Abstract

A variety of weathering protocols are in use in industry and research laboratories to both replicate and accelerate the effects of weathering on coating systems. This work focuses on the use of two artificial and one natural weathering protocol (QUV, GM9540P, Florida beach exposure) in combination with spatially resolved transmission-mode Fourier transform infrared (FT-IR) spectroscopy for the purpose of chemically depth-profiling highly opaque high solids multi-layer poly(ester-urethane) coatings employed by the U.S. Department of Defense. Samples were prepared via subjection to 6/12-week GM9540P exposure, 7/13/25-week Florida beach exposure, or 6-/18-week QUV protocol. Thin (3 μm) cross-section samples were prepared via microtomy and depth-dependant trends in chemical evolutions were analyzed using transmission-mode micro-FT-IR. Scanning electron/energy-dispersive microscopy (SEM/EDS) was conducted on 10 μm cross-sections and spatial distribution/chemical makeup of inorganic constituents were analyzed. An apparent synergistic relationship between weathering protocols was found. It was theorized that a combination of chemistry and morphology of the inorganic fillers was primarily responsible for greater-than-expected photooxidative modification of the polymeric binder.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Epoxy Resin Curing Processes · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Wicks · Prog. Org. Coat. · 2002 · 44 · 16110.1016/S0300-9440(02)00002-4 ↗
2. Hare · 1994
3. Hare · 2001
4. Wilhelm · Polymer · 1997 · 38 · 401910.1016/S0032-3861(96)00984-6 ↗
5. Irusta · Polym. Degrad. Stabil. · 1999 · 63 · 11310.1016/S0141-3910(98)00073-1 ↗
6. Allen · Polym. Degrad. Stabil. · 1998 · 61 · 18310.1016/S0141-3910(97)00114-6 ↗
7. Bajsic · Polym. Degrad. Stabil. · 1996 · 52 · 22310.1016/0141-3910(95)00231-6 ↗
8. Yang · Polym. Degrad. Stabil. · 2002 · 77 · 10310.1016/S0141-3910(02)00085-X ↗
9. Yang · Polym. Degrad. Stabil. · 2003 · 80 · 5110.1016/S0141-3910(02)00382-8 ↗
10. Yang · Polym. Degrad. Stabil. · 2001 · 74 · 34110.1016/S0141-3910(01)00166-5 ↗
11. Mayne · Br. Polym. J. · 1970 · 2 · 24010.1002/pi.4980020407 ↗
12. Monney · Polym. Degrad. Stabil. · 1998 · 62 · 35310.1016/S0141-3910(98)00018-4 ↗
13. Gerlock · Polym. Degrad. Stabil. · 1998 · 62 · 22510.1016/S0141-3910(97)00279-6 ↗
14. Nichols · Polym. Degrad. Stabil. · 1997 · 56 · 8110.1016/S0141-3910(96)00198-X ↗
15. Adamsons · Prog. Org. Coat. · 2002 · 45 · 6910.1016/S0300-9440(02)00106-6 ↗
16. Duncan · Met. Finish. · 2001 · 99 · 3110.1016/S0026-0576(01)81110-7 ↗
17. Wicks · 1999
18. 1991 · vol. 6.02
19. Q-Panel Lab Products, Q-SUN Xenon Test Chamber Operating Manual, 2002, p. 22.
20. 1999 · vol. 14.04
21. Allen · Polym. Degrad. Stabil. · 2002 · 76 · 30510.1016/S0141-3910(02)00027-7 ↗
22. Pavia · 1996
23. Lin-Vien · 1991
24. Miyazawa · J. Chem. Phys. · 1955 · 24 · 40810.1063/1.1742489 ↗
25. Serra · J. Non-Cryst. Solids · 2003 · 332 · 2010.1016/j.jnoncrysol.2003.09.013 ↗