Microstructure and tensile properties of A356 alloy with different Sc/Zr additions
Source abstract
Abstract
Abstract Addition of rare earth elements for improving the tensile properties of aluminum alloys has attracted great attention. In this study, a systematic analysis on the microstructure and tensile properties of A356–0.13Ti alloys with different contents of scandium (Sc) and scandium/zirconium (Sc/Zr) after solution and aging treatment process was carried out. The addition of Sc/Zr into A356–0.13Ti alloys can greatly refine the grain size and modify the deleterious coarse eutectic Si structure and harmful acicular iron‐containing phase morphology. As a result, the maximum value of strength (298 MPa) and ductility (elongation of 8.4%) are acquired by co‐addition of Sc/Zr after solution and aging treatment process, which indicates that the tensile properties of A356 alloy are greatly enhanced by the synergistic effect of co‐addition of Sc/Zr.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Bauxite Residue and Utilization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering and Tianjin Key Laboratory of Composites and Functional Materials Tianjin University 300350 Tianjin China
Collaborative Innovation Center of Chemical Science and Engineering 300072 Tianjin China
Funding
National Natural Science Foundation of China
References (37)
Show source-provided references
1. 10.1016/S1359‐6454(98)00059‐710.1016/S1359‐6454(98)00059‐7 ↗
2. Precipitation processes in an Al–Mg//2Si(Mn) alloy
3. 10.1016/S1359‐6454(97)00493‐X10.1016/S1359‐6454(97)00493‐X ↗
4. The structure of the metastable precipitates formed during ageing of an Al–Mg–Si alloy
5. 10.1016/j.msea.2004.11.04810.1016/j.msea.2004.11.048 ↗
6. 10.1016/j.actamat.2014.10.05510.1016/j.actamat.2014.10.055 ↗
7. 10.1016/j.msea.2005.06.02410.1016/j.msea.2005.06.024 ↗
8. 10.1016/j.jallcom.2009.07.06410.1016/j.jallcom.2009.07.064 ↗
9. 10.1179/174328005X1431110.1179/174328005X14311 ↗
10. 10.1016/j.matdes.2015.09.04510.1016/j.matdes.2015.09.045 ↗
11. 10.1016/S1359‐6454(98)00257‐210.1016/S1359‐6454(98)00257‐2 ↗
12. 10.1016/j.msea.2013.11.03910.1016/j.msea.2013.11.039 ↗
13. 10.1016/j.actamat.2012.03.03110.1016/j.actamat.2012.03.031 ↗
14. 10.1007/BF0264620410.1007/BF02646204 ↗
15. 10.1016/j.matchar.2011.11.00510.1016/j.matchar.2011.11.005 ↗
16. 10.1016/j.jallcom.2014.07.03710.1016/j.jallcom.2014.07.037 ↗
17. 10.1016/j.scriptamat.2004.11.02110.1016/j.scriptamat.2004.11.021 ↗
18. 10.1016/j.msea.2016.06.02210.1016/j.msea.2016.06.022 ↗
19. 10.1016/j.msea.2014.08.04110.1016/j.msea.2014.08.041 ↗
20. 10.1016/j.actamat.2010.12.01410.1016/j.actamat.2010.12.014 ↗
21. 10.1016/j.msea.2014.03.00510.1016/j.msea.2014.03.005 ↗
22. 10.1016/j.jallcom.2015.10.29610.1016/j.jallcom.2015.10.296 ↗
23. 10.1016/j.actamat.2009.12.03810.1016/j.actamat.2009.12.038 ↗
24. 10.1016/j.actamat.2015.02.00410.1016/j.actamat.2015.02.004 ↗
25. 10.1016/j.matdes.2013.10.01810.1016/j.matdes.2013.10.018 ↗
26. Effect of minor Sc and Zr on recrystallization behavior and mechanical properties of novel Al–Zn–Mg–Cu alloys
27. 10.1016/j.actamat.2005.08.01610.1016/j.actamat.2005.08.016 ↗
28. 10.1038/nmat165210.1038/nmat1652 ↗
29. 10.1016/j.scriptamat.2004.03.03310.1016/j.scriptamat.2004.03.033 ↗
30. 10.1016/j.commatsci.2015.04.03510.1016/j.commatsci.2015.04.035 ↗
31. 10.1016/j.matdes.2003.11.00710.1016/j.matdes.2003.11.007 ↗
32. Solidified microstructure of semisolid A356–Ce alloy with two‐way intermittent electromagnetic stirring
33. Improvement of anisotropy of as‐cast Cu–Ag alloy with columnar grains by homogenization
34. Texture evolution and mechanical properties of 6016 aluminum alloys as equal channel angular rolling at different preheat temperatures
35. Properties of A356 aluminum alloy with ce addition and its refining mechanism
36. Microstructure characterization in a Zn modified Al–Mg–Mn alloy
37. 10.1007/s12598‐015‐0623‐110.1007/s12598‐015‐0623‐1 ↗