journal article·2018-09Open access

Imaging x70 weld cross-section using electromagnetic testing

Hanyang Xu, Jorge Ricardo Salas Avila, Fanfu Wu, Matthew J. Roy, Yuedong Xie, Frank Zhou, Anthony Peyton, Wuliang Yin

Abstract

Weld inspection is significant in manufacturing to improve productivity and ensure safety. During the welding process, steel microstructures experience complex transformations depending on welding conditions such as heat input, welding speed, component size and temperature, etc. Examining weld microstructures can reveal valuable information on its metallurgical, mechanical and electromagnetic properties. Electromagnetic (EM) testing is of great practical interest to characterise the weld microstructures in a non-destructive and expedient manner. In this paper, an experimental scanning method using a cup-ferrite enclosed T-R sensor has been devised to image the EM properties of a cross-section of an X70 steel submerged arc welding (SAW) specimen. These images show good correlation with the hardness testing and metallurgical information of the specimen. An approximate linear relationship was found between the EM signal and the hardness of the SAW of X70 steel weld. The scanning method can serve as a complementary tool for hardness testing without the need for sophisticated surface preparation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Non-Destructive Testing Techniques · Welding Techniques and Residual Stresses · Ultrasonics and Acoustic Wave Propagation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Boyer · 1987 · vol. 1987 · 188
2. John · 1992
3. Theoretical analysis of Barkhausen noise in carbon steels10.1109/TMAG.1987.1065664 ↗
4. Barkhausen noise characterisation during elastic bending and tensile-compression loading of case-hardened and tempered samples10.1007/s10853-012-6571-3 ↗
5. Experimental verification of the linear relationship between stress and the reciprocal of the peak barkhausen voltage in ASTM A36 steel10.1109/TMAG.2012.2234728 ↗
6. Distortion analysis of magnetic excitation - a novel approach for the non-destructive microstructural evaluation of ferromagnetic steel
7. Imaging the continuous conductivity profile within layered metal structures using inductance spectroscopy10.1109/JSEN.2004.842637 ↗
8. Evaluating the permeability distribution of a layered conductor by inductance spectroscopy10.1109/TMAG.2006.880992 ↗
9. Exploring the relationship between ferrite fraction and morphology and the electromagnetic properties of steel10.1007/s10853-006-1327-6 ↗
10. Measurement of permeability and ferrite/austenite phase fraction using a multi-frequency electromagnetic sensor10.1016/j.ndteint.2008.01.009 ↗
11. Eddy current evaluation of cast irons for material characterization10.1016/S0304-8853(02)01068-5 ↗
12. Eddy currents and hardness testing for evaluation of steel decarburizing10.1016/j.ndteint.2006.04.005 ↗
13. Measurement of electromagnetic properties of power station steels10.1016/j.ndteint.2012.06.008 ↗
14. Measurement of the magnetic properties of P9 and T22 steel taken from service in power station10.1016/j.jmmm.2014.01.057 ↗
15. Evaluation of mechanical properties in medium carbon steel with a point mode electromagnetic sensor10.1016/j.sna.2017.11.001 ↗
16. Relation between mechanical microhardness and impedance variations in eddy current testing10.1016/j.ndteint.2003.09.002 ↗
17. Electrical conductivity field analysis for evaluation of FSW joints in AA6013 and AA7075 alloys10.1016/j.jmatprotec.2010.08.030 ↗
18. The effect of the weld fusion zone shape on residual stress in submerged arc welding10.1007/s00170-016-9542-z ↗
19. ISO · 2009
20. Boiler, A.., Pressure Vessel Code Section IX: qualification Standard for welding and brazing procedures, welders, brazers, and welding and brazing operators, Ed. 2007 with 2009 addenda included. ASME. American Society of Mechanical Engineers.
21. Effect of titanium addition on the microstructure and inclusion formation in submerged arc welded HSLA pipeline steel10.1016/j.jmatprotec.2008.09.021 ↗
22. Characterisation of weldment hardness, impact energy and microstructure in API X65 steel10.1016/j.ijpvp.2012.05.011 ↗
23. Effects of welding speed, energy input and heat source distribution on temperature variations in butt joint welding10.1016/j.jmatprotec.2005.06.018 ↗
24. Effect of increasing deposition rate on the bead geometry of submerged arc welds10.1016/S0924-0136(97)00139-8 ↗
25. Prediction and control of weld bead geometry and shape relationships in submerged arc welding of pipes10.1016/j.jmatprotec.2005.03.001 ↗