journal article·1981-04Open access

A new method for the detection of thermal oxidation in polyethylene pipes

U.W. Gedde, B. Terselius, J.-F. Jansson

Polymer Testing· Volume 2· Issue 2

Abstract

Dumb-bell shaped specimens containing the inner wall surface of the pipe cut from 12 polyethylene pipes of different origin were subjected to constant uniaxial tensile loads at 313 K in air. The brittleness of the inner wall surface layer of the thermally oxidized pipes manifested itself in a shift of the unstable/stable necking transition to lower stresses and longer times. With the aid of optical and scanning electron microscopy, the brittleness of the inner wall surface layer of the oxidized pipes was demonstrated in distinctive surface cracks, which were the dominant feature of the drawn samples of the oxidized pipes. No such surface cracks were observed in the non-oxidized samples. The surface crack patterns were characterized in terms of crack frequency (longitudinal and transverse), width of fragments of cracked top layer (lB), plastic strain of the fragments of the cracked top layer (εpl) and thickness of the cracked top layer (H). Correlations were found that can be interpreted according to basic principles of fracture mechanics. Through knowledge of, for example, εpl and lB the values of the other variables can be predicted. The thickness of the cracked top layer corrected for the reduction in thickness due to plastic deformation is approximately equal to the thickness of the oxidized layer as determined by polarized microscopy. Drawing in an Instron Tensile Testing Machine at an elongation rate of 10 mm/min at 298 K also revealed the distinctive surface cracks in the oxidized samples. On the basis of these results, a new method for the detection of thermal oxidation in polyethylene pipes is proposed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Mechanical Behavior of Composites · Material Properties and Processing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Special report: Test Application of Method for Simplified Quality Control of HDPE Pipes
2. Gedde · Polym. Test. · 1980 · 1 · 30310.1016/0142-9418(80)90013-6 ↗
3. On the Necking and Fracture Behaviour of Polyethylene
4. Terselius, B., Gedde, U. W. and Jansson, J-F.Polym. Eng. Sci., in press.
5. Holmström · 1976 · 57 · 33
6. Magill · J. Polym. Sci., Polym. Lett. · 1968 · 6 · 85310.1002/pol.1968.110061206 ↗
7. Mandelkern · J. Polym. Sci., Polym. Lett. · 1968 · 6 · 61510.1002/pol.1968.110060901 ↗
8. Magill · J. Appl. Phys. · 1964 · 35 · 324910.1063/1.1713206 ↗
9. Lindenmeyer · J. Appl. Phys. · 1964 · 35 · 5510.1063/1.1713098 ↗
10. Magill · J. Polym. Sci., Polym. Phys. Ed. · 1967 · 5 · 89
11. Hoffman · 1976
12. Hoffman · J. Res. Nat. Bur. Stand., A. Chem. Phys. · 1975 · 79A · 67110.6028/jres.079A.026 ↗
13. Maxfield · Macromolecules · 1977 · 10 · 114110.1021/ma60059a046 ↗
14. Mandelkern · J. Polym. Sci., Polym. Phys. Ed. · 1979 · 17 · 191310.1002/pol.1979.180171108 ↗
15. Gedde · Polym. Eng. Sci. · 1979 · 19 · 7710.1002/pen.760190204 ↗
16. Gedde · Polym. Eng. Sci. · 1980 · 20 · 57910.1002/pen.760200811 ↗
17. Gedde · Polym. Eng. Sci. · 1981 · 21 · 17210.1002/pen.760210310 ↗
18. Failure in Polymers
19. Arridge · Polymer · 1976 · 17 · 49510.1016/0032-3861(76)90129-4 ↗
20. Horgan · Int. J. Solids Struct. · 1974 · 10 · 83710.1016/0020-7683(74)90027-4 ↗