journal article·2012-06

Surface recrystallization of a Ni 3 Al based single crystal superalloy at different annealing temperature and blasting pressure

Yuxiao Wu, Ruibo Yang, Shusuo Li, Yue Ma, Shengkai Gong, Yafang Han

Rare Metals· Volume 31· Issue 3
Publisher page

Abstract

Abstract The effects of annealing temperature and grit blasting pressure on the recrystallization behavior of a Ni 3 Al based single crystal superalloy were studied in this work. The results show that the precipitation of the Y‐NiMo phase occurs at 900 and 1000 °C, which precedes recrystallization. The initial recrystallization temperature was between 1000 and 1100 °C. Cellular recrystallization was formed at 1100 and 1200 °C, which consisted of large columnar γ′ and fine γ + γ′. The dendrite arm closed to the interdendritic region may act as nucleation sites during initial recrystallization by a particle simulated nucleation mechanism at 1280 °C. The size of the grains first turned large and then became small upon the pressure while the recrystallization depth increased all the time.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Advanced Materials Characterization Techniques · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Key Laboratory of Aerospace Materials and Performance (Ministry of Education) School of Materials Science and Engineering Beijing University of Aeronautics and Astronautics 100191 Beijing China

Beijing Institute of Aeronautical Materials 100095 Beijing China

References (30)

Show source-provided references
1. 10.1016/j.msea.2010.04.07110.1016/j.msea.2010.04.071 ↗
2. 10.1007/s12598‐010‐0140‐110.1007/s12598‐010‐0140‐1 ↗
3. 10.1007/s11661‐004‐0364‐510.1007/s11661‐004‐0364‐5 ↗
4. 10.1179/02670830322500834710.1179/026708303225008347 ↗
5. Okazaki M. · 2000 · 505
6. Mechanical behavior and processing of DS and single crystal superalloys
7. 10.1007/s12613‐011‐0422‐010.1007/s12613‐011‐0422‐0 ↗
8. 10.1016/S1000‐9361(09)60244‐210.1016/S1000‐9361(09)60244‐2 ↗
9. 10.1016/j.matchar.2010.04.00710.1016/j.matchar.2010.04.007 ↗
10. 10.1007/s12598‐010‐0055‐x10.1007/s12598‐010‐0055‐x ↗
11. 10.1016/S1006‐706X(10)60031‐310.1016/S1006‐706X(10)60031‐3 ↗
12. 10.1179/02670830322501073110.1179/026708303225010731 ↗
13. 10.1179/02670830322500830110.1179/026708303225008301 ↗
14. 10.7449/2000/Superalloys_2000_229_23810.7449/2000/Superalloys_2000_229_238 ↗
15. 10.1007/BF0098074910.1007/BF00980749 ↗
16. 10.1179/026708309X1249554850842810.1179/026708309X12495548508428 ↗
17. Surface recrystalliztion in a Ni3Al base single crystal alloy IC6SX
18. 10.1016/j.intermet.2010.08.01910.1016/j.intermet.2010.08.019 ↗
19. Effects of withdrawal rate on microstructure and stress rupture properties of a Ni3Al‐based single crystal superalloy IC6SX
20. 10.1016/j.intermet.2007.05.00810.1016/j.intermet.2007.05.008 ↗
21. 10.1016/S0921‐5093(01)01355‐710.1016/S0921‐5093(01)01355‐7 ↗
22. Effect of long term aging on microstructure and mechanical properites of Ni3Al base alloy IC6
23. 10.1016/0921‐5093(94)03305‐610.1016/0921‐5093(94)03305‐6 ↗
24. 10.4028/www.scientific.net/MSF.650.20510.4028/www.scientific.net/MSF.650.205 ↗
25. Humphreys F.J. · 2004 · 310
26. 10.1007/BF0240278810.1007/BF02402788 ↗
27. 10.1023/A:100484852858210.1023/A:1004848528582 ↗
28. Humphreys F.J. · 2004 · 48
29. WuY.X. Recrystallization of Ni3Al Based Single Crystal Superalloys[Dissertation] Beihang University Beijing 2011:31.
30. Mao W. M. · 1994 · 56