article·2002-05-01

Influences of Heat Treatment and Grain Size on the Damping Capacity of an Fe–Cr–Al Alloy

Z.C. Zhou, J.N. Wei, F.S. Han

Publisher page

Abstract

The effect of heat treatment and grain size on the damping capacity of an Fe–Cr–Al alloy with composition of (wt%) Fe–25Cr–5Al has been investigated. It has been shown that annealing temperature and grain size have a significant influence on the damping capacity and strain amplitude dependence of the alloy. Moderate annealing and grain size are necessary for a higher damping capacity, although if annealing does not yield relatively large grains, it has little effect on the damping capacity. The alloy has a rather low damping capacity after being water quenched or cold worked due to a high internal stress in the structure. It has been found that a relaxation maximum appears in the internal friction–temperature plot at about 550 °C and its activation energy is 2.6 (±0.3) eV. It is proposed that the peak originates from the Zener relaxation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Metal Alloys Wear and Properties · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.