Hydrogenated amorphous silicon p–i–n solar cells deposited under well controlled ion bombardment using pulse‐shaped substrate biasing
Source abstract
Abstract
ABSTRACT We applied pulse‐shaped biasing (PSB) to the expanding thermal plasma deposition of intrinsic hydrogenated amorphous silicon layers at substrate temperatures of 200 °C and growth rates of about 1 nm/s. Fourier transform infrared spectroscopy of intrinsic films showed a densification with increasing deposited energy and a reduction in void content, whereas dual‐beam photoconductivity measurements showed an increase in Urbach energy above 4.8 eV/Si atom. From dark conductivity and photoconductivity measurements, we determined a maximum photoresponse of 2 × 106 at 3 eV/Si atom, which decreased at higher deposited energies because of a higher dark conductivity as a result of a lower band gap. p–i–n solar cells with PSB applied during the intrinsic layer deposition showed initial energy conversion efficiencies of 7.4% at around 1 eV/Si atom. Decreasing open‐circuit voltage at >1 eV/Si atom can be related to a lower band gap, whereas the short‐circuit current drops at >4.8 eV/Si atom, predominantly because of hole collection losses as determined from quantum efficiency measurements. The reduced fill factor for >1 eV/Si atom was presumably related to a decrease in mobility‐lifetime product because of an increase in defect density. Copyright © 2011 John Wiley & Sons, Ltd.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Thin-Film Transistor Technologies · Silicon and Solar Cell Technologies · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Photovoltaic Materials and Devices Group/DIMES Delft University of Technology PO Box 5053 Delft 2600 GB The Netherlands
Department of Applied Physics, Plasma and Material Processing Group Eindhoven University of Technology 5600 MB Eindhoven The Netherlands
Funding
Ministry of Economic Affairs, Agriculture and Innovation
References (21)
Show source-provided references
1. 10.1002/047001400810.1002/0470014008 ↗
2. 10.1063/1.36897710.1063/1.368977 ↗
3. vanErvenAJM RCMBosch WeeberAW BijkerMD.Effects of different firing profiles on layer characteristics and passivation properties of industrial deposited silicon nitride films.19th European Photovoltaic Solar Energy Conference and Exhibition 2004.
4. 10.1088/0963-0252/19/1/01501210.1088/0963-0252/19/1/015012 ↗
5. 10.1063/1.278687310.1063/1.2786873 ↗
6. 10.1063/1.289010010.1063/1.2890100 ↗
7. 10.1088/0963-0252/8/3/20210.1088/0963-0252/8/3/202 ↗
8. 10.1063/1.37371510.1063/1.373715 ↗
9. 10.1063/1.322569010.1063/1.3225690 ↗
10. 10.1063/1.350579410.1063/1.3505794 ↗
11. Real time spectroscopic ellipsometry on ultrathin (<50 Å) hydrogenated amorphous silicon films on Si(100) and GaAs(100)
12. 10.1063/1.179335910.1063/1.1793359 ↗
13. 10.1103/PhysRevE.72.03640710.1103/PhysRevE.72.036407 ↗
14. The defect density in amorphous silicon.
15. 10.1063/1.12136710.1063/1.121367 ↗
16. 10.1002/(SICI)1521-396X(199810)169:2<239::AID-PSSA239>3.0.CO;2-F10.1002/(SICI)1521-396X(199810)169:2<239::AID-PSSA239>3.0.CO;2-F ↗
17. 10.1016/0379-6787(80)90028-910.1016/0379-6787(80)90028-9 ↗
18. 10.1103/PhysRevLett.81.368310.1103/PhysRevLett.81.3683 ↗
19. 10.1002/pip.51810.1002/pip.518 ↗
20. Green MA · 1992
21. 10.1063/1.9483010.1063/1.94830 ↗