Suppression of dead zones in slot-coated organic thin films by monitoring of meniscus formation for OLEDs
Source abstract
Abstract
There inevitably appear dead zones in organic thin films fabricated by sheet-to-sheet slot-die coating because a coating start varies and the recovery time of internal pressure in slot-die head differs for each coating, resulting in poor coating repeatability. Slot-coated thin films within dead zones are thinner or thicker, possibly causing non-uniform light emission from solution-processable organic light-emitting diodes (OLEDs). To tackle it, we have devised an automatic coating start method based on the monitoring of meniscus formation. It automatically starts coatings when the cross-sectional area of meniscus reaches a certain optimal value in such a way that the start of each coating is kept unchanged. It is found that high-viscosity (4800 cPs) polydimethylsiloxane (PDMS) requires a longer time for the internal pressure of slot-die head to reach a steady state than low-viscosity (80 cPs) poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS). It can be reduced to a great extent by applying a method of discharging the solution in advance (pre-discharging scheme). Compared with high-viscosity PDMS films, low-viscosity PEDOT:PSS films are shown to have longer dead zones and poorer repeatability due to the fact that the dead zone of relatively thin films varies sensitively to a small change in the coating start timing. With this scheme, we have successfully fabricated a highly uniform OLED device with no dead zones in the emission area.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Light-Emitting Diodes Research · Organic Electronics and Photovoltaics · Green IT and Sustainability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Fabrication of organic light emitting diodes (oleds) for flat panel displays
2. Simple-structured efficient white organic light emitting diode via solution process10.1016/j.microrel.2017.07.076 ↗
3. Fully solution-processed perovskite solar cells fabricated by lamination process with silver nanoparticle film as top electrode10.1016/j.egyr.2020.04.037 ↗
4. Facile fabrication of solution-processed solid-electrolytes for high-energy-density all-solid-state-batteries by enhanced interfacial contact
5. Catalyst layer formulations for slot-die coating of PEM fuel cell electrodes10.1016/j.ijhydene.2022.08.157 ↗
6. All solution-processed micro-structured flexible electrodes for low-cost light-emitting pressure sensors fabrication10.1038/s41598-017-07284-8 ↗
7. Slot-die coating of sol–gel-based organic–inorganic nanohybrid dielectric layers for flexible and large-area organic thin film transistors10.1016/j.apsusc.2020.147198 ↗
8. Ambient fabrication of flexible and large-area organic light-emitting devices using slot-die coating10.1038/ncomms2002 ↗
9. Slot-die coating large-area formamidinium-cesium perovskite film for efficient and stable parallel solar module
10. In situ investigations of simultaneous two-layer slot die coating of component-graded anodes for improved high-energy Li-ion batteries10.1002/ente.201901251 ↗
11. Solution-coating technology for AMOLED displays
12. 43.3: slot die coating for OLED displays10.1889/1.3069746 ↗
13. Predicting a process window for the roll-to-roll deposition of solvent-engineered SnO 2 in perovskite solar cells10.1039/D2MA00841F ↗
14. Reaching highly uniform perovskite ink flow from a slot-die head toward printed solar cells10.1002/adem.202201561 ↗
15. Numerical simulation on preparing uniform and stable perovskite wet film in slot-die coating process10.1021/acsomega.3c00959 ↗
16. Reexamination of Hagen-Poiseuille flow: shape dependence of the hydraulic resistance in microchannels10.1103/PhysRevE.71.057301 ↗
17. Design of pressure-driven microfluidic networks using electric circuit analogy10.1039/C2LC20799K ↗
18. Slot die coating of lithium-ion battery electrodes: investigations on edge effect issues for stripe and pattern coatings10.1007/s11998-013-9498-y ↗
19. The effect of shear-thickening on the stability of slot-die coating10.1002/aic.15336 ↗
20. Slot-die coating operability window for nanoparticle bed deposition in a microscale selective laser sintering tool10.1115/1.4049668 ↗
21. PEDOT:PSS for flexible and stretchable electronics: modifications, strategies, and applications10.1002/advs.201900813 ↗
22. Mechanisms for doped PEDOT:PSS electrical conductivity improvement10.1039/D1MA00290B ↗
23. Elschner · 2010
24. Highly conductive and transparent PEDOT:PSS films with a fluorosurfactant for stretchable and flexible transparent electrodes10.1002/adfm.201101775 ↗
25. Stretchable PDMS encapsulation via SiO2 doping and atomic layer infiltration for flexible displays