Conductivity modification of proton conducting polymer gel electrolytes with the addition of fumed silica
Source abstract
Abstract
Abstract The addition of nano size fumed silica to non aqueous proton conducting polymer gel electrolytes containing ammonium hexafluorophosphate (NH4PF6) has been found to modify the conductivity and viscosity behavior. Two maxima observed in the conductivity vs. fumed silica plot at very low concentrations have been explained to be due to an increase in free ion concentration with the dissociation of ion aggregates, and the formation of a high conducting interfacial layer between the particles of fumed silica and polymer gel electrolytes respectively. The change in free ion concentration has been monitored by pH measurements whereas change in mobility has been checked from viscosity measurements. The dissociation of ion aggregates with the addition of fumed silica has also been supported by FTIR results. The variation of conductivity and viscosity with temperature has also been studied and conductivity of nano dispersed gels does not show any change with time. (© 2006 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advanced Battery Technologies Research · Advancements in Battery Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. 10.1007/BF0062596010.1007/BF00625960 ↗
2. 10.1016/S0378-7753(98)00232-810.1016/S0378-7753(98)00232-8 ↗
3. 10.1016/S0378-7753(00)00436-510.1016/S0378-7753(00)00436-5 ↗
4. 10.1016/S0378-7753(00)00673-X10.1016/S0378-7753(00)00673-X ↗
5. 10.1016/S0378-7753(98)00193-110.1016/S0378-7753(98)00193-1 ↗
6. 10.1016/0167-2738(82)90072-810.1016/0167-2738(82)90072-8 ↗
7. 10.1016/0167-2738(89)90185-910.1016/0167-2738(89)90185-9 ↗
8. 10.1149/1.139182410.1149/1.1391824 ↗
9. 10.1149/1.139342310.1149/1.1393423 ↗
10. 10.1038/2881810.1038/28818 ↗
11. 10.1016/S0378-7753(03)00263-510.1016/S0378-7753(03)00263-5 ↗
12. 10.1016/S0378-7753(99)00363-810.1016/S0378-7753(99)00363-8 ↗
13. 10.1016/j.ssi.2005.05.00110.1016/j.ssi.2005.05.001 ↗
14. 10.1016/S0167-2738(97)00082-910.1016/S0167-2738(97)00082-9 ↗
15. 10.1016/0379-6779(91)91788-C10.1016/0379-6779(91)91788-C ↗
16. 10.1007/BF0237555410.1007/BF02375554 ↗
17. 10.1149/1.139155910.1149/1.1391559 ↗
18. 10.1007/BF0270745410.1007/BF02707454 ↗
19. 10.1016/S0167-2738(02)00505-210.1016/S0167-2738(02)00505-2 ↗
20. 10.1016/j.eurpolymj.2005.05.01010.1016/j.eurpolymj.2005.05.010 ↗
21. J. P.SharmaandS. S.Sekhon J. Mater. Sci. available online DOI: 10.1007/s10853‐006‐6317‐1.
22. 10.1016/S0167-2738(98)00457-310.1016/S0167-2738(98)00457-3 ↗
23. A.Chandra P. C.Srivastava andS.Chandra in: Solid State Ionics: Materials and Applications edited by B. V. R. Chowdari S. Chandra S. Singh and P. C. Srivastava (World Scientific Singapore 1992) p. 397.
24. 10.1103/PhysRevLett.55.510.1103/PhysRevLett.55.5 ↗
25. 10.1021/j100182a06810.1021/j100182a068 ↗
26. 10.1016/S0167-577X(02)01065-010.1016/S0167-577X(02)01065-0 ↗
27. 10.1021/j100124a00710.1021/j100124a007 ↗
28. S. C.BrownandA. B.Harvey in: Infrared and Raman Spectroscopy edited by E. G. Brame and J. G. Grasselli (Marcel Dekker New York 1976) p. 888.
29. 10.1016/S0013-4686(03)00175-010.1016/S0013-4686(03)00175-0 ↗
30. 10.1023/A:100515122089310.1023/A:1005151220893 ↗
31. 10.1021/jp000142f10.1021/jp000142f ↗