journal article·2011-06

Characterisation by means of a finite element model of the influence of moisture content on the mechanical and fracture properties of the polyamide 6 reinforced with short glass fibre

D. Ferreño, I. Carrascal, E. Ruiz, J.A. Casado

Polymer Testing· Volume 30· Issue 4
Publisher page

Abstract

Abstract This study involves the determination of the mechanical and fracture properties of polyamide 6 reinforced with short glass fibres (35 wt. %) at five different moisture contents (0, 1, 2, 3, and 6 wt. %, respectively). The mechanical characterisation consisted of tensile tests on plane specimens to determine the influence of moisture content on the material’s mechanical parameters. The study of fracture properties was carried out by performing single-edge notch bending tests on specimens with the levels of moisture mentioned above in order to obtain the critical stress intensity factor, K Ic . The experimental results showed that the material fracture behaviour cannot be properly described following this methodology; for this reason, a more ambitious scope was established, consisting of determining the J-integral during stable propagation by combining the experimental force vs. displacement curves with the results of a finite element numerical model. The analysis clearly demonstrates the improvement in the material’s toughness as humidity increases. The subsequent fractographic study performed through scanning electron microscopy allowed the influence of moisture content on the fracture micro-mechanisms developed during fracture and propagation to be determined.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical Behavior of Composites · Polymer crystallization and properties · Natural Fiber Reinforced Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Moisture-related Failure. Engineering Plastics
2. Carrascal · Anales de Mecánica de la Fractura · 1998 · 319
3. Moisture absorption and its influence on the tensile properties of glass fibre reinforced PA 6,6
4. The hygrothermal behaviour of glass fibre reinforced PA66 composites: a study of the effect of water absorption on their mechanical properties10.1007/BF01160550 ↗
5. Influence of absorbed moisture on fatigue crack propagation behaviour in polyamides10.1007/BF00542366 ↗
6. A study of the mechanical behaviour of a glass fibre reinforced polyamide 6,6: experimental investigation10.1016/j.polymertesting.2006.03.008 ↗
7. Fracture behaviour of glass fibre polyamide mouldings. Polym
8. ASTM D5045-99 (2007) e1. Standard Test Methods for Plane-Strain Fracture Toughness and Strain Energy Release Rate of Plastic Materials
9. ISO 13586:2000. Plastics – Determination of fracture toughness (GIC and KIC) – Linear elastic fracture mechanics (LEFM) approach.
10. Strong · 1999
11. Callister · 2006
12. Ford’s Prototype Electric Ka
13. Brydson · 1989
14. Osswald · 2006
15. Carrascal · Anales de Mecánica de la Fractura · 1999 · 221
16. Moisture Sorption mechanism of aromatic Polyamide fibers: diffusion of moisture in Poly (p-phenylene terephthalamide) fibers10.1177/004051759306300401 ↗
17. 2004 · vol. 08.03
18. ISO 527–2: 1994. Plastics. Determination of tensile properties, part 2: Test conditions for moulding and extrusion plastics.
19. Anderson · 1995
20. 2005 · vol. 03.01
21. 2005 · vol. 03.01
22. Irwin · 1956 · 289
23. Ashby · 2005 · vol. 1
24. A path independent integral and the approximate analysis of strain concentration by notches and cracks10.1115/1.3601206 ↗
25. Begley · 1972
26. Landes · 1972
27. Obtaining the J-Δa curves of an X-750 Alloy from rising load test results and iso-a curves obtained by means of finite elements model10.1016/j.engfailanal.2008.06.001 ↗
28. Maspoch. Fracture behaviour of de-aged poly(lactic acid) assessed by essential work of fracture and J-Integral methods10.1016/j.polymertesting.2010.09.004 ↗
29. Fracture characterization of ductile polymers through methods based on load separation10.1016/j.polymertesting.2008.12.004 ↗
30. J-integral evaluation of PA6 nanocomposite with improved toughness10.1016/j.polymertesting.2006.03.005 ↗
31. ANSYS User’s Manual, Release 11, 2008.