journal article·2014-04

Stability of graphene–silicon heterostructure solar cells

V. V. Brus, M. A. Gluba, X. Zhang, K. Hinrichs, J. Rappich, N. H. Nickel

physica status solidi (a)· Volume 211· Issue 4
Publisher page

Abstract

The stability of undoped graphene–silicon heterostructure solar cells was investigated. Single‐layer graphene was grown by chemical vapor deposition on copper foil. Prior to the transfer of graphene to the silicon wafer, the flat Si(111) surface was passivated with hydrogen or methyl groups (CH3). The conversion efficiency,η, of the H terminated Si device was negligible small (0.1%), whereas that of the CH3passivated Si was 2 and 4.2% at 100 mW (AM 1.5) and 20 mW of light intensity, respectively. After 28 days in ambient atmosphereηdecreased only slightly to 1.5 and 3.7%. This small change ofηis due to the high stability of the CH3passivated graphene–Si(111) interface. The methylated Si surface shows a high degree of chemical stability especially during the graphene transfer process.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Graphene research and applications · Silicon Nanostructures and Photoluminescence · Nanowire Synthesis and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Helmholtz‐Zentrum Berlin für Materialien und Energie GmbH Institut für Silizium‐Photovoltaik Kekuléstr. 5 12489 Berlin Germany

Department of Electronics and Energy Engineering Chernivtsi National University Kotsubinsky Str. 2 58012 Chernivtsi Ukraine

Leibniz‐Institut für Analytische Wissenschaften – ISAS – e.V., Department Berlin Albert‐Einstein‐Strasse 9 12489 Berlin Germany

Funding

European Union through the EFRE program

References (16)

Show source-provided references
1. 10.1021/nl900152510.1021/nl9001525 ↗
2. 10.1109/OMEMS.2010.567219210.1109/OMEMS.2010.5672192 ↗
3. 10.1038/nnano.2010.13210.1038/nnano.2010.132 ↗
4. 10.1063/1.292477110.1063/1.2924771 ↗
5. 10.1021/nl072838r10.1021/nl072838r ↗
6. 10.1002/adma.20090438310.1002/adma.200904383 ↗
7. 10.1039/c0cc05139j10.1039/c0cc05139j ↗
8. 10.1021/nl204414u10.1021/nl204414u ↗
9. 10.1021/nl400353f10.1021/nl400353f ↗
10. S.Avasthi W.Mcclain J.Schwarti andJ. C.Sturm in: 70th Annu. Device Research Conference (DRC) (2012) p.93.10.1109/DRC.2012.6256955 ↗
11. 10.1063/1.144581010.1063/1.1445810 ↗
12. 10.1021/jp301013t10.1021/jp301013t ↗
13. 10.1126/science.117124510.1126/science.1171245 ↗
14. 10.1063/1.37032710.1063/1.370327 ↗
15. 10.1016/j.solener.2011.12.00910.1016/j.solener.2011.12.009 ↗
16. 10.1021/nl072364w10.1021/nl072364w ↗