Electrical and Optical Properties of Cr2O3 Films Prepared by Chemical Vapour Deposition
Source abstract
Abstract
Polycrystalline Cr2O3 films are prepared by normal pressure chemical vapour deposition (CVD), and electrical and optical properties of the films are investigated. The films are transparent from 800 to 1000 nm wavelength, and absorbing for wavelengths shorter than 800 nm. The optical band gap energy is Eopt = 2.98 to 3.09 eV for films formed at different substrate temperatures. The electrical conductivity σ of the films is from 1 × 10−2 to 2.5 × 10−3 S cm−1 at 500 K. The films are p-type semiconducting. At temperatures higher than 500 K. the conduction is due to small polaron hopping. For temperatures lower than 500 K, a T−1/4 dependence of σT1/2 is found, which is attributed to variable-range hopping.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Transition Metal Oxide Nanomaterials · ZnO doping and properties · Luminescence Properties of Advanced Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.