Fabrication of nano‐grained negative temperature coefficient thermistors with high electrical stability
Source abstract
Abstract
Abstract Dense nano‐grained Ni 0.7 Mn 2.3 O 4 negative temperature coefficient (NTC) thermistors were fabricated by a novel two‐step sintering approach that combines rapid sintering and principle of conventional two‐step sintering technique. Samples were sintered at 1042 °C for 30 s in the first rapid step and then at 850–950 °C for 20 h in the second soaking step. Crystal phase, microstructure and electrical properties of sintered samples were studied by X‐ray diffraction (XRD), scanning electron microscopy (SEM), resistance temperature relationship and aging performance. Sintered samples show a single‐phase cubic spinel structure and indicate a high relative density ranging from 84% to 91% of the theoretical density. Moreover, average grain sizes of sintered samples under SEM are distributed between 254 and 570 nm. Meanwhile, the resistivity and the aging coefficient significantly decrease when soaking sintering temperature rises. In addition, the obtained material constant ( B ) ranges from 3931 to 3981 K. Ni 0.7 Mn 2.3 O 4 ‐3 (soaking at 900 °C) and Ni 0.7 Mn 2.3 O 4 ‐4 (soaking at 950 °C) present little aging behavior, implying great electrical stability.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electrical and Thermal Properties of Materials · Ferroelectric and Piezoelectric Materials · Advanced Sensor Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Ningxia Key Laboratory of Photovoltaic Materials Ningxia University 750021 Yinchuan China
School of Materials Science and Engineering North Minzu University 750021 Yinchuan China
Funding
National Natural Science Foundation of China
References (32)
Show source-provided references
1. 10.1016/j.jallcom.2012.04.03810.1016/j.jallcom.2012.04.038 ↗
2. 10.1007/s10854-017-6361-410.1007/s10854-017-6361-4 ↗
3. 10.1111/j.1551‐2916.2009.02990.x10.1111/j.1551‐2916.2009.02990.x ↗
4. 10.1016/j.ssi.2007.01.02810.1016/j.ssi.2007.01.028 ↗
5. 10.1111/j.1551‐2916.2009.03289.x10.1111/j.1551‐2916.2009.03289.x ↗
6. 10.1016/j.scriptamat.2007.04.02610.1016/j.scriptamat.2007.04.026 ↗
7. 10.1016/j.jallcom.2008.07.07610.1016/j.jallcom.2008.07.076 ↗
8. 10.3724/SP.J.1077.2009.0100810.3724/SP.J.1077.2009.01008 ↗
9. 10.1016/S0921‐5107(02)00538‐X10.1016/S0921‐5107(02)00538‐X ↗
10. 10.1016/j.ceramint.2005.10.01010.1016/j.ceramint.2005.10.010 ↗
11. 10.17222/mit.2015.22810.17222/mit.2015.228 ↗
12. 10.1016/j.ceramint.2016.05.06510.1016/j.ceramint.2016.05.065 ↗
13. 10.1016/j.ssi.2010.02.00810.1016/j.ssi.2010.02.008 ↗
14. 10.1038/3500454810.1038/35004548 ↗
15. 10.1111/j.1551‐2916.2005.00728.x10.1111/j.1551‐2916.2005.00728.x ↗
16. 10.1016/j.jeurceramsoc.2018.02.03710.1016/j.jeurceramsoc.2018.02.037 ↗
17. Synthesis of dense, fine‐grained hexagonal barium ferrite ceramics by two‐step sintering process
18. 10.1039/C5RA26760A10.1039/C5RA26760A ↗
19. 10.1016/j.ceramint.2013.12.13310.1016/j.ceramint.2013.12.133 ↗
20. Zirconia films prepared by sol‐gel method on surface of ZrH1.8 in different heat treatment atmospheres
21. Fabrication of high strength scandium oxide ceramics
22. 10.1179/174328008X25435810.1179/174328008X254358 ↗
23. 10.1016/j.jeurceramsoc.2008.05.04310.1016/j.jeurceramsoc.2008.05.043 ↗
24. 10.1007/s10853‐012‐6282‐910.1007/s10853‐012‐6282‐9 ↗
25. 10.1016/j.matlet.2017.02.01010.1016/j.matlet.2017.02.010 ↗
26. 10.1142/S0219581X1100824110.1142/S0219581X11008241 ↗
27. 10.1016/j.jeurceramsoc.2006.07.00210.1016/j.jeurceramsoc.2006.07.002 ↗
28. 10.1016/j.jeurceramsoc.2014.03.02510.1016/j.jeurceramsoc.2014.03.025 ↗
29. 10.1016/j.jallcom.2013.08.01410.1016/j.jallcom.2013.08.014 ↗
30. 10.1007/s10854-018-8927-110.1007/s10854-018-8927-1 ↗
31. 10.1016/j.jallcom.2016.03.13910.1016/j.jallcom.2016.03.139 ↗
32. 10.1007/s10832‐008‐9467‐510.1007/s10832‐008‐9467‐5 ↗