journal article·2021-01Open access

Advancing reliability assessments of photovoltaic modules and materials using combined‐accelerated stress testing

Michael Owen‐Bellini, Peter Hacke, David C. Miller, Michael D. Kempe, Sergiu Spataru, Tadanori Tanahashi, Stefan Mitterhofer, Marko Jankovec, Marko Topič

Abstract

Abstract Previously undiscovered failure modes in photovoltaic (PV) modules continue to emerge in field installations despite passing protocols for design qualification and quality assurance. Failure to detect these modes prior to widespread use could be attributed to the limitations of present‐day standard accelerated stress tests (ASTs), which are primarily designed to identify known degradation or failure modes at the time of development by applying simultaneous or sequential stress factors (usually two at most). Here, we introduce an accelerated testing method known as the combined‐accelerated stress test (C‐AST), which simultaneously combines multiple stress factors of the natural environment. Simultaneous combination of multiple stress factors allows for improved identification of failure modes with better ability to detect modes not known a priori. A demonstration experiment was conducted that reproduced the field‐observed cracking of polyamide‐ (PA‐) and polyvinylidene fluoride (PVDF)–based backsheet films, a failure mode that was not detected by current design qualification and quality assurance testing requirements. In this work, a two‐phase testing protocol was implemented. The first cycle (“Tropical”) is a predominantly high‐humidity and high‐temperature test designed to replicate harsh tropical climates. The second cycle (“Multi‐season”) was designed to replicate drier and more temperate conditions found in continental or desert climates. Testing was conducted on 2 × 2‐cell crystalline‐silicon cell miniature modules constructed with both ultraviolet (UV)–transmitting and UV‐blocking encapsulants. Cracking failures were observed within a cumulative 120 days of the Tropical condition for one of the PA‐based backsheets and after 84 days of Tropical cycle followed by 42 days of the Multi‐season cycle for the PVDF‐based backsheet, which are both consistent with failures seen in fielded modules. In addition to backsheet cracking, degradation modes were observed including solder/interconnect fatigue, various light‐induced degradation modes, backsheet delamination, discoloration, corrosion, and cell cracking. The ability to simultaneously apply multiple stress factors may allow many of the test sequences within the standardized design qualification procedure to be performed using a single test setup.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Integrated Circuits and Semiconductor Failure Analysis · Silicon and Solar Cell Technologies · Photovoltaic System Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Renewable Energy Laboratory Golden CO 80401 USA

DTU Fotonik Frederiksborgvej 399, Building 130 Roskilde 4000 Denmark

Renewable Energy Research Center National Institute of Advanced Industrial Science and Technology (AIST) Fukushima 963‐0298 Japan

Faculty of Electrical Engineering University of Ljubljana Tržaška cesta 25 Ljubljana SI‐1000 Slovenia

Funding

Javna Agencija za Raziskovalno Dejavnost RS · U.S. Department of Energy

References (57)

Show source-provided references
1. International Electrotechnical Commision.IEC 61215‐2: crystalline silicon terrestrial photovoltaic (PV) modules—design qualification and type approval.International Electrotechnical Commission.2016.
2. 10.1016/B978-0-12-814501-2.00011-610.1016/B978-0-12-814501-2.00011-6 ↗
3. WohlgemuthJ.IEC 61215: what it is and isn't (presentation) NREL (National Renewable Energy Laboratory). inNREL Photovoltaic Reliability Workshop.2012.
4. FischerRM KetolaWD.Error analyses and associated risk for accelerated weathering results. in3rd International Service Life Symposium.2004.
5. Evaluation of the uncertainty in accelerated stress testing
6. 10.1109/JPHOTOV.2014.230547210.1109/JPHOTOV.2014.2305472 ↗
7. Potential induced degradation of solar cells and panels
8. 10.1109/PVSC.2010.561447210.1109/PVSC.2010.5614472 ↗
9. A new mc‐Si degradation effect called LeTID
10. Understanding the snail trail effect in silicon solar modules on microstructural scale
11. ChoudhuryKR.Material degradation impacting performance of PV modules in the field. inNREL Photovoltaic Reliability Workshop.2019.
12. IEC TS 62788–7‐2.Measurement procedures for materials used in photovoltaic modules—Part 7‐2: environmental exposures—accelerated weathering tests of polymeric materials.
13. 10.1002/pip.258010.1002/pip.2580 ↗
14. GambogiW MacMasterS YuBL et al.Sequential testing that better predicts field performance. in4th Atlas‐NIST Workshop.2017.
15. GambogiW.Sequential stress testing to predict photovoltaic module durability. in7th World Conference on Photovoltaic Energy Conversion.2018.10.1109/PVSC.2018.8547260 ↗
16. SpataruS HackeP Owen‐BelliniM.Combined‐accelerated stress testing system for photovoltaic modules. inProceedings of 45th IEEE Photovoltaics Specialists Conference.2018.10.1109/PVSC.2018.8547335 ↗
17. Owen‐BelliniM Sulas‐KernDB SpataruS NorthH HackeP.In‐situ performance characterization of photovoltaic modules during combined‐accelerated stress testing. in46th IEEE Photovoltaics Specialist Conference.2019.10.1109/PVSC40753.2019.9198956 ↗
18. KempeMD LockmanT MorseJ.Development of testing methods to predict cracking in photovoltaic backsheets. in46th IEEE Photovoltaics Specialist Conference.2019.10.1109/PVSC40753.2019.8980818 ↗
19. 10.1016/j.solmat.2019.11008210.1016/j.solmat.2019.110082 ↗
20. 10.1016/j.solmat.2019.11019410.1016/j.solmat.2019.110194 ↗
21. 10.1109/JPHOTOV.2018.286378910.1109/JPHOTOV.2018.2863789 ↗
22. 10.1002/pip.286110.1002/pip.2861 ↗
23. HolleyWH AgroSC GalicaJP et al.Investigation into the causes of browning in EVA encapsulated flat\nplate PV modules.Proc. 1994 IEEE 1st World Conf. Photovolt. Energy Convers. ‐ WCPEC (A Jt. Conf. PVSC PVSEC PSEC).1994;1:893‐896.10.1109/WCPEC.1994.520105 ↗
24. 10.1016/j.solener.2014.06.02710.1016/j.solener.2014.06.027 ↗
25. 10.1016/0927-0248(92)90013-F10.1016/0927-0248(92)90013-F ↗
26. HartmanK HackeP Owen‐BelliniM et al.Validation of advanced photovoltaic module materials and processes by combined‐accelerated stress testing (C‐AST). in46th IEEE Photovoltaics Specialist Conference.2019.10.1109/PVSC40753.2019.8980545 ↗
27. International A.ASTM G155—standard practive for operating xenon arc light apparatus for exposure of non‐metallic materials.2013.
28. International A.ASTM D7869‐17 standard practice for xenon arc exposure test with enhanced light and water exposure for transportation coatings.2017.https://doi.org/10.1520/D7869-1710.1520/D7869-17 ↗
29. 10.5194/hess-11-1633-200710.5194/hess-11-1633-2007 ↗
30. 10.1002/pip.86110.1002/pip.861 ↗
31. 10.1002/pip.110310.1002/pip.1103 ↗
32. 10.1016/j.solmat.2011.01.02010.1016/j.solmat.2011.01.020 ↗
33. 10.1109/JPHOTOV.2016.258377910.1109/JPHOTOV.2016.2583779 ↗
34. 10.1175/1520-0450(1996)035<0601:IMFAOS>2.0.CO;210.1175/1520-0450(1996)035<0601:IMFAOS>2.0.CO;2 ↗
35. 10.1038/sdata.2018.21410.1038/sdata.2018.214 ↗
36. Owen‐belliniM BettsTR.Thermo‐mechanical stresses of silicon photovoltaic modules.2017.
37. 10.1109/PVSC.2017.836673710.1109/PVSC.2017.8366737 ↗
38. 10.1109/JPHOTOV.2020.297113910.1109/JPHOTOV.2020.2971139 ↗
39. International Electrotechnical Commision.IEC 60904‐1 photovoltaic devices part 1: measurement of photovoltaic current‐voltage characteristics.2006.
40. Owen‐BelliniM MillerDC SchelhasLT et al.Correlation of advanced accelerated stress testing with polyamide‐based photovoltaic backsheet field‐failures. in46th IEEE Photovoltaics Specialist Conference.2019.10.1109/PVSC40753.2019.8980750 ↗
41. 10.1002/pip.326010.1002/pip.3260 ↗
42. Owen‐BelliniM HackeP SpataruS MillerDC KempeMD.Combined‐accelerated stress testing for advanced reliability assessment of photovoltaic modules. in35th European PV Solar Energy Conference and Exhibition.2018.
43. TanahashiT SakuraiK ShiodaT et al.Reproducing the “framing” by a sequential stress test. in46th IEEE Photovoltaics Specialist Conference.2019.10.1109/PVSC40753.2019.8980920 ↗
44. 10.1016/j.egypro.2016.10.08310.1016/j.egypro.2016.10.083 ↗
45. 10.1002/pen.76021090810.1002/pen.760210908 ↗
46. 10.1016/j.solmat.2011.01.03110.1016/j.solmat.2011.01.031 ↗
47. 10.1557/jmr.2004.19.1.310.1557/jmr.2004.19.1.3 ↗
48. 10.1002/pip.314410.1002/pip.3144 ↗
49. 10.1016/j.solener.2005.02.00810.1016/j.solener.2005.02.008 ↗
50. 10.1021/ma050390f10.1021/ma050390f ↗
51. 10.1016/j.solmat.2018.09.01010.1016/j.solmat.2018.09.010 ↗
52. 10.1002/pip.58610.1002/pip.586 ↗
53. Understanding light‐induced degradation of c‐Si solar cells
54. 10.1002/pip.77910.1002/pip.779 ↗
55. 10.1016/j.egypro.2015.07.01210.1016/j.egypro.2015.07.012 ↗
56. Light induced degradation of rear passivated mc‐Si solar cells
57. 10.1016/j.solener.2018.06.04410.1016/j.solener.2018.06.044 ↗