18. T. Liu. Recycled micro-sized silicon anode for high-voltage lithium-ion batteries. 2024, 7: 1057-1066.10.1038/s41893-024-01393-9 ↗
19. M. Je. Constructing pure Si anodes for advanced lithium batteries. 2023, 56: 2213-2224.10.1021/acs.accounts.3c00308 ↗
20. H. S. Zhao. Si-based anodes: Advances and challenges in Li-ion batteries for enhanced stability. 2024, 7: 11.10.1007/s41918-024-00214-z ↗
21. Z. X. Xiao. Micro-sized CVD-derived Si–C anodes: Challenges, strategies, and prospects for next-generation high-energy lithium-ion batteries. 2025, 18: 4037-4052.10.1039/D5EE01568E ↗
22. G. G. Eshetu. Production of high-energy Li-ion batteries comprising silicon-containing anodes and insertion-type cathodes. 2021, 12: 5459.10.1038/s41467-021-25334-8 ↗
23. C. Ge. Recent Advances in fibrous materials for hydroelectricity generation. 2025, 17: 29.10.1007/s40820-024-01537-8 ↗
24. P. S. Jia. Revisiting the kinetics enhancement strategies of Si anodes through deconstructing particle-interface-electrode integration. 2025, 18: 2720-2746.10.1039/D4EE05595K ↗
25. X. C. Wang. Anode interphase design for fast-charging lithium-based rechargeable batteries. 2025, 18: 2648-2667.10.1039/D4EE06107A ↗
26. Y. Zhang. In operando monitoring the stress evolution of silicon anode electrodes during battery operation via optical fiber sensors. 2024, 20: 2311299.10.1002/smll.202311299 ↗
27. Z. Y. Cao. Metallized polymer current collector as “stress acceptor” for stable micron-sized silicon anodes. 2025, 101: 786-794.10.1016/j.jechem.2024.09.071 ↗
28. A. J. Louli. Operando pressure measurements reveal solid electrolyte interphase growth to rank Li-ion Cell performance. 2019, 3: 745-761.10.1016/j.joule.2018.12.009 ↗
29. R. A. Dressler. Investigation of the failure mechanisms of Li-ion pouch cells with Si/graphite composite negative electrodes and single wall carbon nanotube conducting additive. 2024, 171: 030532.10.1149/1945-7111/ad3398 ↗
30. Y. Koyama. Harnessing the actuation potential of solid-state intercalation compounds. 2006, 16: 492-498.10.1002/adfm.200500633 ↗
31. W. X. Huang. Onboard early detection and mitigation of lithium plating in fast-charging batteries. 2022, 13: 7091.10.1038/s41467-022-33486-4 ↗
32. L. A. Berla. Mechanical behavior of electrochemically lithiated silicon. 2015, 273: 41-51.10.1016/j.jpowsour.2014.09.073 ↗
33. D. H. S. Tan. Carbon-free high-loading silicon anodes enabled by sulfide solid electrolytes. 2021, 373: 1494-1499.10.1126/science.abg7217 ↗
34. B. Hertzberg. Ex-situ depth-sensing indentation measurements of electrochemically produced Si–Li alloy films. 2011, 13: 818-821.10.1016/j.elecom.2011.05.011 ↗
35. R. M. Zhan. Promises and challenges of the practical implementation of prelithiation in lithium-ion batteries. 2021, 11: 2101565.10.1002/aenm.202101565 ↗
36. Y. T. Ou. A salt-free medium facilitating electrode prelithiation towards fast-charging and high-energy lithium-ion batteries. 2025, 16: 7956.10.1038/s41467-025-63257-w ↗
38. Y. S. Ye. Quadruple the rate capability of high-energy batteries through a porous current collector design. 2024, 9: 643-653.10.1038/s41560-024-01473-2 ↗
39. V. Vanpeene. In situ characterization of Si-based anodes by coupling synchrotron X-ray tomography and diffraction. 2019, 56: 799-812.10.1016/j.nanoen.2018.11.079 ↗
40. S. E. Sandoval. Structural and electrochemical evolution of alloy interfacial layers in anode-free solid-state batteries. 2023, 7: 2054-2073.10.1016/j.joule.2023.07.022 ↗
41. Z. Y. Zhang. An all-electrochem-active silicon anode enabled by spontaneous Li–Si alloying for ultra-high performance solid-state batteries. 2024, 17: 1061-1072.10.1039/D3EE03877G ↗
42. J. Chen. Electrolyte design for LiF-rich solid-electrolyte interfaces to enable high-performance microsized alloy anodes for batteries. 2020, 5: 386-397.10.1038/s41560-020-0601-1 ↗
43. K. Cheng. Material-electrolyte interfacial interaction enabling the formation of an inorganic-rich solid electrolyte interphase for fast-charging Si-based lithium-ion batteries. 2024, 17: 2631-2641.10.1039/D4EE00407H ↗
44. M. Bai. An in-situ polymerization strategy for gel polymer electrolyte Si|Ni-rich lithium-ion batteries. 2024, 15: 5375.10.1038/s41467-024-49713-z ↗
45. S. Bai. Elucidating the role of prelithiation in Si-based anodes for interface stabilization. 2023, 13: 2301041.10.1002/aenm.202301041 ↗