Manufacturing of cast A356 matrix composite reinforced with nano‐ to micrometer‐sized SiC particles
Source abstract
Abstract
Abstract In this study, large micron‐sized SiC particles were fragmented via ball‐milling process in the presence of iron and nickel powders, separately, to fabricate composite powders of Fe–SiC and Ni–SiC. Continuous fracturing of brittle SiC powders leads to the formation of multi‐modal‐sized SiC powders with size of from 50 nm to slightly higher than 10 µm after 36‐h ball milling. The milled powders were then incorporated into the semisolid melt of A356 aluminum alloy to ease the incorporation of fine SiC particles by using iron and nickel as their carrier agents. The final as‐cast composites were then extruded at 500 °C with a reduction ratio of 9:1. Lower‐sized composite powders with slight agglomeration are obtained for the 36‐h milled Ni–SiC mixture compared to that of Fe–SiC powders, leading to incorporation of SiC particles into the melt with a lower size and suitable distribution for the Ni–SiC mixture. It is found that lower‐sized composite particles could release the fine SiC particles into the melt more easily, while large agglomerated composite particles almost remain in its initial form, resulting in sites of stress concentration and low‐strength aluminum matrix composites. Ultimate tensile strength (UTS) and yield strength (YS) values of 243 and 135 MPa, respectively, are obtained for the aluminum matrix composite in which nickel acts as the carrier of fine ceramic particles.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Bauxite Residue and Utilization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Materials Engineering Sahand University of Technology 65175‐4171 Tabriz Iran
Advanced Processing Technology Research Centre School of Mechanical and Manufacturing Engineering Dublin City University Dublin 9 Ireland
Funding
Iran National Science Foundation
References (31)
Show source-provided references
1. 10.1016/j.matdes.2015.06.02710.1016/j.matdes.2015.06.027 ↗
2. SoltaniS KhosroshahiRA MousavianRT JiangZ‐Y BoostaniAF BrabazonD.Stir casting process for manufacture of Al–SiC composites.Rare Met.2015.10.1007/s12598‐015‐0565‐710.1007/s12598-015-0565-7 ↗
3. 10.1007/s00170‐015‐7246‐410.1007/s00170‐015‐7246‐4 ↗
4. 10.1016/j.matdes.2015.09.13010.1016/j.matdes.2015.09.130 ↗
5. 10.1016/j.matdes.2015.09.06310.1016/j.matdes.2015.09.063 ↗
6. 10.1016/j.msea.2015.09.05010.1016/j.msea.2015.09.050 ↗
7. 10.1016/j.matdes.2012.07.00710.1016/j.matdes.2012.07.007 ↗
8. 10.1016/j.enconman.2015.04.01710.1016/j.enconman.2015.04.017 ↗
9. 10.1007/s11665‐013‐0835‐110.1007/s11665‐013‐0835‐1 ↗
10. 10.1016/j.ceramint.2014.01.03810.1016/j.ceramint.2014.01.038 ↗
11. 10.1007/s12613‐013‐0824‐210.1007/s12613‐013‐0824‐2 ↗
12. 10.2298/JMMB120701032R10.2298/JMMB120701032R ↗
13. 10.1016/j.ceramint.2014.04.05510.1016/j.ceramint.2014.04.055 ↗
14. 10.1179/1743294414Y.000000033510.1179/1743294414Y.0000000335 ↗
15. NooriH MousavianRT KhosroshahiRA BrabazonD DamadiSR.Effect of SiC particle morphology on Co–P electroless coating characteristics.Surf Eng.2015.10.1179/1743294415Y.0000000035
16. 10.1007/s11663‐014‐0186‐910.1007/s11663‐014‐0186‐9 ↗
17. RajuKSR RajuVR RajuPRM GhosalP.Launching particle to constant reinforcement ratio as a parameter for improving the nanoreinforcement distribution and tensile strength of aluminum nanometal matrix composites. In:Proceedings of International Conference on Advances in Design and Manufacturing. Tiruchirappalli 2015.1.10.3139/146.111246 ↗
18. 10.1504/IJNM.2015.07052710.1504/IJNM.2015.070527 ↗
19. 10.1016/j.compositesa.2014.10.01010.1016/j.compositesa.2014.10.010 ↗
20. 10.1179/1743284711Y.000000000910.1179/1743284711Y.0000000009 ↗
21. 10.1088/0953‐8984/24/25/25530410.1088/0953‐8984/24/25/255304 ↗
22. Assembly of metals and nanoparticles into novel nanocomposite superstructures
23. 10.3390/coatings402023110.3390/coatings4020231 ↗
24. 10.1016/S0921‐5093(03)00639‐710.1016/S0921‐5093(03)00639‐7 ↗
25. 10.1016/j.jallcom.2006.11.18110.1016/j.jallcom.2006.11.181 ↗
26. 10.1016/j.matchar.2010.06.00210.1016/j.matchar.2010.06.002 ↗
27. 10.1016/j.compositesa.2006.02.01010.1016/j.compositesa.2006.02.010 ↗
28. 10.1016/j.msea.2013.06.03010.1016/j.msea.2013.06.030 ↗
29. 10.1016/S0921‐5093(02)00380‐510.1016/S0921‐5093(02)00380‐5 ↗
30. 10.1016/j.intermet.2009.03.00310.1016/j.intermet.2009.03.003 ↗
31. Measurement of van der Waal’s forces between iron/iron surfaces in water by atomic force microscopy