article·2014-09-16Open access

Manufacturing 100-µm-thick silicon solar cells with efficiencies greater than 20% in a pilot production line

Barbara Terheiden, Tabitha Ballmann, Renate Horbelt, Yvonne Schiele, Sabine Seren, Jan Ebser, Giso Hahn, Verena Mertens, Max Koentopp, M. Scherff, J. W. Müller, Zachary C. Holman, Antoine Descoeudres, Stefaan De Wolf, Silvia Martín de Nicolás, Jonas Geissbuehler, Christophe Ballif, Bernd Weber, Pierre Saint‐Cast, Michael Rauer, Christian Schmiga, Stefan W. Glunz, Dominique J. Morrison, S Devenport, D. Antonelli, Chiara Busto, F.S. Grasso, Francesca Ferrazza, Elisa Tonelli, Wolfgang Oswald

Abstract

Reducing wafer thickness while increasing power conversion efficiency is the most effective way to reduce cost per Watt of a silicon photovoltaic module. Within the European project 20 percent efficiency on less than 100-µm-thick, industrially feasible crystalline silicon solar cells (“20plµs”), we study the whole process chain for thin wafers, from wafering to module integration and life-cycle analysis. We investigate three different solar cell fabrication routes, categorized according to the temperature of the junction formation process and the wafer doping type: p-type silicon high temperature, n-type silicon high temperature and n-type silicon low temperature. For each route, an efficiency of 19.5% or greater is achieved on wafers less than 100 µm thick, with a maximum efficiency of 21.1% on an 80-µm-thick wafer. The n-type high temperature route is then transferred to a pilot production line, and a median solar cell efficiency of 20.0% is demonstrated on 100-µm-thick wafers.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Photovoltaic System Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.