Microstructure and properties of aging Cu–Cr–Zr alloy
Source abstract
Abstract
Abstract The crystallography and morphology of precipitate particles in a Cu matrix were studied using an aged Cu–Cr–Zr alloy by transmission electron microscopy (TEM) and high‐resolution transmission electron microscopy (HRTEM). The tensile strength and electrical conductivity of this alloy after various aging processes were tested. The results show that two kinds of crystallographic structure associated with chromium‐rich phases, fcc and bcc structure, exist in the peak‐aging of the alloy. The orientation relationship between bcc Cr precipitate and the matrix exhibits Nishiyama–Wasserman orientation relationship. Two kinds of Zr‐rich phases (Cu 4 Zr and Cu 5 Zr) can be identified and the habit plane is parallel to {111} Cu plane during the aging. The increase in strength is ascribed to the precipitation of Cr‐ and Zr‐rich phase.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and mechanical properties · Copper Interconnects and Reliability · Nanoporous metals and alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
No. 23 Research Institute China Electronics Technology Group Corporation 201900 Shanghai China
Institute of Electric Lighting Source Fudan University 200433 Shanghai China
References (26)
Show source-provided references
1. 10.1016/S0022‐3115(01)00691‐210.1016/S0022‐3115(01)00691‐2 ↗
2. 10.1016/S1359‐6462(02)00350‐010.1016/S1359‐6462(02)00350‐0 ↗
3. 10.1007/BF0258615810.1007/BF02586158 ↗
4. 10.1016/S0022‐3115(99)00285‐810.1016/S0022‐3115(99)00285‐8 ↗
5. 10.1016/j.jnucmat.2008.12.26610.1016/j.jnucmat.2008.12.266 ↗
6. 10.1016/S0921‐5093(98)01149‐610.1016/S0921‐5093(98)01149‐6 ↗
7. 10.1016/j.actamat.2012.01.03810.1016/j.actamat.2012.01.038 ↗
8. 10.1016/j.matlet.2007.03.08510.1016/j.matlet.2007.03.085 ↗
9. 10.1007/BF0266938010.1007/BF02669380 ↗
10. 10.1016/0036‐9748(86)90154‐710.1016/0036‐9748(86)90154‐7 ↗
11. 10.1016/0001‐6160(88)90244‐110.1016/0001‐6160(88)90244‐1 ↗
12. 10.1016/0001‐6160(79)90072‐510.1016/0001‐6160(79)90072‐5 ↗
13. 10.1007/BF0265841310.1007/BF02658413 ↗
14. 10.1023/A:100431070084610.1023/A:1004310700846 ↗
15. 10.1016/S1359‐6454(99)00411‐510.1016/S1359‐6454(99)00411‐5 ↗
16. 10.2320/matertrans.MBW20073610.2320/matertrans.MBW200736 ↗
17. 10.1016/S0921-5093(02)00852-310.1016/S0921-5093(02)00852-3 ↗
18. 10.1179/mst.1985.1.4.27010.1179/mst.1985.1.4.270 ↗
19. Hot‐compression deformation behavior of Cu–Cr–Zr alloy
20. 10.1179/174328407X18584810.1179/174328407X185848 ↗
21. 10.1007/s10853‐007‐2159‐810.1007/s10853‐007‐2159‐8 ↗
22. 10.1016/j.actamat.2009.12.00410.1016/j.actamat.2009.12.004 ↗
23. 10.1016/j.jallcom.2011.04.14110.1016/j.jallcom.2011.04.141 ↗
24. 10.1016/j.actamat.2007.01.03710.1016/j.actamat.2007.01.037 ↗
25. 10.1007/BF0073783910.1007/BF00737839 ↗
26. 10.1007/s12598‐013‐0074‐510.1007/s12598‐013‐0074‐5 ↗