Reliability and degradation mechanism of AlGaAs/InGaAs and InAlAs/InGaAs HEMTs

M. Dammann, Arnulf Leuther, Fouad Benkhelifa, T. Feltgen, W. Jantz

Publisher page

Abstract

The long-term stability of AlGaAs/GaAs and InAlAs/InGaAs high electron mobility transistors (HEMTs), tested under high drain voltage and/or high temperature operation is reported. HEMTs with high In content in the active channel, alternatively fabricated on InP substrates and on GaAs substrates covered by a metamorphic buffer (MHEMT), are compared. Despite the high dislocation density in the buffer layer MHEMTs and InP based HEMTs exhibit comparable reliability. AlGaAs/GaAs HEMTs are more reliable than their InAlAs/InGaAs counterparts, especially when operated at high drain voltage. Failure mechanisms are thermally activated gate sinking, Ohmic contact degradation and hot electron induced degradation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.