journal article·2025-04

In‐situ interfacial reactions in boron nitride‐reinforced zinc implants for achieving strength and toughness

Ci‐Jun Shuai, Jin Zhang, Ming‐Li Yang, Chong‐Xian He, Xiong Shuai, Xin‐Yi Xiao, Dong‐Sheng Wang, Yin‐Jin Shao, You‐Wen Yang

Rare Metals· Volume 44· Issue 4
Publisher page

Abstract

Abstract Boron nitride (BN), as a nano‐reinforcement, offers notable benefits for zinc (Zn)‐based implants due to its distinct asymmetric hexagonal structure and high fracture strength. However, the limited interface adhesion between BN and Zn limits its potential for strengthening and toughening. In this study, copper (Cu) was in situ grown on acidified BN through chemical synthesis and subsequently incorporated into laser additive manufacturing of Zn to enhance interface bonding. During this process, the Cu on BN experienced a displacement reaction with Zn due to thermal reduction induced by the high‐energy laser, leading to the replacement of Cu by Zn and the formation of a robust covalent bond between BN and the Zn matrix, thereby improving load transfer. Additionally, the reduced Cu further interacted with Zn to produce the CuZn 5 phase, which was evenly dispersed in the Zn matrix under Marangoni vortices, resulting in both dispersion and Orowan strengthening. Consequently, the ultimate tensile strength of the composites achieved (251 ± 7) MPa. The fracture toughness also showed a notable increase from 12.10 to 24.03 MPa·m 1/2 , as the unique structure of BN effectively redistributed stress at the crack tip and absorbed considerable fracture energy. Furthermore, the Cu@BN/Zn implants demonstrated excellent antibacterial properties.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Boron and Carbon Nanomaterials Research · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of Precision Manufacturing for Extreme Service Performance Central South University 410083 Changsha China

Jiangxi Province Key Laboratory of Additive Manufacturing of Implantable Medical Device Jiangxi University of Science and Technology 330013 Nanchang China

Mechanical Engineering Department University of North Texas 76201 Denton USA

College of Mechanical Engineering Tongling University 244061 Tongling China

Department of Rehabilitation Ganzhou People’s Hospital 341099 Ganzhou China

Funding

National Natural Science Foundation of China

References (55)

Show source-provided references
1. 10.1038/s41467‐019‐14153‐710.1038/s41467‐019‐14153‐7 ↗
2. 10.1007/s12598‐015‐0601‐710.1007/s12598‐015‐0601‐7 ↗
3. 10.1016/j.jmrt.2024.03.05010.1016/j.jmrt.2024.03.050 ↗
4. 10.1016/j.actbio.2019.07.03810.1016/j.actbio.2019.07.038 ↗
5. 10.13373/j.cnki.cjrm.XY2103000810.13373/j.cnki.cjrm.XY21030008 ↗
6. 10.1016/j.jma.2024.03.01410.1016/j.jma.2024.03.014 ↗
7. 10.1016/j.ijmecsci.2024.10956610.1016/j.ijmecsci.2024.109566 ↗
8. 10.1016/j.cej.2021.12931710.1016/j.cej.2021.129317 ↗
9. 10.1088/2631‐7990/ad392910.1088/2631‐7990/ad3929 ↗
10. 10.1007/s12598‐024‐02753‐210.1007/s12598‐024‐02753‐2 ↗
11. 10.1016/j.pmatsci.2022.10096310.1016/j.pmatsci.2022.100963 ↗
12. 10.1038/s41586‐021‐03488‐110.1038/s41586‐021‐03488‐1 ↗
13. 10.1016/j.msea.2021.14096910.1016/j.msea.2021.140969 ↗
14. 10.1016/j.jmst.2022.10.05810.1016/j.jmst.2022.10.058 ↗
15. 10.1021/acs.nanolett.5b0184210.1021/acs.nanolett.5b01842 ↗
16. 10.1016/j.jallcom.2022.16611710.1016/j.jallcom.2022.166117 ↗
17. 10.1016/j.jre.2022.05.00610.1016/j.jre.2022.05.006 ↗
18. 10.1016/j.apsusc.2019.04.11110.1016/j.apsusc.2019.04.111 ↗
19. 10.1016/j.msea.2017.10.03010.1016/j.msea.2017.10.030 ↗
20. 10.1016/j.carbon.2020.12.05910.1016/j.carbon.2020.12.059 ↗
21. 10.1007/s12598‐024‐02782‐x10.1007/s12598‐024‐02782‐x ↗
22. 10.1016/j.carbon.2017.11.03310.1016/j.carbon.2017.11.033 ↗
23. 10.1016/j.surfin.2024.10384610.1016/j.surfin.2024.103846 ↗
24. 10.13373/j.cnki.cjrm.XY2205000610.13373/j.cnki.cjrm.XY22050006 ↗
25. 10.1016/j.vacuum.2023.11293910.1016/j.vacuum.2023.112939 ↗
26. 10.1039/d3bm01283b10.1039/d3bm01283b ↗
27. 10.1021/acs.langmuir.3c0095510.1021/acs.langmuir.3c00955 ↗
28. 10.1021/acscatal.4c0196110.1021/acscatal.4c01961 ↗
29. 10.1021/acs.chemrev.9b0044310.1021/acs.chemrev.9b00443 ↗
30. 10.1016/j.jmrt.2022.08.09310.1016/j.jmrt.2022.08.093 ↗
31. 10.1016/j.jallcom.2020.15776510.1016/j.jallcom.2020.157765 ↗
32. 10.1088/2053‐1591/ab6c1d10.1088/2053‐1591/ab6c1d ↗
33. ChourasiyaA KrishnaCM. Mechanical and microstructure behavior of AA7050 metal matrix composite reinforced with TiO2/BN.Int J Metalcasting..2024.10.1007/s40962‐023‐01248‐710.1007/s40962-023-01248-7 ↗
34. 10.1016/j.diamond.2023.11002810.1016/j.diamond.2023.110028 ↗
35. 10.1038/s41598‐022‐24427‐810.1038/s41598‐022‐24427‐8 ↗
36. 10.1007/s40962‐023‐01070‐110.1007/s40962‐023‐01070‐1 ↗
37. 10.1007/s11665‐023‐08838‐w10.1007/s11665‐023‐08838‐w ↗
38. 10.1007/s12633‐022‐01823‐310.1007/s12633‐022‐01823‐3 ↗
39. 10.1016/j.mtcomm.2023.10745710.1016/j.mtcomm.2023.107457 ↗
40. 10.1080/17452759.2024.231778010.1080/17452759.2024.2317780 ↗
41. 10.1016/j.matchar.2023.11328210.1016/j.matchar.2023.113282 ↗
42. 10.1038/s41467‐024‐45657‐610.1038/s41467‐024‐45657‐6 ↗
43. 10.1007/s12598‐023‐02341‐w10.1007/s12598‐023‐02341‐w ↗
44. 10.1016/j.actamat.2023.11907910.1016/j.actamat.2023.119079 ↗
45. 10.1016/j.actamat.2022.11862910.1016/j.actamat.2022.118629 ↗
46. 10.1016/j.msea.2018.06.03510.1016/j.msea.2018.06.035 ↗
47. 10.1016/j.jmst.2023.10.05210.1016/j.jmst.2023.10.052 ↗
48. 10.1002/adfm.20221034510.1002/adfm.202210345 ↗
49. 10.1007/s42242‐023‐00264‐010.1007/s42242‐023‐00264‐0 ↗
50. 10.1007/s12598‐022‐02098‐810.1007/s12598‐022‐02098‐8 ↗
51. 10.1038/s41467‐019‐09946‐910.1038/s41467‐019‐09946‐9 ↗
52. 10.1088/1748‐605x/ad4aa910.1088/1748‐605x/ad4aa9 ↗
53. 10.1088/2631‐7990/ad01fd10.1088/2631‐7990/ad01fd ↗
54. 10.3969/j.issn.1009‐3842.2023.06.00110.3969/j.issn.1009‐3842.2023.06.001 ↗
55. 10.1016/j.actbio.2023.02.02910.1016/j.actbio.2023.02.029 ↗