journal article·2002-06

Comparison of normal and oblique incidence ultrasonic measurements for the detection of environmental degradation of adhesive joints

K Vine, P Cawley, A.J Kinloch

NDT & E International· Volume 35· Issue 4
Publisher page

Abstract

Abstract Normal and oblique incidence ultrasonic scans have been conducted on two and three layer adhesive joint specimens exposed to water at 50 °C for periods of up to 18 months. The joints consisted of aluminium alloy adherends, which were subjected to one of four different surface pre-treatments prior to being coated (for the two layer specimens) or bonded (for the three layer specimens) with an epoxy polymer. Overall, the oblique incidence technique detected the same types of defect as the normal incidence scans, except when the resolution was too poor to detect the smallest defects. No defect was detected using oblique incidence scans that could not be detected using normal incidence scans. In the two layer specimens, two main types of defects were detected: edge disbonds and micro defects. Micro defects were detected in regions remote from the edges and these small scale isolated defects took several forms. The detection of micro defects was a strong indicator that the interphase of the specimen had been attacked and weakened by the ingressing water molecules and, indeed, the number of such defects correlated to the loss of interfacial toughness. In the case of the three layer specimens, the extent of edge disbonding was much lower than in the corresponding two layer specimens. Also, no micro defects were detected ultrasonically in any of the three layer specimens. However, examination of some of the failure surfaces from the three layer specimens suggested that micro defects might have been present but that they were too small to be detected at the spatial resolution of the ultrasonic scans. Therefore, for the three layer joint specimens, there were no indicators from the ultrasonic scans, which could reveal whether the joint had suffered attack and weakening of the interphase regions by the ingressing moisture. There was no evidence in any of the tests of a gradual change in either the normal or oblique incidence reflection coefficient moving into an apparently well bonded region from either the edge disbonds or the micro defects.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ultrasonics and Acoustic Wave Propagation · Non-Destructive Testing Techniques · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Kinloch · 1983
2. The surface characterisation and adhesive bonding of aluminium
3. Past experiences in the development of tests for adhesive bond strength10.1163/156856191X00503 ↗
4. A comparison of different methods for the detection of a weak adhesive/adherend interface in bonded joints
5. Study of adhesive bonds using low-frequency obliquely incident ultrasonic waves10.1121/1.394053 ↗
6. Ultrasonic oblique incidence for improved sensitivity in interface weakness determination10.1016/0308-9126(88)90337-9 ↗
7. An ultrasonic interface layer model for bond evaluation10.1163/156856191X00530 ↗
8. The characterisation of oxide layers in adhesive joints using ultrasonic reflection measurements10.1098/rspa.1996.0101 ↗
9. Analysis of boundary conditions for elastic wave interaction with an interface between two solids10.1121/1.400374 ↗
10. Characterization of adhesive bonding using leaky Lamb waves
11. Characterization of glued bonds using ultrasonic reflected beam
12. Adhesive bondline interrogation using Stoneley wave methods10.1063/1.325943 ↗
13. An ultrasonic interface-wave method for predicting the strength of adhesive bonds10.1063/1.329016 ↗
14. Ultrasonic evaluation of the adhesion degree in layered joints
15. Interface characterization by true guided modes
16. The angular and frequency characteristics of reflectivity from a solid layer embedded between two solids with imperfect boundary conditions10.1121/1.398924 ↗
17. Evaluation of interfacial properties in adhesive joints of aluminium alloys using angle-beam ultrasonic spectroscopy10.1163/156856191X00549 ↗
18. Ultrasonic evaluation of environmentally degraded adhesive joints
19. Ultrasonic evaluation of environmental degradation of adhesive joints
20. The ultrasonic pulse-echo technique as applied to adhesion10.1088/0022-3727/6/7/305 ↗
21. Models for ultrasonic characterisation of environmental interfacial degradation in adhesive joints
22. Adhesive joint durability assessed using open-faced peel specimens10.1080/00218469808012248 ↗
23. Nondestructive characterisation of adhesive joint durability using ultrasonic reflection measurements10.1080/09349849909409638 ↗
24. Models for ultrasonic characterisation of environmental degradation of interfaces in adhesive joints10.1063/1.357301 ↗
25. Cawley P, Kinloch AJ, Vine K. Correlation of non destructive measurements and toughness changes in adhesive joints during environmental attacks. J Adhes (in press).
26. Measurement of adhesive joint fracture properties as a function of environmental degradation10.1016/S0143-7496(98)00028-1 ↗
27. Determination of density and elastic constants of a thin PAA oxide film by acoustic microscopy10.1121/1.428087 ↗
28. The calculation of adhesive strain energies from double-cantilever beam test specimens10.1007/BF00735649 ↗
29. Comments on mixed-mode fracture in adhesive joints10.1007/BF00034074 ↗
30. The role of the interphase in the environmental failure of adhesive joints10.1016/S1359-6454(00)00240-8 ↗