Abstract
Polycrystalline CuInSe2 films are prepared by flash-evaporation at substrate temperatures in the range 373 to 573 K, and film dc conductivity is investigated at temperatures from 83 to 400 K. P- and n-type films are formed at substrate temperatures of 373 and above 423 K, respectively. The conduction of these films is due to thermal excitation of carriers above 290 K, which involves thermionic emission over grain boundaries. The p- and n-type films deposited at the substrate temperatures of 373 and 423 K indicate impurity conduction. At temperatures lower than 290 K, a T—1/4 dependence of conductivity is observed for the films due to variable-range hopping of carriers.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Quantum Dots Synthesis And Properties · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.