journal article·2015-01

Pressure nitric acid leaching of alkali‐pretreated low‐grade limonitic laterite

Yong‐Lu Zhang, Cheng‐Yan Wang, Yong‐Qiang Yang, Fei Yin, Bao‐Zhong Ma

Rare Metals· Volume 34· Issue 1
Publisher page

Abstract

Abstract The pressure nitric acid leaching of alkali‐pretreated low‐grade limonitic laterite, as well as removing impurity Al(III) and preparing intermediate product of nickel/cobalt sulphide from leaching liquor were investigated. After pretreatment, iron exists in the form of amorphous iron oxides, while nickel is adsorbed on the surface of iron oxides in the form of nickel oxide. The preferable pressure leaching conditions are determined as follows: leaching temperature of 458 K, leaching duration of 60 min, initial acidity of nitric acid of 1.90 mol · L −1 and liquid to solid ratio of 3:1 (volume to mass ratio). Under these conditions, the leaching efficiencies of Ni, Co and Al are 95 %, 88 % and 55 %, respectively, and that of Fe is less than 1 %. The loss rates of Ni and Co are 1.8 % and 1.5 %, respectively, during the step of removing impurity Al(III). The sulphide precipitation process produces the interim production of nickel/cobalt sulphides, recovering greater than 99 % of Ni and Co in the purified solution. The iron‐rich (>60 %) pressure leaching residue with low Cr, S can be further reclaimed as the raw materials for iron making.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Extraction and Bioleaching · Extraction and Separation Processes · Minerals Flotation and Separation Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Metallurgy Beijing General Research Institute of Mining and Metallurgy 100160 Beijing China

Funding

National Natural Science Foundation of China

References (21)

Show source-provided references
1. 10.1007/s11663‐998‐0062‐610.1007/s11663‐998‐0062‐6 ↗
2. 10.1016/j.hydromet.2007.11.00910.1016/j.hydromet.2007.11.009 ↗
3. 10.1016/j.hydromet.2007.11.01010.1016/j.hydromet.2007.11.010 ↗
4. Thermodynamic research on production of ferronickel alloy by electric furnace reduction from lateritic nickel ore
5. 10.1016/j.mineng.2007.11.00210.1016/j.mineng.2007.11.002 ↗
6. Experimental study on laterite‐nickel ore with sulfating roasting‐water immersion methods
7. 10.1016/j.hydromet.2004.11.01110.1016/j.hydromet.2004.11.011 ↗
8. 10.1016/j.hydromet.2010.03.01210.1016/j.hydromet.2010.03.012 ↗
9. 10.1016/j.mineng.2003.08.01510.1016/j.mineng.2003.08.015 ↗
10. 10.1016/j.hydromet.2009.07.00610.1016/j.hydromet.2009.07.006 ↗
11. 10.1016/j.hydromet.2009.07.01210.1016/j.hydromet.2009.07.012 ↗
12. 10.1016/j.oregeorev.2010.05.00310.1016/j.oregeorev.2010.05.003 ↗
13. 10.1016/j.hydromet.2009.08.00610.1016/j.hydromet.2009.08.006 ↗
14. The thunder from down under: everything you wanted to know about laterites but were afraid to ask
15. 10.1016/S0304‐386X(98)00023‐110.1016/S0304‐386X(98)00023‐1 ↗
16. 10.1016/S0304‐386X(00)00092‐X10.1016/S0304‐386X(00)00092‐X ↗
17. 10.1016/S0304‐386X(00)00094‐310.1016/S0304‐386X(00)00094‐3 ↗
18. 10.1016/S0304‐386X(03)00043‐410.1016/S0304‐386X(03)00043‐4 ↗
19. 10.1016/j.mineng.2011.03.00110.1016/j.mineng.2011.03.001 ↗
20. 10.1016/j.hydromet.2010.06.01010.1016/j.hydromet.2010.06.010 ↗
21. 10.1002/ceat.20050036510.1002/ceat.200500365 ↗