Effects of minor Sc on the microstructure and mechanical properties of Al‐Zn‐Mg‐Cu‐Zr based alloys
Source abstract
Abstract
Abstract Five kinds of Al‐Zn‐Mg‐Cu‐Zr based alloys with different Sc additions were prepared by ingot metallurgy. The effects of minor Sc on the microstructure and mechanical properties of Al‐Zn‐Mg‐Cu‐Zr based alloys were investigated using tensile tests, optical microscopy (OM), and transmission electron microscopy (TEM). The results show that the ultimate tensile strength and yield strength are improved by 94 and 110 MPa, respectively, and the elongation to failure remains at a reasonable extent (11.1%) in the Al‐Zn‐Mg‐Cu‐Zr based alloy with 0.21 wt.% Sc addition after solution heat treatment at 475°C for 40 min and then aged at 120°C for 24 h. The addition of minor Sc induces the formation of Al 3 (Sc,Zr) particles, which are highly effective in refining the cast microstructures, retarding recrystallization, and pinning dislocations. The increment of strength is attributed mainly to fine grain strengthening, precipitation strengthening of Al 3 (Sc,Zr) particles, and substructure strengthening.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering Central South University Changsha 410083 China
Department of Civil Engineering Hunan City University Yiyang 413000 China
References (15)
Show source-provided references
1. 10.4028/www.scientific.net/MSF.331-337.124910.4028/www.scientific.net/MSF.331-337.1249 ↗
2. 10.4028/0‐87849‐960‐1.253910.4028/0‐87849‐960‐1.2539 ↗
3. 10.1007/s11661‐005‐0332‐810.1007/s11661‐005‐0332‐8 ↗
4. 10.4028/www.scientific.net/MSF.331-337.110710.4028/www.scientific.net/MSF.331-337.1107 ↗
5. Effect of minor Sc and Zr on microstructures and mechanical properties of Al‐Zn‐Mg based alloys
6. 10.1007/s11661‐999‐0154‐110.1007/s11661‐999‐0154‐1 ↗
7. 10.1016/j.msea.2003.10.37410.1016/j.msea.2003.10.374 ↗
8. 10.4028/www.scientific.net/MSF.396-402.75710.4028/www.scientific.net/MSF.396-402.757 ↗
9. 10.1016/S1359‐6454(01)00050‐710.1016/S1359‐6454(01)00050‐7 ↗
10. 10.1007/s11661‐004‐0135‐310.1007/s11661‐004‐0135‐3 ↗
11. 10.1016/S1001‐0521(08)60105‐910.1016/S1001‐0521(08)60105‐9 ↗
12. 10.4028/www.scientific.net/MSF.396‐402.115110.4028/www.scientific.net/MSF.396‐402.1151 ↗
13. 10.1007/s11771‐000‐0033‐910.1007/s11771‐000‐0033‐9 ↗
14. 10.1016/S1003‐6326(06)60406‐810.1016/S1003‐6326(06)60406‐8 ↗
15. 10.4028/www.scientific.net/MSF.396-402.112710.4028/www.scientific.net/MSF.396-402.1127 ↗