Modified Ramped Current Stress Technique for Monitoring Thin Dielectrics Reliability and Charge Degradation
Source abstract
Abstract
Herein, a novel technique to monitor the quality and reliability of thin nano‐scale dielectric films is suggested. The method is based on the modification of the current stress technique (J‐Ramp) described in the corresponding JEDEC standard. The proposed technique, in addition to the J‐ramp tests, allows monitoring a change of charge state of the gate dielectric during all the tests. To implement this, in the suggested method before each transition to a higher current level, the current level is switched to the injection mode by a measurement current level and the change of voltage across the metal–insulator–semiconductor (MIS) structure is measured. A density of the measurement current level is chosen based on the condition that under this current level, a considerable charge degradation of the dielectric should not be observed, and the switches to the measurement current level should not considerably influence the studied sample. In addition to the monitoring of the charge injected until the dielectric breakdown, the proposed method allows to monitor the value of the injected charge at which the unacceptable degradation of MIS device characteristics takes place and, accordingly, to estimate the reliability of the dielectric film based on statistical measurements of these values.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · Advancements in Semiconductor Devices and Circuit Design
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Bauman Moscow State Technical University The Kaluga branch, Bazhenov st. 2 248000 Kaluga Russia
Moscow Institute of Physics and Technology (National Research University) Institutskiy per. 9 141701 Dolgoprudnyi Moscow Region Russia
References (28)
Show source-provided references
1. 10.1002/978047045526510.1002/9780470455265 ↗
2. 10.1063/1.214771410.1063/1.2147714 ↗
3. 10.1109/TED.2019.293361210.1109/TED.2019.2933612 ↗
4. Palumbo F. · Adv. Funct. Mater. · 2019 · 1900657 · 1900657
5. 10.1063/1.33522310.1063/1.335223 ↗
6. 10.1103/PhysRevB.49.1027810.1103/PhysRevB.49.10278 ↗
7. 10.1063/1.36282110.1063/1.362821 ↗
8. 10.1016/j.microrel.2012.06.00710.1016/j.microrel.2012.06.007 ↗
9. 10.1063/1.513892210.1063/1.5138922 ↗
10. 10.1063/1.488211610.1063/1.4882116 ↗
11. 10.1063/1.497991510.1063/1.4979915 ↗
12. 10.1063/1.131836910.1063/1.1318369 ↗
13. 10.1016/S0026-2714(03)00188-410.1016/S0026-2714(03)00188-4 ↗
14. 10.1016/j.microrel.2016.07.12010.1016/j.microrel.2016.07.120 ↗
15. A.Kim E.Wu B.Li B.Linder inIEEE Inter. Reliability Physics Symp. (IRPS) IEEE Monterey CA2019 p.1.10.1109/IRPS.2019.8720572 ↗
16. JEDEC Standard JESD35–A: Procedure for the Wafer–Level Testing of Thin Dielectrics 2001.
17. JEDEC Standard JESD92 Procedure for characterizing time depend dielectric breakdown of ultra-thin gate dielectrics 2003.
18. JEDEC Standard 122E Failure Mechanisms and Models tor Semiconductor Devices 2009.
19. 10.1063/1.33521910.1063/1.335219 ↗
20. 10.1002/pssc.20140011910.1002/pssc.201400119 ↗
21. 10.1088/1757-899X/168/1/01205710.1088/1757-899X/168/1/012057 ↗
22. 10.1117/12.226717310.1117/12.2267173 ↗
23. 10.1063/1.498579410.1063/1.4985794 ↗
24. 10.1002/pssa.20153241610.1002/pssa.201532416 ↗
25. 10.1016/j.sse.2005.05.00210.1016/j.sse.2005.05.002 ↗
26. 10.3390/s2008238210.3390/s20082382 ↗
27. 10.12693/APhysPolA.136.26310.12693/APhysPolA.136.263 ↗
28. 10.1002/pssc.20140015110.1002/pssc.201400151 ↗