Preparation and characterization of polypropylene/waste tyre dust blends with addition of DCP and HVA-2 (PP/WTDP-HVA2)

M. Awang, H. Ismail

Polymer Testing· Volume 27· Issue 3
Publisher page

Abstract

Abstract Preparation of polypropylene (PP)/waste tyre dust (WTD) blends with addition of dicumyl peroxide (DCP) and N,N′-m-phenylenebismaleimide (HVA-2) (PP/WTDP-HVA2) was described. The blends were characterized based on their tensile properties, swelling resistance and morphology, as well as thermal properties. The results reveal that the presence of both chemicals in PP/WTDP-HVA2 blends brought about noticeable improvements in tensile properties, swelling resistance and interfacial adhesion. The thermal stability was also improved, indicating existence of some chemical interaction between WTD and the PP matrix in the presence of both DCP and HVA-2 during processing. The results imply that both chemicals had great influences on WTD destabilization, leading to the enlargement and intensification of the copolymer formation and, hence, improved the interfacial adhesion between WTD and the PP matrix. A competing reaction mechanism that may contribute to the property enhancement of PP/WTDP-HVA2 blends was proposed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Polymer Nanocomposites and Properties · Polymer crystallization and properties · Polymer Science and PVC

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Discarded tire recycling practices in United States, Japan and Korea10.1016/S0921-3449(97)00041-4 ↗
2. Reclamation and recycling of waste rubber10.1016/S0079-6700(00)00020-4 ↗
3. Gu · 2005
4. Resource recovery from used rubber tires10.1016/S0301-4207(99)00025-2 ↗
5. Effect of curing system on the mechanical properties and heat ageing resistance of natural rubber/tire tread reclaimed rubber blends10.1016/j.polymertesting.2005.04.008 ↗
6. LDPE-based thermoplastic elastomers containing ground tire rubber with and without dynamic curing10.1016/S0141-3910(02)00007-1 ↗
7. Polypropylene-based blends containing waste tire dust: effects of trans-polyoctylene rubber (TOR) and dynamic vulcanization10.1016/j.polymertesting.2007.04.007 ↗
8. Effect of waste tire dust (WTD) size on the mechanical and morphological properties of polypropylene/waste tire dust (PP/WTD) blends10.1080/03602550600553739 ↗
9. A comparative study of the effect of degradation on the properties of PP/NR and PP/RR Blends10.1081/PPT-120029966 ↗
10. M. Awang, H. Ismail, M.A. Hazizan, Processing and properties of environment-friendly blends containing polypropylene-latex modified waste tire dust (PP/WTDML). Polym. Test. 2008, in press.10.1016/j.polymertesting.2007.09.008 ↗
11. Peroxide vulcanization of elastomers10.5254/1.3547647 ↗
12. Effect of vulcanization system on properties of thermoplastic vulcanizates based on epoxidized natural rubber/polypropylene blends10.1016/j.polymertesting.2005.09.007 ↗
13. Preparation of polypropylene/natural rubber blends having high impact strength at low temperature
14. Elliot · 1990
15. Composites of natural rubber with linear low-density polyethylene10.1002/app.1995.070580706 ↗
16. Young · 1991
17. Crystallinity changes and melting behaviour of the uniaxially oriented iPP exposed to high doses of gamma radiation10.1016/j.polymdegradstab.2004.07.021 ↗
18. Elastomeric polypropylene from alumina-supported tetraalkyl group IVB catalysts. 2. Chain microstructure, crystallinity, and morphology10.1021/ma00200a007 ↗
19. The effect of gamma radiation on the properties of polypropylene blends with styrene–butadiene–styrene copolymers10.1016/j.polymdegradstab.2003.09.020 ↗
20. Thermal degradation and mechanical properties of PET blends10.1016/j.polymdegradstab.2005.03.003 ↗
21. Thermal degradation behaviour of isotactic polypropylene blended with lignin10.1016/j.polymdegradstab.2005.01.052 ↗
22. Thermal degradation and ageing behaviour of novel thermoplastic elastomeric nylon-6/acrylate rubber reactive blends10.1016/S0141-3910(98)00044-5 ↗