journal article·2012-04

Investigation of CMP of Ni in the Preparation Process of Micro-Electro-Mechanical System Devices

Chu Xiangfeng, Li Xiujin, Dong Yongping, Zhang Wangbing, Bai Linshan

Publisher page

Abstract

Abstract CMP (chemical mechanical polish) experiments were carried out by using high purity nickel and home-made slurry. The effects of polishing down force, pH value, H 2 O 2 concentration, chelating agent species and their concentration as well as particle concentration on the material removal rate (MRR) were investigated. The results reveal that MRR can reach 312.3 nm/min under the following conditions: the down force is 13.79 kPa, H 2 O 2 concentration is 0.5% (mass fraction), pH = 3.0, SiO 2 concentration is 0.5% and EDTA concentration is 1%, The better surface quality can be obtained under the following conditions: the down force is 13.79 kPa, H 2 O 2 concentration is 1%, pH = 4.0, SiO 2 concentration is 1%, EDTA concentration is 1%, and the surface roughness R a can reach 5 nm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Advanced machining processes and optimization · Advanced Machining and Optimization Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Allameh · Materials Science and Engineering A[J] · 2004 · 371 · 25610.1016/j.msea.2003.12.020 ↗
2. Hemker · Materials Science and Engineering A[J] · 2001 · 319–321 · 88210.1016/S0921-5093(01)00956-X ↗
3. Lou · Materials Science and Engineering A[J] · 2006 · 441 · 29910.1016/j.msea.2006.08.048 ↗
4. Du · Microelectronic Engineering[J] · 2004 · 75 · 23410.1016/j.mee.2004.05.007 ↗
5. Kourouklis · Sensors and Actuators A[J] · 2003 · 106 · 26310.1016/S0924-4247(03)00180-8 ↗
6. Du · Journal of Materials Science Letters[J] · 2003 · 22 · 162310.1023/A:1026353028626 ↗
7. Anik · Journal of Applied Electrochemistry[J] · 2005 · 35 · 110.1007/s10800-004-1763-4 ↗
8. Xing · Chinese Journal of Semiconductors[J] · 2004 · 25 · 1726
9. Xin · Wear[J] · 2010 · 268 · 83710.1016/j.wear.2009.12.005 ↗
10. Qin · Thin Solid Films[J] · 2004 · 446 · 27710.1016/j.tsf.2003.09.060 ↗