journal article·2025-11-14

Thickness-dependent perpendicular magnetic anisotropy and topological Hall effect in magnetic Weyl Co 2 MnGa and topological insulator Bi 2 Te 3 –based heterostructures

Nikita Sharma, Lalit Pandey, Nakul Kumar, Soumyarup Hait, Nanhe Kumar Gupta, Shubhashish Pati, Saurav Singh, Mitali, Sujeet Chaudhary

Physical Review B· Volume 112· Issue 17
Publisher page

Abstract

We have investigated the magnetic and transport properties of a unique combination of the topological Weyl ferromagnet (FM) ${\mathrm{Co}}2\mathrm{MnGa}$ (CMG) and the topological insulator (TI) ${\mathrm{Bi}}2{\mathrm{Te}}3$ (BT) in order to explore quantum materials and their heterostructures with nontrivial topology in real space as well as momentum space. The thickness- and temperature-dependent properties of this heterostructure are studied in detail. The interfacial perpendicular magnetic anisotropy is observed in ${\mathrm{Co}}2\mathrm{MnGa}$ at a thickness as high as 3 nm. The thickness-dependent tuning of the Fermi level leads to distinct transport characteristics in CMG($t$)/BT heterostructures. The study also reports two unconventional observations in the Hall effect, i.e., the sign reversal of the anomalous Hall effect and the emergence of the topological Hall effect, both of which exhibit a significant dependence on temperature. The topological Hall effect, characterized by a high squareness ratio and a large Hall resistivity value of $\ensuremath{\sim}189\phantom{\rule{0.28em}{0ex}}\mathrm{n}\mathrm{\ensuremath{\Omega}}\phantom{\rule{0.16em}{0ex}}\mathrm{cm}$ at 5 K, is observed in a wide temperature range below ${T}c$ in the CMG(7 nm)/BT(10 nm) heterostructure. This effect can be attributed to the presence of chiral magnetic textures induced by the interfacial Dzyaloshinskii-Moriya interaction, arising from the strong spin-orbit coupling (SOC) of BT. This conclusion is supported by the absence of such unconventional signatures in transport and magnetic measurements in another similar series CMG($t$)/W(10 nm). Therefore, the interplay of strong intrinsic Berry curvature in CMG (as deduced from scaling mechanisms) and the high SOC of BT enable the FM/TI combination to host unconventional spin textures, which may provide an important building block for the next generation of spintronic devices.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Topological Materials and Phenomena · Chemical and Physical Properties of Materials · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Indian Institute of Technology Delhi

Funding

Indian Institute of Technology Roorkee

References (51)

Show source-provided references
1. 10.1016/j.vacuum.2017.01.03110.1016/j.vacuum.2017.01.031 ↗
2. 10.1103/PhysRevB.107.17440210.1103/PhysRevB.107.174402 ↗
3. 10.1063/1.496070510.1063/1.4960705 ↗
4. 10.1016/j.pmatsci.2023.10114210.1016/j.pmatsci.2023.101142 ↗
5. 10.1080/14686996.2020.181236410.1080/14686996.2020.1812364 ↗
6. 10.1038/srep1235210.1038/srep12352 ↗
7. 10.1103/PhysRevLett.119.15640110.1103/PhysRevLett.119.156401 ↗
8. 10.1103/PhysRevB.100.05442210.1103/PhysRevB.100.054422 ↗
9. 10.1038/s41467-023-42222-510.1038/s41467-023-42222-5 ↗
10. 10.1063/5.010203910.1063/5.0102039 ↗
11. 10.1002/adfm.20241319410.1002/adfm.202413194 ↗
12. 10.1016/j.jmmm.2020.16639710.1016/j.jmmm.2020.166397 ↗
13. 10.1063/1.497607810.1063/1.4976078 ↗
14. 10.3390/s2309456410.3390/s23094564 ↗
15. 10.1063/5.003717810.1063/5.0037178 ↗
16. 10.1063/5.007353710.1063/5.0073537 ↗
17. 10.1038/nature0891610.1038/nature08916 ↗
18. 10.1103/PhysRevB.75.12130610.1103/PhysRevB.75.121306 ↗
19. 10.1016/j.progsurf.2006.03.00110.1016/j.progsurf.2006.03.001 ↗
20. 10.1038/s41467-023-40714-y10.1038/s41467-023-40714-y ↗
21. 10.1021/acsnano.1c0551910.1021/acsnano.1c05519 ↗
22. 10.1103/PhysRevB.110.09440210.1103/PhysRevB.110.094402 ↗
23. 10.1021/acs.nanolett.3c0157310.1021/acs.nanolett.3c01573 ↗
24. 10.1126/sciadv.abq276510.1126/sciadv.abq2765 ↗
25. 10.1209/0295-5075/104/1700110.1209/0295-5075/104/17001 ↗
26. 10.1002/andp.20190028710.1002/andp.201900287 ↗
27. 10.1038/s41598-017-13211-810.1038/s41598-017-13211-8 ↗
28. 10.1063/5.016666310.1063/5.0166663 ↗
29. See Supplemental Material at http://link.aps.org/supplemental/10.1103/tghq-yymk for details of the XRR profiles; AFM topography images of the CMG(t)/BT(10 nm), t=(a) 5 nm, (b) 7 nm, (c) 9 nm, (d) 11 nm; EDS spectrum of CMG (t=3, 5, 7, 9, and 11 nm)/BT(10 nm); coercivity and saturation magnetization dependence on CMG thickness for CMG(t)/BT(10) heterostructure; variation of saturation magnetization in in-plane MH loops versus thickness of CMG; and variation of magnetic field, HT, corresponding to the dip observed in AHE and MR data.
30. 10.1039/D0RA05429A10.1039/D0RA05429A ↗
31. 10.1063/5.008880710.1063/5.0088807 ↗
32. 10.3390/nano1101025110.3390/nano11010251 ↗
33. 10.1038/s41427-019-0116-z10.1038/s41427-019-0116-z ↗
34. 10.1038/ncomms946210.1038/ncomms9462 ↗
35. 10.1038/s41467-023-38995-410.1038/s41467-023-38995-4 ↗
36. 10.1021/acs.nanolett.9b0219110.1021/acs.nanolett.9b02191 ↗
37. 10.1038/s41535-021-00315-810.1038/s41535-021-00315-8 ↗
38. 10.1073/pnas.220850511910.1073/pnas.2208505119 ↗
39. 10.1103/PhysRevLett.103.08720610.1103/PhysRevLett.103.087206 ↗
40. 10.1103/PhysRevB.78.09240510.1103/PhysRevB.78.092405 ↗
41. 10.1016/S0031-8914(58)93541-910.1016/S0031-8914(58)93541-9 ↗
42. 10.1103/PhysRevB.105.03512410.1103/PhysRevB.105.035124 ↗
43. 10.1103/PhysRevB.109.L20110810.1103/PhysRevB.109.L201108 ↗
44. 10.1021/acs.jpcc.4c0644010.1021/acs.jpcc.4c06440 ↗
45. 10.1038/s43246-022-00238-210.1038/s43246-022-00238-2 ↗
46. 10.1103/PhysRevB.98.21444010.1103/PhysRevB.98.214440 ↗
47. 10.1103/PhysRevB.91.04112210.1103/PhysRevB.91.041122 ↗
48. 10.1103/PhysRevLett.108.26720110.1103/PhysRevLett.108.267201 ↗
49. 10.1103/PhysRevB.110.10443010.1103/PhysRevB.110.104430 ↗
50. 10.1021/acsnano.0c0541310.1021/acsnano.0c05413 ↗
51. 10.1103/PhysRevLett.119.17680910.1103/PhysRevLett.119.176809 ↗