Abstract

Abstract A waterborne aliphatic polyurethane-based coating was studied for accelerated ultra-violet (UV), water (WT), and thermal (TH) aging for a period of 1000 h. To monitor the coating durability, samples were tested every 200 h. ATR-FTIR spectroscopy was used to monitor the chemical changes occurring during the aging process. UV–vis with integrating sphere was used to track the change in diffused reflectance, while the optical microscope and the scanning white light interferometry (SWLI) were used for surface characterization. FTIR studies of coatings subjected to UV exposure indicated a decrease in functional groups such as CO NH, C H, C O, and C O C. The appearance of functional groups such as N H is attributed to chain scission of the polyurethane binder in the coating. Investigation of the degradation mechanism in water and thermal aging showed physical effects through water penetration and the mismatch in the coefficient of thermal expansion as the primary causes of degradation. In all aging scenarios, the reduction of reflectivity was largely due to physical defects caused by the different aging mechanisms.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Polymer composites and self-healing · Building materials and conservation · Photopolymerization techniques and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Cool coatings heat up savings
2. Cool roofs, hot topic
3. Environmental Protection Agency, 40 CFR Parts 59, 1998.
4. Szycher · 1999
5. Blank · Prog. Org. Coat. · 1992 · 20 · 23510.1016/0033-0655(92)80017-Q ↗
6. Ludwick · J. Appl. Polym. Sci. · 2008 · 110 · 71210.1002/app.28523 ↗
7. Decker · Polym. Degrad. Stab. · 2004 · 83 · 30910.1016/S0141-3910(03)00276-3 ↗
8. Wang · Chin. J. Chem. · 2005 · 23 · 125710.1002/cjoc.200591257 ↗
9. Jana · High Perform. Polym. · 2010 · 22 · 310.1177/0954008308097460 ↗
10. Saha · Prog. Org. Coat. · 2011 · 70 · 37610.1016/j.porgcoat.2010.09.034 ↗
11. Teather · 2014
12. Stoye · 1998 · 161
13. Farrokhpay · Adv. Colloid Interface Sci. · 2009 · 151 · 2410.1016/j.cis.2009.07.004 ↗
14. Clayton · Surf. Coat. Int. · 1997 · 9 · 41410.1007/BF02699712 ↗
15. ASTM Standard D 4674, Standard Practice for Accelerated Testing for Color Stability of Plastics Exposed to Indoor Office Environments, Annual Book of ASTM Standard.
16. ASTM Standard D 870-02, Standard Practice for Testing Water Resistance of Coatings Using Water Immersion, Annual Book of ASTM Standard.
17. ASTM Standard D 6944-03, Standard Test Method for Resistance for Cured Coatings to Thermal Cycling, Annual Book of ASTM Standard.
18. 2007
19. Yang · Polym. Degrad. Stab. · 2001 · 74 · 34110.1016/S0141-3910(01)00166-5 ↗
20. Kim · Langmuir · 2000 · 16 · 538210.1021/la990619i ↗
21. Zhang · Polym. Degrad. Stab. · 2013 · 98 · 52710.1016/j.polymdegradstab.2012.12.003 ↗
22. Irusta · Polym. Degrad. Stab. · 1999 · 63 · 11310.1016/S0141-3910(98)00073-1 ↗
23. Pappas · J. Paint Technol. · 1974 · 46 · 65
24. Gerteis · J. Paint Technol. · 1971 · 43 · 99
25. Santos · Prog. Org. Coat. · 2005 · 54 · 34410.1016/j.porgcoat.2005.07.010 ↗
26. Santos · Mater. Corros. · 2000 · 51 · 48110.1002/1521-4176(200007)51:7<481::AID-MACO481>3.0.CO;2-G ↗
27. Stachelek · J. Biomed. Mater. Res. · 2006 · 78A · 65310.1002/jbm.a.30828 ↗
28. Boubaki · Mater. Des. · 2009 · 30 · 395810.1016/j.matdes.2009.05.038 ↗
29. Morimoto · Polym. Eng. Sci. · 1984 · 24 · 94310.1002/pen.760241202 ↗
30. Rao · J. Am. Ceram. Soc. · 1970 · 53 · 12410.1111/j.1151-2916.1970.tb12051.x ↗
31. Hummer · Powder Diffr. · 2007 · 22 · 35210.1154/1.2790965 ↗
32. McCollough · J. Gen. Appl. Phys. · 1931 · 1 · 334