Abstract

Abstract Complex concentrated alloys (CCAs) containing the L2 1 phase are recognized for their exceptional strength and thermal stability, positioning them as strong candidates for transformative applications in aerospace, energy, and structural sectors. This investigation delves into the AlFe x NiTiV 40− x ( x = 0, 10, 20, 30, 35, 40; at%) CCAs, aiming to unlock the synergistic potential of BCC and L2 1 phases. By conducting an in‐depth analysis of microstructure, phase behavior, and mechanical properties, the intricate relationships between chemistry, structure, and properties are illuminated within this alloy system. The Al 15 Fe 35 Ni 30 Ti 15 V 5 alloy demonstrates remarkable mechanical properties, achieving a yield strength of 2140.9 MPa and ultimate compressive strength of 2699.7 MPa, primarily through solid solution strengthening and precipitation hardening. Notably, its low lattice mismatches and nanoprecipitate strengthening yield an impressive specific yield strength at 600 °C (245.2 MPa(g·cm −3 ) −1 ). Phase modulation achieves the synergistic optimization of specific strengths at both room and high temperatures in CCAs containing the L2 1 phase, opening new avenues for designing advanced lightweight and high strength alloys for elevated‐temperature applications.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering Harbin Institute of Technology (Shenzhen) 518055 Shenzhen China

Institute of Special Environments Physical Sciences Harbin Institute of Technology (Shenzhen) 518055 Shenzhen China

State Key Laboratory of Advanced Welding and Joining Harbin Institute of Technology 150001 Harbin China

Funding

Basic and Applied Basic Research Foundation of Guangdong Province · National Natural Science Foundation of China · the Shenzhen Science and Technology Plan-Technology Innovation · Guangdong Basic and Applied Basic Research Foundation · the Shenzhen Knowledge Innovation Plan-Fundamental Research · the Startup Foundation from Shenzhen

References (56)

Show source-provided references
1. 10.1007/s12598‐016‐0788‐210.1007/s12598‐016‐0788‐2 ↗
2. 10.1016/j.corsci.2021.11005010.1016/j.corsci.2021.110050 ↗
3. 10.1007/s12598‐023‐02482‐y10.1007/s12598‐023‐02482‐y ↗
4. 10.1016/j.eng.2023.06.00810.1016/j.eng.2023.06.008 ↗
5. 10.1016/j.jnucmat.2021.15343110.1016/j.jnucmat.2021.153431 ↗
6. 10.1016/j.engfailanal.2023.10762810.1016/j.engfailanal.2023.107628 ↗
7. 10.1007/s12598‐022‐01965‐810.1007/s12598‐022‐01965‐8 ↗
8. 10.1007/s12598‐018‐1016‐z10.1007/s12598‐018‐1016‐z ↗
9. 10.1016/j.actamat.2018.04.00110.1016/j.actamat.2018.04.001 ↗
10. 10.1126/science.112173810.1126/science.1121738 ↗
11. 10.1038/s41578‐019‐0121‐410.1038/s41578‐019‐0121‐4 ↗
12. 10.1016/j.ijplas.2022.10339810.1016/j.ijplas.2022.103398 ↗
13. 10.1016/j.pmatsci.2020.10070910.1016/j.pmatsci.2020.100709 ↗
14. 10.1016/j.jallcom.2013.11.08410.1016/j.jallcom.2013.11.084 ↗
15. 10.1038/s41467‐020‐14641‐110.1038/s41467‐020‐14641‐1 ↗
16. 10.1126/science.aba372210.1126/science.aba3722 ↗
17. 10.1007/s12598‐021‐01953‐410.1007/s12598‐021‐01953‐4 ↗
18. 10.1007/s12598‐022‐01971‐w10.1007/s12598‐022‐01971‐w ↗
19. 10.1016/j.scriptamat.2014.12.00610.1016/j.scriptamat.2014.12.006 ↗
20. 10.1007/BF0264403510.1007/BF02644035 ↗
21. 10.1007/BF0264403610.1007/BF02644036 ↗
22. 10.1007/s12598‐024‐02657‐110.1007/s12598‐024‐02657‐1 ↗
23. 10.1016/j.scriptamat.2021.11413210.1016/j.scriptamat.2021.114132 ↗
24. 10.1016/j.actamat.2023.11880610.1016/j.actamat.2023.118806 ↗
25. 10.1007/s40843‐022‐2178‐x10.1007/s40843‐022‐2178‐x ↗
26. 10.1016/j.actamat.2016.08.03510.1016/j.actamat.2016.08.035 ↗
27. 10.1016/S0921‐5093(99)00713‐310.1016/S0921‐5093(99)00713‐3 ↗
28. 10.1016/j.actamat.2021.11689010.1016/j.actamat.2021.116890 ↗
29. 10.1016/j.actamat.2022.11850610.1016/j.actamat.2022.118506 ↗
30. 10.1016/j.msea.2022.14299910.1016/j.msea.2022.142999 ↗
31. 10.1016/j.scriptamat.2022.11488910.1016/j.scriptamat.2022.114889 ↗
32. 10.1016/j.actamat.2017.11.01310.1016/j.actamat.2017.11.013 ↗
33. 10.1016/j.msea.2021.14200310.1016/j.msea.2021.142003 ↗
34. 10.1016/j.matdes.2023.11182410.1016/j.matdes.2023.111824 ↗
35. 10.1016/j.actamat.2014.05.01610.1016/j.actamat.2014.05.016 ↗
36. 10.1002/adem.20090006110.1002/adem.200900061 ↗
37. 10.1016/j.jmrt.2023.06.17610.1016/j.jmrt.2023.06.176 ↗
38. 10.1016/j.actamat.2017.12.06110.1016/j.actamat.2017.12.061 ↗
39. 10.1007/BF0065204910.1007/BF00652049 ↗
40. 10.1016/j.actamat.2013.11.04910.1016/j.actamat.2013.11.049 ↗
41. 10.1016/j.dib.2018.10.07110.1016/j.dib.2018.10.071 ↗
42. 10.1016/j.intermet.2018.01.01710.1016/j.intermet.2018.01.017 ↗
43. 10.1007/BF0054098810.1007/BF00540988 ↗
44. 10.1088/0370‐1301/64/9/30310.1088/0370‐1301/64/9/303 ↗
45. 10.1007/s11661‐015‐2969‐210.1007/s11661‐015‐2969‐2 ↗
46. 10.1016/j.actamat.2018.07.02510.1016/j.actamat.2018.07.025 ↗
47. 10.1016/j.jallcom.2020.15611110.1016/j.jallcom.2020.156111 ↗
48. 10.1016/j.ijplas.2017.10.00510.1016/j.ijplas.2017.10.005 ↗
49. 10.1126/sciadv.aat871210.1126/sciadv.aat8712 ↗
50. 10.1007/BF0267041610.1007/BF02670416 ↗
51. 10.1017/S000192400008812610.1017/S0001924000088126 ↗
52. JiY ZhangL XingL PangJ YunzhuoL ZhuZ HuamengF ZhangH LiH ZhangH. Microstructural optimization of FexCrNiAl0.5Ti0.5high entropy alloys toward high ductility.Appl Phys Lett.2021.10.1063/5.006067810.1063/5.0060678 ↗
53. 10.1002/adma.20200672310.1002/adma.202006723 ↗
54. 10.1016/j.intermet.2022.10753910.1016/j.intermet.2022.107539 ↗
55. 10.1016/j.matdes.2013.12.07210.1016/j.matdes.2013.12.072 ↗
56. 10.1038/s41467‐018‐06600‐810.1038/s41467‐018‐06600‐8 ↗