Abstract
Abstract The corrosion of glassy (Ni 8 Nb 5 ) 99.5 Sb 0.5 alloy was investigated in 1, 6 mol/L HCl, 1 mol/L H 2 SO 4 and 3% NaCl solutions, respectively, by immersion tests and electrochemical measurements and compared with that of pure Ni, Nb and Sb. The stability of passive film was studied using potentiostatic current transients and XPS depth profiling. The surface morphology of the glassy alloy after electrochemical potentiodynamic polarization test was observed using SEM. The result indicates that the Ni-Nb-Sb alloy shows good corrosion resistance in 1 mol/L HCl, 1 mol/L H 2 SO 4 and 3 wt% NaCl solutions. The corrosion resistance, however, is poor in 6 mol/L HCl solution. The amorphous alloy is crystallized after electrochemical corrosion in chloride media. Transpassive dissolution is observed during potentiodynamic polarization test in chloride media, which appears to be associated with oxygen evolution. At low potentials, the growth of passive film is diffusion-controlled. At high potentials, however, the active corrosion is the predominant.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Electrodeposition and Electroless Coatings · Nanoporous metals and alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Inoue · Mater Sci Eng A[J] · 1997 · 226–228 · 40110.1016/S0921-5093(97)80051-2 ↗
2. Inoue · Mater Trans JIM[J] · 2002 · 43 · 195210.2320/matertrans.43.1952 ↗
3. Zhang · Mater Trans JIM[J] · 2002 · 43 · 70810.2320/matertrans.43.708 ↗
4. Lee · J Mater Res[J] · 2003 · 18 · 210110.1557/JMR.2003.0295 ↗
5. Zhang · Mater Trans JIM[J] · 2003 · 44 · 232210.2320/matertrans.44.2322 ↗
6. Wang · J Mater Res[J] · 2007 · 22 · 110.1557/jmr.2007.0020 ↗
7. Greer · International Materials Reviews[J] · 2002 · 47 · 8710.1179/095066001225001067 ↗
8. Wang · Mater Trans JIM[J] · 1999 · 40 · 113010.2320/matertrans1989.40.1130 ↗
9. Pang · Mater Trans[J] · 2002 · 43 · 177110.2320/matertrans.43.1771 ↗
10. Liu · J Mater Res[J] · 2007 · 22 · 86910.1557/jmr.2007.0104 ↗
11. Yi · J Mater Res[J] · 2000 · 15 · 242510.1557/JMR.2000.0348 ↗
12. Lee · Intermetallics[J] · 2004 · 12 · 113310.1016/j.intermet.2004.04.027 ↗
13. Habazaki · Mater Sci Eng A[J] · 2001 · 304 · 69610.1016/S0921-5093(00)01571-9 ↗
14. Hu · J Alloy Compd[J] · 2008 · 460 · 71410.1016/j.jallcom.2008.01.075 ↗
15. Zhu · Mater Sci Eng A[J] · 2008 · 492 · 22110.1016/j.msea.2008.04.021 ↗
16. Tan · Materials Chemistry and Physics[J] · 2008 · 108 · 2910.1016/j.matchemphys.2007.08.036 ↗
17. Zhang · J Alloy Compd[J] · 2010 · 491 · 51310.1016/j.jallcom.2009.10.259 ↗
18. Brandice · 2008 · 218
19. Pavlov · Electrochim Acta[J] · 1991 · 36 · 208110.1016/0013-4686(91)85213-Q ↗
20. Schultze · Electrochim Acta[J] · 1983 · 28 · 97310.1016/0013-4686(83)85175-5 ↗
21. Pang · Corrosion Science[J] · 2006 · 48 · 62510.1016/j.corsci.2005.02.013 ↗
22. Lohrengel · Mater Sci Eng R[J] · 1993 · 11 · 110.1016/0927-796X(93)90007-P ↗
23. Massiani · J Non-cryst Solid[J] · 1993 · 159 · 9210.1016/0022-3093(93)91286-C ↗
24. Gebert · Mater Sci Eng A[J] · 1999 · 267 · 29410.1016/S0921-5093(99)00105-7 ↗