journal article·2016-10

Cathodic delamination of polyurethane/multiwalled carbon nanotube composite coatings from steel substrates

N.W. Khun, G.S. Frankel

Publisher page

Abstract

Abstract Polyurethane composite coatings with different multiwalled carbon nanotube (MWCNT) contents were prepared on steel substrates to study the effect of MWCNT content on the cathodic delamination of the polyurethane composite coatings. The cathodic delamination of the polyurethane composite coatings was measured using a Scanning Kelvin Probe (SKP). An increase in MWCNT content to 0.5 wt% significantly reduced the cathodic delamination of the polyurethane composite coatings because the high density of MWCNTs blocked the transport pathways of water and oxygen molecules through the coating. It could be concluded that the incorporation of MWCNTs was a possible way to lessen the cathodic delamination of the polyurethane coatings.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Carbon Nanotubes in Composites · Smart Materials for Construction · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Hexafluorozirconic acid based surface pretreatments: characterization and performance assessment10.1016/j.electacta.2010.07.037 ↗
2. Mansfeld · 1998 · vol. 689 · 174
3. Probing photodegradation beneath the surface: a depth profiling study of UV-degraded polymeric coatings with microchemical imaging and nanoindentation10.1007/s11998-007-9052-x ↗
4. Effects of surface roughness texture and polymer degradation on cathodic delamination of epoxy coated steel samples10.1016/j.corsci.2012.10.014 ↗
5. Determination of the oxygen reduction products on ASTM A516 steel during cathodic protection10.1023/A:1003451418717 ↗
6. Cathodic delamination of polyurethane films on oxide covered steel-combined adhesion and interface electrochemical studies10.1016/j.corsci.2009.04.014 ↗
7. The scanning Kelvin probe; a new technique for the in situ analysis of the delamination of organic coatings10.1016/0300-9440(94)00542-7 ↗
8. Nanotube composites: a recipe for strength10.1038/20326 ↗
9. Exceptionally high Young’s modulus observed for individual carbon nanotubes10.1038/381678a0 ↗
10. Growth and field electron emission of vertically aligned multiwalled carbon nanotubes10.1016/S0009-2614(00)00751-X ↗
11. Tribological behavior of carbon-nanotube-filled PTFE composite10.1023/A:1024869305259 ↗
12. Novel behaviour of friction and wear of epoxy composites reinforced by carbon nanotubes10.1016/j.wear.2006.01.033 ↗
13. Elastic moduli of multi-walled carbon nanotubes and the effect of van der Waals forces10.1016/S0266-3538(03)00072-1 ↗
14. Polystyrene–acrylonitrile–CNTs nanocomposites preparations and tribological behavior research10.1016/j.wear.2008.04.021 ↗
15. Corrosion resistance of Pb–Sn composite coatings reinforced by carbon nanotubes10.1007/s11998-010-9269-y ↗
16. Galvanic function of zinc rich coatings facilitated by percolating structure of the carbon nanotubes. Part II: protection properties and mechanism of the hybrid coatings10.1016/j.porgcoat.2013.11.004 ↗
17. Corrosion behavior of multiwall carbon nanotube/magnesium composites in 3.5% NaCl10.1016/j.electacta.2011.05.082 ↗
18. The influence of carbon nanotubes on the corrosion behavior of AZ31B magnesium alloy10.1016/j.corsci.2010.08.009 ↗
19. Effect of carbon nanotubes on corrosion of Mg-CNT composites10.1016/j.corsci.2010.02.025 ↗
20. Nanocomposite of polypyrrole and alumina nanoparticles as a coating filler for the corrosion protection of aluminium alloy 2024-T310.1016/j.apsusc.2008.02.099 ↗
21. Carbon nanotube reinforced siloxane PMMA hybrid coatings with high corrosion resistance10.1016/j.porgcoat.2012.11.015 ↗
22. The delamination of polymeric coatings from steel. Part 1: calibration of the Kelvin probe and basic delamination mechanism10.1016/S0010-938X(98)00166-8 ↗
23. Potential control under thin aqueous layers using a Kelvin probe10.1016/j.corsci.2006.10.017 ↗
24. Nitrogen-induced degradation of corrosion resistance of platinum/ruthenium/nitrogen-doped diamond-like carbon thin films10.1149/1.3428724 ↗
25. Corrosion behavior of nitrogen doped diamond-like carbon thin films in NaCl solutions10.1016/j.corsci.2009.05.050 ↗
26. The delamination of polymeric coatings from steel. Part 2: first stage of delamination effect of type and concentration of cations on delamination, chemical analysis of the interface10.1016/S0010-938X(98)00167-X ↗
27. Effect of hexafluorozirconic acid pretreatment on cathodic delamination of epoxy coatings from steel substrates10.5006/1407 ↗
28. Degradation of carbon fiber-reinforced epoxy composites by ultraviolet radiation and condensation10.1177/002199802761675511 ↗
29. The delamination of polymeric coatings from electrogalvanized steel—a mechanistic approach. Part 2: delamination from a defect down to steel10.1016/S0010-938X(00)00048-2 ↗
30. Investigation of surface morphology, wear resistance, and adhesiveness of AA6061-T6 treated in a hexafluorozirconic acid-based solution10.5006/0798 ↗
31. Composition and corrosion protection of hexafluorozirconic acid treatment on steel
32. Evolution of the adsorbed water layer structure on silicon oxide at room temperature10.1021/jp053042o ↗
33. A spectroscopic technique for studies of water transport along the interface and hydrolytic stability of polymer/substrate systems10.1080/00218469908009557 ↗
34. The science of adhesion. Part 2: mechanics and mechanisms of adhesion10.1007/BF00540361 ↗
35. Annealing of a cyanurate prepolymer adhesive on aluminium and gold substrates10.1080/00218460108029596 ↗
36. Gradient of the mechanical modulus in glass-epoxy-metal joints as measured by brillouin microscopy10.1080/00218460490476973 ↗
37. Effects of carbon nanotube content on adhesion strength and wear and corrosion resistance of epoxy composite coatings on AA2024-T310.1016/j.porgcoat.2013.08.003 ↗