Abstract
Due to their many benefits, especially their high hydrophobicity, silicone rubber-based composite materials gradually substitute conventional porcelain and glass insulators. However, polymeric-based materials are degraded when subjected to various external environmental stresses, which deteriorates their anticipated qualities and shortens their lifetime. This study investigates the aging characteristics of five types of high-temperature vulcanized silicone rubber (HTV-SR) filled with nano-silica/micro-alumina. Samples of materials with different specifications were subjected to various environmental conditions in a specialized weather chamber for 5000 h. The degree of deterioration was analyzed using multiple diagnostic methods: hydrophobicity categorization, fourier transform infrared spectroscopy, leakage current, mechanical property testing, and thermogravimetric analysis. The experimental results showed that SR impregnated with low-level nano silica filler revealed superior anti-aging properties compared to its high concentration and unfilled counterpart. SP-3 (2% nano-silica and 10% micro-alumina) displayed the lowest surface roughness and the best hydrophobicity among the composite test samples. In addition, the highest tensile strength (4.1 MPa) and lowest leakage current (2.5 μA) were recorded. The composite containing 2% nano-silica appears to be the highest resistance candidate to the multi-stress aging test, which can be explained by the strong molecular contact amongst nano-silica and SR.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High voltage insulation and dielectric phenomena · Dielectric materials and actuators · Advanced Sensor and Energy Harvesting Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Aging of silicone rubber-based composite insulators under multi-stressed conditions: an overview10.1088/2053-1591/ab3f0d ↗
2. Thermal distribution analysis and suppression mechanism of carbonized tracking and erosion in silicone rubber/SiO2 nanocomposites10.1016/j.polymertesting.2018.07.013 ↗
3. A review on characteristics and assessment techniques of high voltage silicone rubber insulator10.1109/TDEI.2022.3194486 ↗
4. Transfer of hydrophobicity of polymeric insulating materials for high voltage outdoor application10.1109/TDEI.2017.006146 ↗
5. Lifetime estimation and orientation effect based on long-term degradation analysis of thermoset and thermoplastic insulators10.3390/polym14193927 ↗
6. Hydrophobicity of silicone rubber used for outdoor insulation (an overview)
7. Field-dependent pollution model under polluted environments for outdoor polymeric insulators10.3390/polym14030516 ↗
8. Improved flashover performance and tracking resistance of silicone rubber by direct fluorination10.1002/app.48556 ↗
9. Effect of arc-levitating from polluted insulators' surface in the low air pressure on its DC flashover performance10.1049/iet-gtd.2010.0789 ↗
10. Pollution flashover characteristics of high-voltage outdoor insulators: analytical study10.1007/s13369-021-05745-x ↗
11. Ageing of silicone rubber insulators in coastal and inland tropical environment10.1109/TDEI.2010.5448085 ↗
12. Effect of AC corona discharge on aging of silicone rubber nanocomposites at high altitude
13. AC performance of HTV-SR and its hybrids loaded with nano-/micro-silica/ATH fillers10.1007/s13369-020-04938-0 ↗
14. Dynamic modelling of polluted outdoor insulator under wet weather conditions
15. Water absorption resistance study of HTV silicone rubber-based hybrid composites
16. Enhancement of electrical, mechanical and thermal properties of silicone based coating with aluminatrihydrate/silica for ceramic insulators10.1016/j.matchemphys.2022.125972 ↗
17. Stress control on polymeric outdoor insulators
18. Performance of silicone rubber composites with SiO2 micro/nano-filler under AC corona discharge10.1109/TDEI.2016.7736840 ↗
19. Review of the performance of high-voltage composite insulators10.3390/polym14030431 ↗
20. Degradation mechanisms of silicone rubber under different aging conditions10.1016/j.polymdegradstab.2019.108936 ↗
21. Understanding variations in the tracking and erosion performance of HTV-SR-based composites due to AC-stressed aging10.3390/polym13213634 ↗
22. Modified IEC 5000-h multistress aging of 28-kV thermoplastic elastomeric insulators10.1109/TPWRD.2007.893184 ↗
23. Accelerated ultraviolet weathering investigation on micro‐/nano‐SiO2 filled silicone rubber composites10.1049/hve.2018.5004 ↗
24. Multistress aging studies on polymeric insulators10.1109/TDEI.2018.006910 ↗
25. Degradation of high voltage polymeric insulators in arid desert's simulated environmental conditions10.3844/ajeassp.2009.438.445 ↗
26. Survey of micro/nano filler use to improve silicone rubber for outdoor insulators
27. Erosion resistance of micro-AlN and nano-SiO 2 hybrid filled silicone rubber composites
28. AC performance of HTV-SR and its hybrids loaded with nano-/micro-silica/ATH fillers10.1007/s13369-020-04938-0 ↗
29. Lifetime estimation based on surface degradation and characterization of HTV silicone-rubber based composites for HVAC and HVDC transmission
30. Influence of filler-polymer interface on performance of silicone nanocomposites10.1109/TIA.2019.2943445 ↗
31. Influence of fillers on silicone rubber for outdoor insulation
32. Polymer nanocomposites-major conclusions and achievements reached so far10.1109/MEI.2013.6648751 ↗
33. Enhanced thermal conductivity of polymer composites via hybrid fillers of anisotropic aluminum nitride whiskers and isotropic spheres10.1016/j.compositesb.2017.02.008 ↗
34. Schneider · 1992
35. A proposal for intensified inspection and acceptance tests of composite insulators as an addition to the guidelines of IEC 61109 Ed. 2: 2008 and IEC 61952 Ed. 2: 200810.1109/TDEI.2010.5448093 ↗
36. Interpreting surface degradation of HTV silicone rubber filled with micro/nano-silica under AC and DC Voltages10.1007/s11664-020-08265-w ↗
37. Guide · 1992
38. Resistance against AC corona discharge of micro-ATH/nano-Al2O3 co-filled silicone rubber composites10.1109/TDEI.2018.006914 ↗
39. AC corona resistance performance of silicone rubber composites with micro/nano silica fillers
40. Hydrophobicity loss and recovery of silicone HV insulation10.1109/TDEI.1999.9286763 ↗
41. Effects of thermal properties on tracking and erosion resistance of micro-ATH/AlN/BN filled silicone rubber composites10.1109/TDEI.2018.007125 ↗
42. Effect of AC corona discharge on hydrophobic properties of silicone rubber nanocomposites