Abstract Adjusting the grain growth orientation may be a feasible way to improve the oxidation resistance. In this work, textured Ti3(SiAl)C2 ceramic was successfully fabricated via the spark plasma sintering technique. The crystal orientation and microstructure were investigated by XRD combined with EBSD. The oxidation behavior of textured Ti3(SiAl)C2 was investigated at 1000–1300 °C for 10 h. The results showed that the oxidation was significantly anisotropic and the surface parallel to the compression direction exhibited better oxidation resistance below 1200 °C. The improved oxidation resistance was primarily attributed to the formation of passivated Al2O3 scale by rapid out-diffusion of Al elements on the orientated (hko) planes in textured Ti3(SiAl)C2. The formation of oxide scales was strongly dependent on the crystallographic orientation of Ti3(SiAl)C2.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Barsoum, M. W. The MN+1AXN phases: a new class of solids: thermodynamically stable nanolaminates. Prog. Solid State Chem. 28, 201–281 (2000).10.1016/S0079-6786(00)00006-6 ↗
2. Sokol, M., Natu, V., Kota, S. & Barsoum, M. W. On the chemical diversity of the MAX phases. Trends Chem. 1, 210–223 (2019).10.1016/j.trechm.2019.02.016 ↗
3. Ramachandran, K., Carmine, Z., Yoshida, K., Tsunoura, T. & Jayaseelan, D. D. Experimental investigation and mathematical modelling of water vapour corrosion of Ti3SiC2 and Ti2AlC ceramics and their mechanical behaviour. J. Eur. Ceram. Soc. 41, 4761–4773 (2021).10.1016/j.jeurceramsoc.2021.03.045 ↗
4. Sun, Z., Zhou, Y. & Li, M. Oxidation behaviour of Ti3SiC2-based ceramic at 900-1300 °C in air. Corros. Sci. 43, 1095–1109 (2001).10.1016/S0010-938X(00)00142-6 ↗
5. Ji, Y. et al. High temperature oxidation resistance of Ti3SiC2 in air and low oxygen atmosphere. Int. J. Appl. Ceram. Tec. 14, 851–859 (2017).10.1111/ijac.12746 ↗
6. Zhang, H. B., Zhou, Y. C., Bao, Y. W. & Li, M. S. Improving the oxidation resistance of Ti3SiC2 by forming a Ti3Si0.9Al0.1C2 solid solution. Acta Mater. 52, 3631–3637 (2004).10.1016/j.actamat.2004.04.015 ↗
7. Zhang, Z. et al. Preparation and anisotropic properties of textured structural ceramics: A review. J. Adv. Ceram. 8, 289–332 (2019).10.1007/s40145-019-0325-5 ↗
8. Hu, C. et al. Shell-like nanolayered Nb4AlC3 ceramic with high strength and toughness. Scr. Mater. 64, 765–768 (2011).10.1016/j.scriptamat.2010.12.045 ↗
9. Li, X. et al. Oxidation and creep behavior of textured Ti2AlC and Ti3AlC2. J. Eur. Ceram. Soc. 42, 364–375 (2022).10.1016/j.jeurceramsoc.2021.10.018 ↗
10. Xu, L. et al. Effect of texture on oxidation resistance of Ti3AlC2. J. Eur. Ceram. Soc. 38, 3417–3423 (2018).10.1016/j.jeurceramsoc.2018.03.009 ↗
11. Xie, X., Yang, R., Cui, Y. Y., Jia, Q. & Bai, C. G. Fabrication of textured Ti2AlC lamellar composites with improved mechanical properties. J. Mater. Sci. Tech. 38, 86–92 (2020).10.1016/j.jmst.2019.05.070 ↗
12. Li, X., Xie, X., Gonzalez-Julian, J., Malzbender, J. & Yang, R. Mechanical and oxidation behavior of textured Ti2AlC and Ti3AlC2 MAX phase materials. J. Eur. Ceram. Soc. 40, 5258–5271 (2020).10.1016/j.jeurceramsoc.2020.07.043 ↗
13. Lapauw, T., Vanmeensel, K., Lambrinou, K. & Vleugels, J. A new method to texture dense Mn+1AX ceramics by spark plasma deformation. Scr. Mater. 111, 98–101 (2016).10.1016/j.scriptamat.2015.08.023 ↗
14. Duan, X. et al. Synthesis of high-purity, isotropic or textured Cr2AlC bulk ceramics by spark plasma sintering of pressure-less sintered powders. J. Eur. Ceram. Soc. 35, 1393–1400 (2015).10.1016/j.jeurceramsoc.2014.11.008 ↗
15. Hu, C., Sakka, Y., Grasso, S., Suzuki, T. & Tanaka, H. Tailoring Ti3SiC2 ceramic via a strong magnetic field alignment method followed by spark plasma sintering. J. Am. Ceram. Soc. 94, 742–748 (2011).10.1111/j.1551-2916.2010.04186.x ↗
16. Wang, Q., Li, M.-H., Chen, G.-Q., Fu, X.-S. & Zhou, W.-L. Effects of texture orientation in Ti3SiC2 on growth kinetics of interfacial compound layers in diffusion bonded TiAl/Ti3SiC2 joints. J. Eur. Ceram. Soc. 41, 244–251 (2021).10.1016/j.jeurceramsoc.2020.09.022 ↗
17. Li, S., Song, G.-M. & Zhou, Y. A dense and fine-grained SiC/Ti3Si(Al)C2 composite and its high-temperature oxidation behavior. J. Eur. Ceram. Soc. 32, 3435–3444 (2012).10.1016/j.jeurceramsoc.2012.04.029 ↗
18. Smialek, J. L. Oxygen diffusivity in alumina scales grown on Al-MAX phases. Corros. Sci. 91, 281–286 (2015).10.1016/j.corsci.2014.11.030 ↗
19. Zuber, A. et al. Towards a better understanding of the high-temperature oxidation of MAX phase Cr2AlC. J. Eur. Ceram. Soc. 42, 2089–2096 (2022).10.1016/j.jeurceramsoc.2021.12.057 ↗
20. Smialek, J. L. Kinetic aspects of Ti2AlC MAX phase oxidation. Oxid. Met. 83, 351–366 (2015).10.1007/s11085-015-9526-7 ↗
21. Gao, N. F., Miyamoto, Y. & Zhang, D. On physical and thermochemical properties of high-purity Ti3SiC2. Mater. Lett. 55, 61–66 (2002).10.1016/S0167-577X(01)00620-6 ↗
22. Chen, J. X. & Zhou, Y. C. Effect of Si content on the oxidation resistance of Ti3Al1-xSixC2 (x⩽ 0.25) solid solutions at 1000–1400 °C in air. Oxid. Met. 65, 123–135 (2006).10.1007/s11085-006-9007-0 ↗
23. Zhou, Y. C., Wan, D. T., Bao, Y. W. & Wang, J. Y. In situ processing and high-temperature properties of Ti3Si(Al)C2/SiC composites. Int. J. Appl. Ceram. Tec. 3, 47–54 (2006).10.1111/j.1744-7402.2006.02057.x ↗
24. Wang, X. H. & Zhou, Y. C. Stability and selective oxidation of aluminum in nano-laminate Ti3AlC2 upon heating in argon. Chem. Mater. 15, 3716–3720 (2003).10.1021/cm030022v ↗
25. Zheng, L.-L., Sun, L.-C., Li, M.-S. & Zhou, Y.-C. Improving the high-temperature oxidation resistance of Ti3(SiAl)C2 by Nb-doping. J. Am. Ceram. Soc. 94, 3579–3586 (2011).10.1111/j.1551-2916.2011.04586.x ↗
26. Guedouar, B. et al. Oxidation behavior of Al-doped Ti3SiC2-20 wt.%Ti5Si3 composite. Ceram. Int. 47, 33622–33631 (2021).10.1016/j.ceramint.2021.08.272 ↗
27. Zhu, X. & Sakka, Y. Textured silicon nitride: processing and anisotropic properties. Sci. Technol. Adv. Mater. 9, 033001 (2008).10.1088/1468-6996/9/3/033001 ↗