Preparation and Property of Novel-Type Au-19.25Ag-12.80Ge Solder Alloy
Source abstract
Abstract
Abstract According to Au-Ag-Ge phase diagram, a novel-type Au-19.25Ag-12.80Ge (mass fraction,%) solder alloy was prepared. The melting characteristic and microstructure of the solder was analyzed by DTA and scanning electron microscope, and its wettability with pure Ni was also studied. The results show that its melting temperature range is 446.76–494.40 °C, and the temperature interval between the solidus and the liquidus is 47.64 °C. When the soldering temperature is in the range of 510–550 °C, the solder alloy has a good wettability with Ni and a wetting ring appears. The interface structure observation reveals that there is one obvious diffusion layer between the solder alloy and base metal; X-ray energy spectrum analysis results show that the diffusion layer is Ge-Ni intermetallics. Thin strip solder alloy with a thickness of 0.1 mm can be prepared by the technique of hot-rolling after coated with aluminum alloy then cold-rolling together with intermediate annealing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Zhang · 1999 · 14
2. Jiang · Rare Metal Materials and Engineering · 2003 · 32 · 295
3. Yue · The Chinese Journal of Nonferrous Metals · 2006 · 16 · 1793
4. Mo · Precious Metals · 2004 · 25 · 45
5. Mo · Rare Metal Materials and Engineering · 2005 · 34 · 497
6. He · 1983 · 19
7. Borzone · Metallurgical Transactions A · 1989 · 20A · 216710.1007/BF02650302 ↗
8. Zhuang · 1989 · 152
9. Li · 1991 · 320
10. Ren · Acta Metallurgica Sinica · 2002 · 38 · 727