journal article·2019-09

Experimental study of 355 nm laser damage ignited by Fe and Ce impurities on fused silica surface

Liu Hongjie, Wang Fengrui, Huang Jin, Meng Jie, Ma yongjun, Lian Yafei, Sun Laixi, Ye Xin, Geng Feng, Jiang Xiaodong, Wu Weidong, Yang Liming

Optical Materials· Volume 95
Publisher page

Abstract

Abstract Laser-induced damage on fused silica surface is often ignited by absorbing impurities introduced by polishing processing. In order to analyze laser damage mechanism induced by Fe and Ce impurity on fused silica surface, this paper presents laser induced damage threshold of three types of fused silica surface dealed with traditional chemo-mechanical or magnetorheological finishing and carries out the surface impurity analysis, photo-thermal absorption analysis and gray haze damage mechanism analysis. The results show the significant different Ce and Fe impurities on the surface of the three kinds of samples. The two impurities both have a serious influence on laser-induced native damage. The analyses of photo-thermal absorption on the surface of optical element show that the haze damage pits morphology is related to the absorptivity of nanoparticles. The native surface damage threshold induced by Fe nanoparticle is lower than by Ce nanoparticle by analyzing atomic force microscopy images and scanning electron microscopy images. The conclusion is different from previous reports which believe Fe element shows a weak relation with laser-induced damage. This paper also analyzes the relationship between gray haze damage and native damage for the first time. The results are helpful to understanding laser induced damage of fused silica ignited by impurities.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · Laser-induced spectroscopy and plasma

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. The national ignition facility: the world's largest optics and laser system10.1117/12.500351 ↗
2. National ignition facility: 1.8MJ, 750TW ultraviolet laser10.1117/12.538463 ↗
3. Status of the LMJ project10.1117/12.294307 ↗
4. Design of 60-kJ SG-Ⅲ laser facility and related technology development10.1117/12.425569 ↗
5. SG-II solid-state laser ICF system10.1117/12.354210 ↗
6. Extracting the distribution of laser damage precursors on fused silica surfaces for 351 nm, 3 ns laser pulses at high fluences (20-150 J/cm2)10.1364/OE.20.011561 ↗
7. Nanosecond to femtosecond laser-induced breakdown in dielectrics10.1103/PhysRevB.53.1749 ↗
8. Concerning the impact of polishing induced contamination of fused silica optics on the laser-induced damage density at 351 nm10.1016/j.optcom.2008.03.031 ↗
9. Depth profiling of polishing induced contamination on fused silica surface10.1117/12.307031 ↗
10. Polishing-induced contamination of fused silica optics and laser induced damage density at 351 nm10.1364/OPEX.13.010163 ↗
11. Imaging subsurface damage of grinded fused silica optics by confocal fluorescence microscopy10.1364/OE.17.003543 ↗
12. The distribution of subsurface damage in fused silica10.1117/12.638821 ↗
13. A method for evaluating subsurface damage in optical glass10.1364/OE.18.017180 ↗
14. Subsurface damage measurement of ground fused silica parts by HF etching techniques10.1364/OE.17.020448 ↗
15. Role of light intensification by cracks in optical breakdown on surfaces10.1364/JOSAA.18.002607 ↗
16. Subsurface defects of fused silica optics and laser induced damage at 351 nm10.1364/OE.21.012204 ↗
17. Laser induced damage characteristics of fused silica optics treated by wet chemical processes10.1016/j.apsusc.2015.09.065 ↗
18. Oxygen plasma etching of fused silica substrates for high power laser optics10.1016/j.apsusc.2018.05.105 ↗
19. Modeling study on the surface morphology evolution during removing the optics surface subsurface damage using atmospheric pressure plasma processing10.1016/j.apsusc.2016.04.157 ↗
20. Subsurface defects characterization and laser damage performance of fused silica optics during HF-etched process10.1016/j.optmat.2013.11.022 ↗
21. HF-based etching processes for improving laser damage resistance of fused silica optical surfaces10.1111/j.1551-2916.2010.04112.x ↗
22. Surface roughness and material-removal rate with magnetorheological finishing without subsurface damage of the surface10.1364/JOT.72.000865 ↗
23. Magnetorheological finishing for removing surface and subsurface defects of fused silica optics10.1117/1.OE.53.9.092010 ↗
24. Residual impurities on fused silica surface processed by different technics and their effects on laser induced damage at 355nm
25. Two mechanisms of crater formation in ultraviolet-pulsed-laser irradiated SiO2 thin films with artificial defects10.1063/1.1924878 ↗
26. Nanoscale laser-induced spallation in SiO2 films containing gold nanoparticles10.1007/s00340-005-2109-6 ↗
27. Testing asymmetry in plasma-ball growth seeded by a nanoscale absorbing defect embedded in a SiO2 thin-film matrix subjected to UV pulsed-laser radiation10.1063/1.2980054 ↗
28. Correlations between embedded single gold nanoparticles in SiO2 thin film and nanoscale crater formation induced by pulsed-laser radiation10.1063/1.1512691 ↗
29. Investigation of laser-induced damage by various initiators on the subsurface of fused silica10.1364/OE.20.022095 ↗
30. Growth behavior of laser-induced damage on fused silica optics under UV, ns laser irradiation10.1364/OE.18.019966 ↗
31. Probability of growth of small damage sites on the exit surface of fused silica optics10.1364/OE.20.013030 ↗