Microstructure and mechanical properties of a new Ti 2 AlNb‐based alloy after aging treatment
Source abstract
Abstract
Abstract A new Ti 2 AlNb‐based alloy with the composition of Ti–22Al–25Nb–1Mo–1V–1Zr–0.2Si (at%) was fabricated in the sequence of arc melting, forging, solid solution and aging. Present paper focuses on the effects of aging temperatures (700, 750, 800, 850 and 900 °C) on microstructure, room‐temperature tensile properties as well as tensile properties at 650 °C and creep properties at 650 °C/150 MPa. It is obvious that the aging treatment promotes the precipitation of O lathes from B2 matrix. With aging temperature increasing, the content of O phase decreases and its size increases gradually, which leads to the decrease in tensile strengths both at room temperature and 650 °C and a little increase in ductility. For creep properties, the sample aged at 700 °C shows the best creep resistance due to its extremely high O phase content. Aging at 800 °C leads to the decrease in the content of O phase and softening of the alloy significantly. However, with aging temperature further increasing from 800 to 900 °C, the precipitated O phase will be coarsened gradually, which strengthens the alloy again.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Titanium Alloys Microstructure and Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Western Superconducting Technologies Co Ltd Shaanxi Province Engineering Laboratory for Aerial Material 710018 Xi'an China
State Key Laboratory of Solidification Processing Northwestern Polytechnical University 710072 Xi'an China
Funding
China Postdoctoral Science Foundation
References (31)
Show source-provided references
1. 10.1016/j.msea.2014.08.01810.1016/j.msea.2014.08.018 ↗
2. 10.1016/j.matchar.2016.02.01110.1016/j.matchar.2016.02.011 ↗
3. 10.1016/j.intermet.2010.02.01010.1016/j.intermet.2010.02.010 ↗
4. WuY LiuG LiuZQ TangZJ WangB.Microstructure mechanical properties and post‐weld heat treatments of dissimilar laser‐welded Ti2AlNb/Ti60 sheet.Rare Met.2018.10.1007/s12598‐018‐1047‐5
5. 10.1016/0001‐6160(88)90141‐110.1016/0001‐6160(88)90141‐1 ↗
6. 10.1002/1527‐2648(200111)3:11<851:AID‐ADEM851>3.0.CO;2‐G10.1002/1527‐2648(200111)3:11<851:AID‐ADEM851>3.0.CO;2‐G ↗
7. 10.1016/S0966‐9795(98)00044‐210.1016/S0966‐9795(98)00044‐2 ↗
8. 10.1016/0036‐9748(89)90345‐110.1016/0036‐9748(89)90345‐1 ↗
9. 10.1007/s12598‐015‐0646‐710.1007/s12598‐015‐0646‐7 ↗
10. 10.1016/j.apsusc.2010.08.10110.1016/j.apsusc.2010.08.101 ↗
11. 10.1016/0956‐716X(93)90198‐210.1016/0956‐716X(93)90198‐2 ↗
12. 10.1016/S1359‐6462(00)00636‐910.1016/S1359‐6462(00)00636‐9 ↗
13. 10.1016/j.scriptamat.2007.03.05310.1016/j.scriptamat.2007.03.053 ↗
14. 10.1016/S0921‐5093(01)01626‐410.1016/S0921‐5093(01)01626‐4 ↗
15. 10.1016/j.msea.2016.10.04710.1016/j.msea.2016.10.047 ↗
16. 10.1016/S0966‐9795(99)00151‐X10.1016/S0966‐9795(99)00151‐X ↗
17. 10.1016/S1875‐5372(15)30016‐310.1016/S1875‐5372(15)30016‐3 ↗
18. 10.1016/j.intermet.2004.12.00310.1016/j.intermet.2004.12.003 ↗
19. 10.1016/S0966‐9795(99)00062‐X10.1016/S0966‐9795(99)00062‐X ↗
20. 10.1016/S0921‐5093(01)01155‐810.1016/S0921‐5093(01)01155‐8 ↗
21. 10.1016/j.msea.2014.09.03510.1016/j.msea.2014.09.035 ↗
22. 10.1016/j.intermet.2014.07.01110.1016/j.intermet.2014.07.011 ↗
23. 10.1016/j.intermet.2013.09.01110.1016/j.intermet.2013.09.011 ↗
24. 10.1016/S1003‐6326(15)63874‐210.1016/S1003‐6326(15)63874‐2 ↗
25. 10.1007/s11669‐005‐0089‐110.1007/s11669‐005‐0089‐1 ↗
26. 10.1016/j.msea.2014.05.07610.1016/j.msea.2014.05.076 ↗
27. 10.1016/j.jallcom.2013.05.01810.1016/j.jallcom.2013.05.018 ↗
28. 10.1016/S0966‐9795(00)00083‐210.1016/S0966‐9795(00)00083‐2 ↗
29. 10.1016/j.msea.2012.07.03610.1016/j.msea.2012.07.036 ↗
30. 10.1016/j.jallcom.2003.08.07810.1016/j.jallcom.2003.08.078 ↗
31. 10.1016/j.msea.2008.07.01410.1016/j.msea.2008.07.014 ↗