Investigation of the performances for CFRP composites exposed to different aging environment at nano-scale
Source abstract
Abstract
The nanomechanical technique was applied to investigate quantitatively the evolution of epoxy matrix and fiber/matrix interface in CFRPs under different hygrothermal conditions (water, seawater and acidic solution at 20, 50 and 80 °C). The moisture penetration depth was originally defined based on the change trend of nanoindentation hardness and elastic modulus from the exposed surface to the center area of sample. The scanned modulus map of composite surface using Peak Force Quantitative Nano-mechanic (PF-QNM)) method was used to deduce the interface thickness. It was found that the moisture uptake of CFRPs in water was higher than that in seawater, but lower than that in acidic solution at the same temperature. High temperature promoted the penetration of water molecules. The moisture penetration depth was about 600 μm for the composites reaching the saturation moisture uptake in the deionized water and seawater at 80 °C, but 800 μm for the composites in the acidic solution. The interface thickness was enlarged with the moisture uptake increasing in water and seawater, which was attributed to the plasticizing effect of water molecules, whereas the acidic solution produced an inverse trend, which might be due to the secondary crosslinking reaction of free radicals.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Tribology and Wear Analysis · Mechanical Behavior of Composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Effects of hygrothermal environment on the shear behavior of composite stiffened panels [J]10.1016/j.compstruct.2020.113341 ↗
2. Impact behavior and damage characteristics of hygrothermally conditioned carbon epoxy composite laminates [J]10.1016/j.matdes.2014.09.030 ↗
3. Seawater ageing of low styrene emission resins for marine composites: mechanical behaviour and nano-indentation studies [J]10.1016/j.compositesa.2008.01.013 ↗
4. Hygrothermal aging behavior and aging mechanism of carbon nanofibers/epoxy composites [J]10.1016/j.conbuildmat.2021.123538 ↗
5. The ageing effect on static and dynamic mechanical properties of fiber reinforced polymer composites under marine environment-A review [J]10.1016/j.matpr.2021.10.084 ↗
6. Physical ageing of epoxy in a wet environment: coupling between plasticization and physical ageing [J]
7. Hygrothermal aging history of amine-epoxy resins: effects on thermo-mechanical properties [J]
8. Experimental investigation on fatigue behaviour of glass/epoxy quasi-isotropic laminate composites under different ageing conditions [J]10.1016/j.ijfatigue.2020.105992 ↗
9. Fatigue performance of single lap joints with CFRP and aluminium substrates prior and after hygrothermal aging [J]10.1111/ffe.13067 ↗
10. Effect of hygrothermal aging on the quasi-static behaviour of CFRP joints varying the overlap length [J]10.1016/j.compstruct.2019.02.035 ↗
11. Effect of hygrothermal aging on the interlaminar shear strength of a carbon fiber composite [J]10.1016/j.prostr.2019.07.063 ↗
12. Dimensional stability and mechanical performance evolution of continuous carbon fiber reinforced polyamide 6 composites under hygrothermal environment [J]10.1016/j.jmrt.2021.06.012 ↗
13. Influence of hygrothermal ageing on the mechanical properties of unidirectional carbon fiber reinforced powder epoxy composites [J]10.1016/j.compositesb.2021.109281 ↗
14. Investigation of the long term effects of moisture on carbon fiber and epoxy matrix composites [J]10.1016/j.compscitech.2012.01.010 ↗
15. Hygrothermal aging of an adhesive reinforced with microparticles of cork [J]10.1080/01694243.2015.1041358 ↗
16. Seawater ageing of low styrene emission resins for marine composites-Mechanical behaviour and nano-indentation studies [J]10.1016/j.compositesa.2008.01.013 ↗
17. Mechanical properties of materials studied from kinetic diagrams of load versus depth of impression during microimpression [J]10.1007/BF01529860 ↗
18. Determination of the Young's modulus and hysteresis by the indentation method [J]10.1134/1.1342446 ↗
19. AFM characterization of the interfacial properties of carbon fiber reinforced polymer composites subjected to hygrothermal treatments [J]10.1016/j.compscitech.2006.03.030 ↗
20. Comparative effects of humid tropical weathering and artificial ageing on a model composite properties from nano-to macro-scale [J]10.1016/j.compositesa.2014.09.028 ↗
21. Characterization of the interphase in carbon fiber/polymer composites using a nanoscale dynamic mechanical imaging technique [J]10.1016/j.carbon.2010.05.008 ↗
22. Mechanical mapping of the interphase in carbon fiber reinforced poly (ether-ether-ketone) composites using peak force atomic force microscopy Interphase shrinkage under coupled ultraviolet and hydro-thermal exposure [J]10.1016/j.polymertesting.2016.09.008 ↗
23. Hygrothermal aging mechanism of carbon fiber/epoxy resin composites based on quantitative characterization of interface structure [J]10.1016/j.polymertesting.2020.107019 ↗
24. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments [J]10.1557/JMR.1992.1564 ↗
25. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology [J]10.1557/jmr.2004.19.1.3 ↗
26. Effect of contact deformations on the adhesion of particles [J]10.1016/0021-9797(75)90018-1 ↗
27. Effects of distilled water and saline solution on the interlaminar shear strength of an aramid/epoxy composite [J]10.1016/0010-4361(91)90203-S ↗
28. In-situ observations in SEM of degradation of graphite/epoxy composite materials due to seawater immersion [J]10.1177/002199839502900701 ↗
29. Prediction of mechanical behaviour of a bulk epoxy adhesive in a marine environment [J]10.1080/00218464.2017.1377616 ↗
30. On the durability of FRP composites for aircraft structures in hygrothermal conditioning [J]10.1016/j.compositesb.2015.09.035 ↗
31. Effect of hot water immersion on the performance of carbon reinforced unidirectional poly (PEEK) composites: stress rupture under end-loaded bending, [J]10.1016/j.compositesa.2006.03.004 ↗