Significant bulk‐related degradation (BRD) is followed by surface‐related degradation (SRD) of effective excess charge carrier lifetime in lifetime samples made of Czochralski silicon during illuminated treatment at 80–150 °C. Samples are passivated with either AlO x :H/SiO x N y :H/SiN x :H or SiO x N y :H/SiN x :H stacks stemming entirely from plasma‐enhanced chemical vapor deposition. Samples show strong variations in BRD depending on passivation stacks and treatment conditions, and a potential link to light and elevated temperature‐induced degradation (LeTID) is discussed. All samples are fired in a belt furnace, and variations of firing temperature and belt speed are shown to influence SRD slightly. SRD is furthermore accelerated with increasing treatment temperature and an apparent activation energy E app = 1.07 ± 0.02 eV is determined in SiO x N y :H/SiN x :H passivated samples. Interpretation of E app is, however, difficult as both changes in interfacial defect and fixed charge density occur in parallel during SRD.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Physics, University of Konstanz Universitätsstr. 10 78464 Konstanz Germany
Funding
German Federal Ministry for Economic Affairs and Energy
References (31)
Show source-provided references
1. 10.1016/j.solmat.2015.11.04710.1016/j.solmat.2015.11.047 ↗
2. H.Fischer W.Pschunder inProc. 26th IEEE Photovolt. Spec. Conf. Rec. Palo Alto USA1973 p.404.
3. J.Schmidt A.Aberle R.Hezel inProc. 26th IEEE Photovolt. Spec. Conf. Rec. Anaheim USA1997 p.13.
4. S. W.Glunz S.Rein W.Warta J.Knobloch W.Wettling inProc. 2nd World Conf. Photovolt. Energy Conver. Vienna Austria1998 p.1343.
5. 10.1109/JPHOTOV.2016.261411910.1109/JPHOTOV.2016.2614119 ↗
6. 10.3390/app801001010.3390/app8010010 ↗
7. 10.1063/1.34506310.1063/1.345063 ↗
8. 10.1063/1.163713610.1063/1.1637136 ↗
9. 10.1063/1.182358710.1063/1.1823587 ↗
10. K.Ramspeck S.Zimmermann H.Nagel A.Metz Y.Gassenbauer B.Birkmann A.Seidl inProc. 27th Eur. Photovolt. Sol. Energy Conf. Exhib. Frankfurt/Main Germany2012 p.861.
11. 10.1002/pssr.20140942410.1002/pssr.201409424 ↗
12. 10.1016/j.solmat.2015.06.01510.1016/j.solmat.2015.06.015 ↗
13. 10.1016/j.egypro.2017.09.30810.1016/j.egypro.2017.09.308 ↗
14. 10.1016/j.solmat.2017.08.00310.1016/j.solmat.2017.08.003 ↗
15. 10.1016/j.solmat.2018.05.03110.1016/j.solmat.2018.05.031 ↗
16. 10.1109/JPHOTOV.2017.275507210.1109/JPHOTOV.2017.2755072 ↗
17. 10.1016/j.solmat.2018.08.01910.1016/j.solmat.2018.08.019 ↗
18. 10.1109/JPHOTOV.2017.277514710.1109/JPHOTOV.2017.2775147 ↗
19. 10.1016/j.solmat.2015.06.05510.1016/j.solmat.2015.06.055 ↗
20. 10.1109/JPHOTOV.2018.285052110.1109/JPHOTOV.2018.2850521 ↗
21. 10.1016/j.egypro.2017.09.33910.1016/j.egypro.2017.09.339 ↗
22. R. A.Sinton A.Cuevas M.Stuckings inProc. 25th IEEE Photovolt. Spec. Conf. Rec. Washington D.C. USA1996 p.457.10.1109/PVSC.1996.564042 ↗
23. 10.1063/1.488659510.1063/1.4886595 ↗
24. 10.1016/j.solmat.2015.06.04310.1016/j.solmat.2015.06.043 ↗
25. A.Schwarz Bachelor Thesis University of Konstanz September2017.
26. 10.1109/JPHOTOV.2017.271341110.1109/JPHOTOV.2017.2713411 ↗
27. 10.1109/JPHOTOV.2017.278385110.1109/JPHOTOV.2017.2783851 ↗
28. J.Fritz A.Zuschlag D.Skorka A.Schmid G.Hahn inProc. 33rd Eur. Photovolt. Sol. Energy Conf. Exhib. Amsterdam The Netherlands2017 p.569.
29. 10.1109/JPHOTOV.2016.255698110.1109/JPHOTOV.2016.2556981 ↗
30. 10.1063/1.494483910.1063/1.4944839 ↗
31. 10.1016/j.egypro.2016.07.01010.1016/j.egypro.2016.07.010 ↗